PhC-2019
Change in the baric dependences of the thermophysical properties of a niobium nanocrystal with a change in size
S.P. Kramynin Institute of Physics named after H.I. Amirkhanova – subdivision of Dagestan Federal Research Center of the Russian Academy of Sciences, Makhachkala, Russia DOI: 10.26456/pcascnn/2019.11.315 Abstract: From a general point of view, the equation of state and the change in thermophysical properties of Nb ...
Application of the fractal theory for studying brushit crystallization process in the presence of additives
V.M. Kiselev, O.A. Golovanova Dostoevsky Omsk State University, Omsk, Russia DOI: 10.26456/pcascnn/2019.11.307 Abstract: The paper considers the possibility of using the fractal analysis method for brushite-based samples, including modified with organic and inorganic additives. The dependencies between fractal parameters and properties of samples are determined. ...
Effect of synthesis parameters on dimensional characteristics of Fe3O4 nanoparticles: neural-network research
A.V. Blinov, A.A. Gvozdenko, M.A. Yasnaya, A.B. Golik, А.A. Blinova, I.M. Shevchenko, V.N. Kramarenko North-Caucasian Federal University, Stavropol, Russia DOI: 10.26456/pcascnn/2019.11.298 Abstract: Our research shows the possibility of using the neural-network processing of experimental data to study the influence of various factors on the process ...
Accounting of tunneling effects when calculating the energy spectrum of the Schrödinger equation
I.N. Belyaeva1, N.A. Chekanov1, I.K. Kirichenko2, N.N. Chekanova3 1Belgorod National Research University, Belgorod, Russia 2National University of Civil Defence of Ukraine, Kharkiv, Ukraine 3Kharkiv Educational and Research Institute of the Higher Educational Institution «University of Banking», Kharkiv, Ukraine DOI: 10.26456/pcascnn/2019.11.291 Abstract: The general scheme of the ...
The computer – assisted solution of the one – dimensional Schrödinger equation taking into account tunneling effects
I.N. Belyaeva1, I.K. Kirichenko2, O.D. Ptashnyi3, N.N. Chekanova4, N.A. Chekanov1, T.A. Yarkho3 1Belgorod National Research University, Belgorod, Russia 2National University of Civil Defence of Ukraine, Kharkiv, Ukraine 3Kharkiv National Automobile and Highway University, Kharkiv, Ukraine 4Kharkiv Educational and Research Institute of the Higher Educational Institution «University of Banking», Kharkiv, Ukraine DOI: 10.26456/pcascnn/2019.11.283 ...
On special features of studying electric conductivity in special electron optics glasses
Z.V. Shomakhov1,2, O.A. Molokanov1, A.M. Karmokov1 1Kabardino-Balkarian State University named after H.M. Berbekov, Nalchik, Russia 2Institute of Applied Mathematics and Automation – branch of the Federal Research Center «Kabardino-Balkarian Scientific Center of the RAS», Nalchik, Russia DOI: 10.26456/pcascnn/2019.11.277 Abstract: The laws of the change in ...
Several peculiarities of high-temperature phase equilibria in nanoparticles of the Six – Ge1-x system
A.V. Shishulin1, A.V. Shishulina2,3 1G.A. Razuvaev institute of organometallic chemistry of Russian Academy of Sciences, Nizhny Novgorod, Russia 2R.E. Alekseev Nizhny Novgorod State Technical University, Dzerzhinsk, Russia 3N.I. Lobachevsky National Research Nizhny Novgorod State University, Nizhny Novgorod, Russia DOI: 10.26456/pcascnn/2019.11.268 Abstract: Phase equilibria in Six – Ge1-x nanoparticles of ...
Features of the electrochromium effect in complex transition metal oxides
B.M. Khubolov1, V.P. Podlinov2 1Kabardino-Balkarian State University named after H.M. Berbekov, Nalchik, Russia 2North-Caucasus Federal University, Stavropol, Russia DOI: 10.26456/pcascnn/2019.11.259 Abstract: Some features of electrochromically sensitive single crystals and thin films of the complex transition metal oxides are reviewed. Based on the results of studies ...
Using the dilatational rheology method for analysis of nanosized systems
S.L. Khil’ko, M.I. Rogatko, R.A. Makarova, R.G. Semenova Public Institution «L.M.Litvinenko Institute of Physical Organic and Coal Chemistry», Donetsk, Ukraine DOI: 10.26456/pcascnn/2019.11.249 Abstract. The regularities of the formation of interfacial layers of nanosized natural polyelectrolytes based on humic substances and their complexes with cationic surfactants ...
Photorefractive properties and optical uniformity of crystals LiNbO3 (6,0 wt. % K2O)
N.A. Teplyakova, N.V. Sidorov, M N. Palatnikov Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the Russian Academy of Sciences», Apatity, Russia DOI: 10.26456/pcascnn/2019.11.241 Abstract: Comparative researches were carried out for lithium niobate crystals with congruent and stoichiometric ...