Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Synthesis and investigation of properties of composite ceramics LuAG: Ce / Al2O3

V.A. Lapin, A.A. Kravtsov, V.E. Suprunchuk, L.V. Tarala, E.V. Medyanik, F.F. Malyavin

North-Caucasus Federal University

DOI: 10.26456/pcascnn/2023.15.157

Original article

Abstract: The purpose of this work was to study the effect of the aluminum oxide impurity content onthe features of  vacuum sintering, optical and luminescent properties of composite ceramics LuAG:Ce / Al2O3. Ceramic powders LC-1, LC-2, LC-3 of the composition Lu2,98Ce0,02Al5O12 / Al2Owere synthesized, where the corundum content was 0, 10, 20 wt.% respectively. The dynamics of shrinkage of ceramic compacts by dilatometry, morphology and elemental analysis of the surface of sintered ceramics LuAG are investigated: Ce / Al2O3 – by scanning electron microscopy. Light transmission and luminescence spectra were obtained. It is shown that with an increase in the content of corundum in the composition of ceramic powder, the temperatures of the beginning and end of shrinkage increase. In this case, the residual porosity is concentrated in areas of ceramics containing mainly corundum crystallites, as a material with a higher sintering temperature. It was revealed that the inclusion of the corundum phase prevents the uncontrolled growth of ceramic grains. Composition with a corundum content of 10 wt.% showed the highest value of luminescence intensity. At the same time, with an increase in the proportion of corundum in composite ceramics, a slight broadening of the luminescence spectra was observed.

Keywords: : LuAG:Ce, ceramics, aluminum oxide, luminescence, optical properties, sintering

  • Viacheslav A. Lapin – Ph.D., Senior Researcher, Sector of Physical and Chemical Methods of Research and Analysis of the Research Laboratory of Technology of Advanced Materials and Laser Media of the Scientific Laboratory Complex of Clean Rooms, Faculty of Physics and Technology, North-Caucasus Federal University
  • Alexander A. Kravtsov – Ph.D., Head of the Nanopowder Synthesis Sector of the Research Laboratory of Technology of Advanced Materials and Laser Media of the Scientific Laboratory Complex of Clean Rooms, Faculty of Physics and Technology, North-Caucasus Federal University
  • Victoria E. Suprunchuk – Ph.D., Senior Researcher, Nanopowder Synthesis Sector of the Research Laboratory of Technology of Advanced Materials and Laser Media of the Scientific Laboratory Complex of Clean Rooms, Faculty of Physics and Technology, North-Caucasus Federal University
  • Ludmila V. Tarala – Researcher, Nanopowder Synthesis Sector of the Research Laboratory of Technology of Advanced Materials and Laser Media of the Scientific Laboratory Complex of Clean Rooms, Faculty of Physics and Technology, North-Caucasus Federal University
  • Evgeniy V. Medyanik – Researcher, Ceramics Sintering Sector of the Research Laboratory of Technology of Advanced Materials and Laser Media of the Scientific Laboratory Complex of Clean Rooms, Faculty of Physics and Technology, North-Caucasus Federal University
  • Fedor F. Malyavin – Head of Ceramics Sintering Sector of the Research Laboratory of Technology of Advanced Materials and Laser Media of the Scientific Laboratory Complex of Clean Rooms, Faculty of Physics and Technology, North-Caucasus Federal University

For citation:

Lapin V.A., Kravtsov A.A., Suprunchuk V.E., Tarala L.V., Medyanik E.V., Malyavin F.F. Sintez i issledovanie svojstv kompozitnoj keramiki LuAG: Ce / Al2O3 [Synthesis and investigation of properties of composite ceramics LuAG: Ce / Al2O3], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 157-168. DOI: 10.26456/pcascnn/2023.15.157.

Full article (in Russian): download PDF file

References:

1. Liu I., Feng T., Sui Z. et al. 50 mm-aperture Nd:LuAG ceramic nanosecond laser amplifier producing 10 J at 10 Hz, Optics Express, 2019, vol. 27, issue 11, pp 15595-15603. DOI: 10.1364/OE.27.015595.
2. Chen X., Hu Z., Cao M. et al. Influence of cerium doping concentration on the optical properties of Ce, Mg: LuAG scintillation ceramics, Journal of the European Ceramic Society, 2018, vol. 38, issue 9, pp 3246-3254. DOI: 10.1016/j.jeurceramsoc.2018.03.023.
3. Zhang Y., Hua S., Wanga Z. et al. Pore-existing Lu3Al5O12:Ce ceramic phosphor: An efficient green color converter for laser light source, Journal of Luminescence, 2018, vol. 197, pp 331-334. DOI: 10.1016/j.jlumin.2018.01.014.
4. Hu S., Lu C., Zhou G. et al. Transparent YAG : Ce ceramics for WLEDs with high CRI : Ce 3+ concentration and sample thickness effects, Ceramics International, 2016, vol. 42, issue 6, pp 6935-6941. DOI: 10.1016/j.ceramint.2016.01.079.
5. Lago M.D., Meneghini M., Trivellin N. et al. Phosphors for LED-based light sources: thermal properties and reliability issues, Microelectronics Reliability, 2012, vol. 52, issue 9-10, pp 2164-2167. DOI: 10.1016/j.microrel.2012.06.036.
6. Zhao C., Duan Y., Lin H. et al. Synthesis and luminescence properties of color-tunable Ce, Mn co-doped LuAG transparent ceramics by sintering under atmospheric pressure, Ceramics International, 2020, vol. 47, issue 7, pp 9156-9163. DOI: 10.1016/j.ceramint.2020.12.040.
7. Kim H.T., Kim J.H., Lee J.-K. Kang Y.C. Green light-emitting Lu3Al5O12:Ce phosphor powders prepared by spray pyrolysis, Materials Research Bulletin, 2012, vol. 47, issue 6, pp 1428-1431. DOI: 10.1016/j.materresbull.2012.02.050.
8. Kravtsov A.A., Chikulina I.S., Vakalov D.S. et al. Issledovanie luminiscencii YAG:Ce, dopirovannogo nanochastitsami serebra [Luminescence of YAG:Ce doped with silver nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 220-227. DOI: 10.26456/pcascnn/2021.13.220. (In Russian).
9. Mares J.A., Beitlerova A., Nikl M. et al. Time development of scintillating response in Ce- or Pr-doped crystals, Physica Status Solidi (C), 2007, vol. 4, issue 3, pp 996-999. DOI: 10.1002/pssc.200673858.
10. Shi, Y., Zhao Y., Cao M. et al. Dense Ce3+ doped Lu3A15O12 ceramic scintillators with low sintering adds: Doping content effect, luminescence characterization and proton irradiation hardness, Journal of Luminescence, 2020, vol. 225, art. no. 117336, 7 p. DOI: 10.1016/j.jlumin.2020.117336.
11. Kim S., Yie H., Choi S. et al. Pore characteristics for improving luminous efficacy of phosphor-in-glass, Optics Express, 2015, vol. 23, issue 24, pp. A1499-A1511. DOI: 10.1364/OE.23.0A1499.
12. Bechtel H., Schmidt P., Busselt W., Schreinemacher B.S. Lumiramic: a new phosphor technology for high performance solid state light sources, Proceedings of SPIE, Eighth International Conference on Solid State Lighting, 2 September 2008, San Diego. 2008, vol. 7058, art. id. 70580E, 10 p. DOI: 10.1117/12.794941.
13. Powder Diffraction File JCPDS-ICDD PDF-2 (Set 1-47). (Release, 2016). Available at: www.url: https://www.icdd.com/pdf-2 (accessed 15.06.2023).
14. Kravtsov A.A., Chikulina I.S., Tarala V.A. et al. Nucleation and growth of YAG: Yb crystallites: A step towards the dispersity control, Ceramics International, 2020, vol. 46, issue 18, pp. 28585-28593. DOI: 10.1016/j.ceramint.2020.08.016.
15. Antonov D.A., Pavlov S.S., Makarov N.A. Korundovaya keramika dlya melyushchikh tel s ponizhennoj temperaturoj spekaniya [Аlumina ceramics for grinding bodies with lower sintering temperature], Sovremennye metody i tekhnologii sozdaniya i obrabotki materialov [Modern methods and technologies for the creation and processing of materials], 2018, vol. 1, pp 12-21. (In Russian).
16. Zhou C., Xie P., Chen Y. et al. Synthesis, sintering and characterization of porous nano-structured CaP bioceramics prepared by a two-step sintering method, Ceramics International, 2015, vol. 41, issue 3, pp 4696-4705. DOI: 10.1016/j.ceramint.2014.12.018.
17. Al-Aqeeli N., Saheb N., Laoui T., Mohammad K. The synthesis of nanostructured WC-based hardmetals using mechanical alloying and their direct consolidation, Journal of Nanomaterials, 2014, vol. 2014, art. id. 640750, 16 p. DOI: 10.1155/2014/640750.
18. Fang M.-H., Leano J.L., Liu R.-S. Control of narrow-band emission in the phosphor materials for the application in light-emitting diodes, ACS Energy Letters, 2018, vol. 3, issue 10, pp. 2573-2586. DOI: 10.1021/acsenergylett.8b01408.

⇐ Prevoius journal article | Content | Next journal article ⇒