Abstract: This paper presents the results of measuring the size of colloidal SiO2 particles by two methods – photon-correlation spectroscopy of dynamic light scattering and acoustic spectroscopy. Mathematical processing of experimental data using the software of the Photocor-Complex and DT-1202 spectrometers made it possible to obtain of the size distribution histograms for silicon dioxide colloidal particles in a standard sample. For the first time it has been established that the optimal parameters for measuring the size of colloidal SiO2 particles by the photon-correlation spectroscopy are the substance concentration less than 1 %, the photodetector position angle of 90 degrees and the number of measurements in a cycle of 100 – 150, and for the acoustic spectroscopy – 1 % substance concentration.
Keywords: photon correlation spectroscopy of dynamic light scattering, acoustic spectroscopy, colloidal particles
- Mariya A. Yasnaya – Ph. D., Assistant professor of the Department of Electronics and Nanotechnology of the Engineering Institute, North Caucasus Federal University
- Andrey V. Blinov – Senior Lecturer of the Department of Electronics and Nanotechnology of the Engineering Institute, North Caucasus Federal University
- Anastasiya A. Blinova – Ph. D., Assistant professor of the Department of Electronics and Nanotechnology of the Engineering Institute, North Caucasus Federal University
- Irina M. Shevchenko – Ph. D., Assistant professor of the Department of Electronics and Nanotechnology of the Engineering Institute, North Caucasus Federal University
- David G. Maglakelidze – student of the Department of Electronics and Nanotechnology of the Engineering Institute, North Caucasus Federal University
- Anna O. Senkova – student of the Department of Electronics and Nanotechnology of the Engineering Institute, North Caucasus Federal University
For citation:
Yasnaya M.A., Blinov A.V., Blinova A.A., Shevchenko I.M., Maglakelidze D.G., Senkova A.O. Opredelenie optimalnykh rezhimov izmereniya razmera kolloidnykh chastits metodami fotonno-korrelyatsionnoj i akusticheskoj spektroskopii [Determination of optimal modes for measuring the size of colloidal particles by photon-correlation spectroscopy and acoustic spectroscopy], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 232-242. DOI: 10.26456/pcascnn/2020.12.232. ⎘
Full article (in Russian): download PDF file
⇐ Prevoius journal article | Content | Next journal article ⇒