Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


The influence of surface and interphase characteristics on the behavior of the phase diagram of nanoparticles of the paladium-platinum alloy

L.P. Aref`eva1, I.G. Shebzukhova2

1 Don State Technical University
2 Kabardino-Balkarian State University named after H.M. Berbekov

DOI: 10.26456/pcascnn/2020.12.243

Original article

Abstract: The melting and crystallization temperatures have been calculated and the phase diagram of Pd – Pt metal particles of 10 nm in size has been constructed. The surface and interfacial energies, their temperature and size dependences were estimated by a modified electron-statistical method. It was found that the form of the phase diagram for Pd – Pt nanoparticles has significant differences from the diagram of bulk phases, including the melting-crystallization hysteresis.

Keywords: size effects, melting temperature, crystallization temperature, phase diagram, melting-crystallization hysteresis, binary nanoparticles, palladium-platinum system

  • Ludmila P. Aref`eva – Ph. D., Docent, Department of Physical and Applied Material Science, Don State Technical University
  • Irina G. Shebzukhova – Dr. Sc., Professor, Department of Theoretical and Experimental Physics, Kabardino-Balkarian State University named after H.M. Berbekov

For citation:

Aref`eva L.P., Shebzukhova I.G. Vliyanie poverkhnostnykh i mezhfaznykh kharakteristik na povedenie fazovoj diagrammy nanochastits splava palladij-platina [The influence of surface and interphase characteristics on the behavior of the phase diagram of nanoparticles of the paladium-platinum alloy], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 243-251. DOI: 10.26456/pcascnn/2020.12.243.

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒