Phase formation in contact layers during contact melting of copper and aluminum
Yu.N. Kasumov1, A.R. Manukyants1, V.A. Sozaev1, B.M. Khubolov2
1 North Caucasian Institute of Mining and Metallurgy (State Technological University)
2 Kabardino-Balkarian State University named after H.M. Berbekov
DOI: 10.26456/pcascnn/2020.12.120
Short communication
Abstract: In this work, an attempt is made to identify the features of the structure of contact layers during the contact melting of copper with aluminum brand AMG-2 (mass composition, %: Mg – 1,8 – 2,8, Mn – 0,2 –0,6, Cu – 0,1, Zn – 0,2, Fe – 0,4, Si – 0,4, rest – aluminum) and aluminum-lithium alloy (Al – 0,4 wt.% Li). The study of contact melting in the system is important for development of contact-reactive soldering technology, obtaining layered intermetallic composite materials, creating heat sinks for semiconductor devices, modeling dendrite formation. It was established that intermetallic compounds are formed in the contact layers, which affect the brittleness of copper-aluminum compounds and eutectic structures.
Keywords: contact melting, contact interaction, aluminium/copper system, euthetics, phase formation in contact layers
- Yuriy N. Kasumov – Ph. D., Docent of the Department of Physical and Mathematical disciplines, North Caucasian Institute of Mining and Metallurgy (State Technological University)
- Artur R. Manukyants – Ph. D., Docent of the Department of Physical and Mathematical disciplines, North Caucasian Institute of Mining and Metallurgy (State Technological University)
- Victor A. Sozaev – Dr. Sc., Professor of the Department of Physical and Mathematical disciplines, North Caucasian Institute of Mining and Metallurgy (State Technological University)
- Boris M. Khubolov – Ph. D., Leading Researcher of Management Research and Innovation Department, Head of the Laboratory of Electrochromic Materials, Department of Experimental and Theoretical Physics, Institute of Physics and Mathematics, Kabardino-Balkarian State University named after H.M. Berbekov
For citation:
Kasumov Yu.N., Manukyants A.R., Sozaev V.A., Khubolov B.M. Fazoobrazovanie v kontaktnykh proslojkakh, voznikayushchikh pri kontaktnom plavlenii medi i alyuminiya [Phase formation in contact layers during contact melting of copper and aluminum], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 120-127. DOI: 10.26456/pcascnn/2020.12.120. ⎘
Full article (in Russian): download PDF file
⇐ Prevoius journal article | Content | Next journal article ⇒