The size dependencies of properties of Mo-W alloy of equiatomic composition
S.P. Kramynin
Institute of Physics named after H.I. Amirkhanova – subdivision of Dagestan Federal Research Center of the Russian Academy of Sciences
DOI: 10.26456/pcascnn/2020.12.128
Original article
Abstract: Based on the parameters of the Mie–Lennard-Jones pair-wised potential of the interatomic interaction for Mo and W, the potential parameters for an equiatomic Mo – W substitution alloy were calculated. Size dependences for the equation of state, modulus of elasticity, coefficient of thermal expansion, isobaric heat capacity, surface energy and surface energy temperature derivative were obtained. Temperature dependencies of coefficient of thermal expansion and isobaric heat capacity for macro- and nano-crystals of Mo – W alloy were also obtained.
Keywords: tungsten, molybdenum, nanocrystal, alloy, size dependences, equation of state, surface energy
- Sergey P. Kramynin – Junior Researcher, Institute of Physics named after H.I. Amirkhanova – subdivision of Dagestan Federal Research Center of the Russian Academy of Sciences
For citation:
Kramynin S.P. Razmernye zavisimosti svojstv splava Mo-W [The size dependencies of properties of Mo-W alloy of equiatomic composition], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 128-135. DOI: 10.26456/pcascnn/2020.12.128. ⎘
Full article (in Russian): download PDF file