PhC-2018
Comparison of the ζ-potential measuring methods accuracy for the colloidal particles
Comparison of the ζ-potential measuring methods accuracy for the colloidal particles A.V. Blinov, Yu.Yu. Snezhkova, M.A. Yasnaya, O.A. Dyudyun, Y.V. Kaznacheev, I.M. Shevchenko North-Caucasian Federal University DOI: 10.26456/pcascnn/2018.10.115 Abstract: The study is devoted to the choice of an optimal method for determining the ζ-potential of colloidal ...
Fhase forming and structural feature twu-layer coating «titanium/nichrome» on artificial polycrystalline diamonds
Fhase forming and structural feature twu-layer coating «titanium/nichrome» on artificial polycrystalline diamonds Z.Zh. Berov, A.R. Manukyants, Y.N. Kasumov, V.A. Sozaev Kabardino-Balkarian State University named after H.M. Berbekov North Caucasian Institute of Mining and Metallurgy (State Technological University) DOI: 10.26456/pcascnn/2018.10.106 Abstract: The phase forming and the ...
Application of the method of field desorption of sodium for studying carbon nanostructures on the surface of rhenium field emitter
Application of the method of field desorption of sodium for studying carbon nanostructures on the surface of rhenium field emitter D.P. Bernatskii, V.G Pavlov Ioffe Institute DOI: 10.26456/pcascnn/2018.10.099 Abstract: Field desorption microscopy was used to study the surface of the rhenium field emitter after its ...
The effect of carbon on the diffusion of cesium on the renium surface
The effect of carbon on the diffusion of cesium on the renium surface D.P. Bernatskii, V.G. Pavlov Ioffe Institute DOI: 10.26456/pcascnn/2018.10.093 Abstract: The diffusion of cesium over the rhenium surface and the rhenium surface coated with carbon was studied by methods of the field electron ...
Solid state wetting and dynamics of solid surface nanorelief
A.G. Bembel, I.V. Talyzin, V.M. Samsonov Tver State University DOI: 10.26456/pcascnn/2018.10.083 Abstract: Using molecular dynamics solid state wetting in the Cu (nanoparticle) / Cu (substrate) system was studied. It has been found that the solid state spreading mechanism corresponds, first of all, to the surface diffusion ...
Peculiarities of structural variations at crystallization of highly filled composites on polymeric basis
B.K. Barakhtin, R.V. Sedletsky Saint Petersburg State Marine Technical University Central Research Institute of Structural Materials «Prometey» named by I.V. Gorynin of National Research Center «Kurchatov Institute» DOI: 10.26456/pcascnn/2018.10.073 Abstract: Composite samples with polymer matrixes of different compositions are investigated. The volume fraction carbon fillings of ...
Computer simulation of the Cu@Si core-shell nanoparticles formation
V.S. Baidyshev N.F. Katanov Khakas State University DOI: 10.26456/pcascnn/2018.10.064 Abstract: In this work computer simulation of the condensation processes of Cu-Si core-shell nanoparticles was performed by the molecular dynamics method. It was shown that simultaneous cooling of atomic vapors of copper and silicon leads to ...
Gold nanocrystal properties dependence on size and shape at isobaric conditions
E.N. Akhmedov Institute for Geothermal Research of the Dagestan Scientific Center of RAS DOI: 10.26456/pcascnn/2018.10.053 Abstract: Using the nanocrystal RP-model, the state equation of a gold was calculated. On the basis of this equation the isobaric dependence of the melting temperature on the size and ...
Modern methods of granulometric analysis of dusted materials containing nanoparticles
A.Yu. Ataeva, G.I. Sverdlik, D.A. Kambolov, A.R. Ataev North Caucasian Institute of Mining and Metallurgy (State Technological University) DOI: 10.26456/pcascnn/2018.10.044 Abstract: In the work the differential and integral distribution of particles of dolomite flour and wings of zinc-containing welsh furnaces by size was studied by ...
The interfacial energy of metalic thin films on the boundary with liquid polar dielectric
L.P. Aref`eva, I.G. Shebzukhova Don State Technical University Kabardino-Balkarian State University named after H.M. Berbekov DOI: 10.26456/pcascnn/2018.10.035 Abstract: Expressions have been obtained for estimating the interfacial energy of metallic thin films at the interface with an organic dielectric coating. The case of the boundary of ...