Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Domain structure and magnetic transport properties on thin ferrite-garnet films

R.M. Eguzhokova, A.I. Ivanova, E.M. Semenova

Tver State University, Tver, Russia

DOI: 10.26456/pcascnn/2019.11.123

Abstract: This article provides an overview of the results of an experiment on the application of the magnetotransport properties of ferrite – garnet films in microfluidic devices, as well as on the determination of the composition of immunomagnetic microspheres. The article provides practical recommendations on the use of ferrite garnet films for the controlled transport of magnetic microspheres.

Keywords: ferrite-garnet films, magnetic microspheres, magnetic manipulation.

Bibliography link:

Eguzhokova, R.M. Domain structure and magnetic transport properties on thin ferrite-garnet films / R.M. Eguzhokova, A.I. Ivanova, E.M. Semenova // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2019. – I. 11. – P. 123-128.

Full text (in Russian): download PDF file