Simulation of the maturation process cystein-silver solution

M.D. Malyshev1, P.O. Baburkin1, A.N. Adamyan1, P.M. Pakhomov1, P.V. Komarov1,2
1Tver State University
2A.N. Nesmeyanov Institute of Organoelement Compounds of Russian Academy of Sciences

DOI: 10.26456/pcascnn/2018.10.453

Abstract: In this paper, the process of maturation of an aqueous solution of L-cysteine and silver nitrate using the method of atomistic molecular dynamics is investigated. To study the maturation process, an atomistic model of the solution was developed. The study allowed to obtain new data on the structure of silver mercaptide clusters and the role of their structural features in the process of further self-organization.
Keywords: hydrogel, supramonomer, computer simulation, atomistic model.

Bibliography link:
Malyshev, M.D. Simulation of the maturation process cystein-silver solution / M.D. Malyshev, P.O. Baburkin, A.N. Adamyan et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 453-459.