Niobium-containing barium titanate crystals switching processes

N.N. Bolshakova, О.V. Bolshakova, V.V. Ivanov, T.I. Ivanova, E.M. Semenova
Tver State University

DOI: 10.26456/pcascnn/2018.10.169

Abstract: The results of research of the processes of polarization of niobium-containing crystals of barium titanate in changing electric fields are presented. It has been established that the time for reorganization of the ferroelastic domain structure is 30-40 times shorter than the switching time of the total polarization of the crystal, which indicates that the main switching time of BaTiO: Nb5+ crystals is determined by the change in its ferroelectric 180° domain structure.
Keywords: processes of switching, domain structure, barium titanate, polarization-optical method, Barkhausen effect.

Bibliography link:
Bolshakova, N.N. Niobium-containing barium titanate crystals switching processes / N.N. Bolshakova, О.V. Bolshakova, V.V. Ivanov et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 169-177.

Full text (in Russian): download PDF file