Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Lubricating oils on the basis of nanoliquids

A.N. Bolotov, V.V. Novikov, O.O. Novikova
Tver State Technical University

DOI: 10.26456/pcascnn/2018.10.159

Abstract: We established applicability of dispersed medium based on diesters of carbonic acids for production the low-viscosity magnetic oil of new generation. It was shown unusual approach to select surfactant-stabilizer for colloidal structure of oils considering their dielectric properties and friction effects. It was submitted the preselection findings of the additions and fillers for magnetic oil which are characterized by the different mechanism of reducing friction.
Keywords: magnetic lubricating oil, friction, wear, lubricant, dispersed medium, dispersed phase, antifriction and wearproof additives.

Bibliography link:
Bolotov, A.N. Lubricating oils on the basis of nanoliquids / A.N. Bolotov, V.V. Novikov, O.O. Novikova // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 159-168.

Full text (in Russian): download PDF file