Investigation of mechanical properties of silicene In a central force field model

Y.E. Nagorny, D.N. Politaev
Belarusian State University

DOI: 10.26456/pcascnn/2017.9.341

Abstract: Numerical simulation of mechanical behaviour of graphene and silicene are made in the central forces field model approximation. Dependences of Young’s modulus and Poisson’s ratio are obtained from the sample sizes. Comparison of results is carried out.
Keywords: central force field, graphene, silicene, Young’s modulus, Poisson’s ratio.

Bibliography link:
Nagorny, Y.E. Investigation of mechanical properties of silicene In a central force field model / Y.E. Nagorny, D.N. Politaev // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2017. – I. 9. – P. 341-346.