Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials
Founded at 2009


Formation of fases at the boundary of the double-layer copper-aluminium film

K.M. Elekoeva1, P.K. Korotkov1, M.Z. Laipanov2, A.R. Manukyants1, V.A. Sozaev1,3, B.M. Khubolov3
1North Caucasian Institute of Mining and Metallurgy (State Technological University)
2Karachaevo-Cherkessky State University named after U.D. Aliev
3Kabardino-Balkarian State University named after H.M. Berbekov

DOI: 10.26456/pcascnn/2017.9.182

Abstract: Outcomes of formation of phases are reduced at the contact melting of recordings of aluminium with copper. With the help of a raster electronic, atomic – force microscopy and X-ray analysis the eutecticum and intermetallic AlCu4 phases are detected.
Keywords: phase forming, contact melting, intermetallides.

Bibliography link:
Elekoeva, K.M. Formation of fases at the boundary of the double-layer copper-aluminium film / K.M. Elekoeva, P.K. Korotkov, M.Z. Laipanov et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2017. – I. 9. – P. 182-188.

Full text (in Russian): download pdf file