Aleksandrov V.D., Amerkhanova Sh.K., Postnikov V.A., Sobolev A.Yu., Sobol O.V.
ANALYSIS OF FUSION AND CRYSTALLIZATION PROCESSES OF CRYSTALLINE HYDRATES ON BASIS OF FUSIBILITY THERMOGRAMS – page 5
Aleksandrov V.D., Amerhanova Sh.K., Pokyntelytsia O.A., Pokyntelytsia A.Ye.
NOVEL ORGANIC HEAT STORAGE MATERIALS BASED ON PHASE TRANSFORMATIONS – page 16
Anokhin E.O., Trusov L.A., Vasiliev A.V., Gorbachev E.A., Eliseev A.A., Kazin P.E.
STUDY OF THE STABILITY OF AQUEOUS COLLOIDS BASED ON HARD-MAGNETIC STRONTIUM HEXAFERRITE NANOPARTICLES – page 22
Antonov A.S., Mikhailova (Zonova) O.V., Sdobnyakov N.Yu., Sokolov D.N., Ivanov D.V.
SCANNING TUNNELING MICROSCOPY FOR THE NANOCOATING «SILVER/MICA»: RELIEF MORPHOLOGY AND ELECTRICAL CHARACTERISTICS – page 31
Apekov A.M., Shebzukhova I.G.
DEPENDENCE OF INTERFACIAL ENERGY OF ALKALI METALS BOUNDING TO HEXANE ON ORIENTATION AND ATOMIC NUMBER OF ELEMENT – page 47
Aref`eva L.P., Shebzuhova I.G.
ANISOTROPY OF WORK FUNCTION OF BCC 4D AND 5D METALS – page 52
Ahkubekov A.A., Korotkov P.K., Manukyants A.R., Ponegev M.Kh., Sozaev V.A.
THE CONTACT MELTING OF COPPER WITH ALUMINUM – page 59
Baburkin P.O.
SIMULATION OF SYNTHESIS AND COLLAPSE OF AB AMPHIPHILIC COPOLYMER WITH THE NUCLEATING HYDROPHOBIC BLOCK – page 63
Bazzal Kh., Fadaijan A.R., Voropay E.S., Zajogin A.P.
INVESTIGATION OF ALUMINUM NITRIDE FORMATION PROCESSES IN PLASMA WHEN THE ALUMINUM ALLOY D16T IS SUBJECTED TO THE EFFECT OF DOUBLE LASER PULSES IN THE AIR – page 70
Baidishev V.S., Gafner Yu.Ya., Kartavych E.A.
MOLECULAR DYNAMICS STUDY OF THE KINETICS OF CuAu CLUSTERS FORMATION IN THE CONDENSATION PROCESS FROM HIGH TEMPERATURE GASEOUS PHASE – page 76
Barakhtin B.K., Vysockaya M.A.
THE STRUCTURE SYSTEM ANALYSIS APPLICATION FOR OPTIMIZATION OF STILLWELDING REGIMES – page 83
Batin V.V., Pan’kin N.A.
CREATING A HEAT SINK METAL-COMPOSITE MATERIAL – page 97
Baturkin S.A.
ON PROSPECTS OF PRODUCTION AND APPLICATION OF AMORPHOUS CHALCOGENIDE FILMS GeSbTe – page 101
Belenkov E.A., Tingaev M.I.
Structure of sp2+sp3 hybrid phases resulting from carbon nanotubes – page 111
Belenkova T.E., Chernov V.M.
STRUCTURE AND ELECTRONIC PROPERTIES OF Α-GRAPHYNE, WHICH CAN BE OBTAINED BY L4-8 GRAPHENE – page 117
Blinov A.V., Kravtsov A.A., Jasnaja M.A., Rusanov A.Yu., Momot E.V.
INFLUENCE OF TEMPERATURE TREATMENT ON THE STRUCTURE AND COMPOSITION OF NANOSIZED ZnO, OBTAINED BY SOL-GEL METHOD – page 123
Bogdanova A.E., Skachkov V.M., Shirokova A.G., Sabirzyanov N.A.
EVALUATION OF BIOACTIVE COATING DURABILITY ON THE TITANIUM OF VARIOUS POROSITY – page 130
Bolotov A.N., Burdo G.B., Novikov V.V., Novikova O.O.
THE INFLUENCE OF THE MAGNETIC FIELD ON THE LUBRICATING PROPERTIES OF THE NANOSTRUCTURED MAGNETIC OIL – page 137
Brylkin Yu.V., Kusov A.L.
RESEARCH OF THE DEPENDENCE OF SURFACE PHYSICAL PROPERTIES FROM THE FRACTAL DIMENSION – page 142
Buldakova L.Yu., Gyrdasova O.I., Krasil’nikov V.N., Baklanova I.V., Yanchenko M.Yu.
SPECTRAL AND VOLTAMMETRIC CHARACTERISTICS OF NANOSTRUCTURED ZnO – page 150
Voropaev S.A., Dushenko N.V., Aronin A.S., Shkinev V.M., Galimov E.M.
STUDY ON THE POSSIBILITY OF DOPING WITH NITROGEN AND SILICON CAVITATION NANODIAMONDS – page 158
Voskresensky V.M., Starodub O.R., Sidorov N.V., Palatnikov M.N.
RESEARCH OF CLUSTER FORMATION IN CRYSTALS OF LITHIUM NIOBATE BY COMPUTER MODELING METHOD – page 165
Greshnyakov V.A., Belenkov E.A.
CRYSTALLINE STRUCTURE AND PROPERTIES OF LA7 DIAMOND-LIKE PHASE – page 174
Grigorov I.G., Shirokova A.G., Bogdanova E.A., Skachkov V.M., Borisov S.V., Sabirzyanov N.A.
SEM STUDY OF THE MICROSTRUCTURE OF BIOCOMPOSITES BASED ON HIGHLY POROUS HONEYCOMB MATERIALS – page 179
Davydova I.M., Мelnik T.N., Yurchenko V.M.
EFFECT OF LATERAL INTERACTION ON THE IMPURITY SEGREGATION IN FILMS – page 186
Dikusar A.E., Pushkarchuk A.L., Potkin V.I., Kilin S.Ya., Soldatov A.G., Kuten S.A., Khmelevskiy A.N., Babichev L.F.
QUANTUM CHEMICAL DESIGNING OF ENDOHEDRAL CONTAINING INDIUM DERIVATIVES OF BUCKMINSTERFULLERENE C60 AND C70 FOR DEVELOPMENT RADIONUCLIDE NANOSIZED AGENTS THAT DESTROY A TUMOR – page 193
Zurkhaeva O.S., Zurkhaev D.S., Aref`eva L.P.
INVESTIGATION OF INFLUENCE OF SCANNING STEP ON IR-TRANMISSION SPECTRA OF NITRIDE ALUMINUM FILMS – page 208
Ivanov V.I., Simakov S.R.
A HOLOGRAPHIC SENSITIVITY OF THE NANOHETEROGENEOUS MEDIUM WITH A BLURRED PHASE TRANSITION – page 216
Ivanov V.I.
NONEQUILIBRIUM CURRENTS IN THIN-LAYER METAL-FERROELECTRIC-METAL SANDWICH STRUCTURE – page 220
Ivanov Yu.F., Laskovnev A.P., Teresov A.D., Cherenda N.N., Uglov V.V., Petrikova E.A., Astashinskaya M.V., Koval N.N.
MODIFICATION OF SURFACE LAYER OF HYPEREUTECTIC SILUMIN BY HIGHINTENSITY PULSED ELECTRON BEAM – page 225
Ivanov Yu.F., Klopotov A.A., Dedov N.V., Popova N.A.
STRUCTURAL PHASE STATES OF Cu-Zn-Al ALLOY POWDERS PRODUCED BY HF–PLASMA-CHEMICAL DENITRATION – page 232
Izmailov V.V., Gusev A.F., Novoselova M.V.
THE INFLUENCE OF THIN FATTY ACID FILMS ON TRIBOLOGICAL PROPERTIES OF A DISCRETE CONTACT OF METAL SURFACES – page 242
Il`ves V.G., Sokovnin S.Yu., Khrustov V.R., Zayats S.V., Pryanichnikov S.V., Zuev M.G.
PROPERTIES OF ZnO CERAMICS SINTERED FROM NANOPOWDERS ZnO-Zn , OBTAINED PULSED ELECTRON EVAPORATION – page 249
Kalazhokov Z.Kh., Kalazhokov Z.Kh., Kalazhokov Kh.Kh., Reutskaya N.S., Kardanova Z.V., Sherieva E.Kh.
THE CALCULATION OF SURFACE THERMODINAMICAL PARAMETERS FOR BINARY ALLOYS OF METALLIC SYSTEM – page 257
Karmokov A.M., Molokanov O.A., Shomakhov Z.V.
THE ELECTRO-PHYSICAL PROPERTIES OF A SPECIAL GLASS ELECTRONIC ENGINEERINGS – page 263
Kidyarov V.I.
SYSTEMATIC COMPARISON OF THE SOLUBILITY AND SUPERSOLUBILITY ON THE BASE OF THE SALT DIMENSIONAL FACTORS – page 270
Kirjushina S.I., Mjagotin A.V.
A NONLINEAR OPTICAL DIAGNOSTICS OF NANO-LIQUIDES – page 280
Knatko M.V., Lapushkin M.N.
EFFECT OF ELECTRIC FIELD ON PROCESSES IN SEMICONDUCTOR NaAuy FILM – page 284
Kolosov A.Yu., Sokolov D.N., Sdobnyakov N.Yu., Komarov P.V., Bogdanov S.S., Bogatov A.A.
METALS COALESCENCE AS A MECHANISM FOR NANOSOLDERING: SEARCHING STABLE CONFIGURATIONS – page 292
Komarov P.V., Ivanov V.A.
THE DEVELOPMENT OF CORSEGRAINED MODEL OF ALUMINOSILICATE HALLOYSITE NANOTUBES – page 302
Koroleva L.F.
WAVE NATURE OF THE SYNTHESIS REACTIONS OF DOPED CALCIUM CARBONATEPHOSPHATES AS ACTIVE BIOMATERIAL FOR OSTEOGENESIS – page 311
Kochengin A.E., Belenkov E.A.
SCHEME FOR OBTAINING POLYMORPHOUS MODIFICATIONS OF GRAPHENE FROM CARBYNE CHAINS – page 316
Krut’ko V.K., Kulak A.I., Musskaya O.N.
ELECTROCHEMICAL DEPOSITION OF APATITE-POLYMER COATINGS ON TITANIUM SURFACE – page 322
Krylov V.I., Ivanova G.D., Khe V.K.
THE LIGHT INDUCED PSEUDO-PRISM METHOD IN NANOFLUID – page 329
Kuznetsov Yu.A., Lapushkin M.N.
ELECTRON-STIMULATED DESORPTION OF CESIUM ATOMS ADSORBED ON GOLD SURFACE – page 333
Kurbanova E.D., Polukhin V.A., Mitrofanova N.S., Rigmant L.K.
SIMULATION OF COORDINATION TRANSFORMATION AND ATOMIC DYNAMICS OF LOW DIMENSIONAL SYSTEMS REINFORCED Cu,Ru,Ru-Pd FILMS GRAPHENE – page 341
Lyuev V.K., Lyuev I.V.
THE TEMPERATURE DEPENDENCE OF THE SURFACE POTENTIAL OF p-TYPE MONOCRYSTALLINE SILICON – page 350
Lyuev V.K., Lyuev I.V.
INFLUENCE OF CHEMICAL TREATMENT AND THE TEMPERATURE ON THE SURFACE POTENTIAL OF THE MONOCRYSTALLINE SILICON KDB -10 (111) – page 354
Magomedov M.N.
ON THE DEPENDENCIES OF THE MELTING PARAMETERS VERSUS NUMBER OF ATOMS IN THE SILICON NANOCRYSTAL – page 358
Markaryan E.S.
THE PROCESSES OF OBTAINING «COMPLEX» FILMS ON ALUMINUM – page 367
Myasnichenko V.S., Ershov P.M., Sdobnyakov N.Yu., Sokolov D.N.
ON THE RELATIONSHIP BETWEEN STRUCTURE AND THERMAL STABILITY PROPERTIES OF COPPER CLUSTERS SIZE UP TO 100 ATOMS IN MOLECULAR-DYNAMICS SIMULATION – page 378
Nagaplezheva R.R., Karmokov A.M., Nagoev B.N., Uyanaeva M.M., Luev V.K.
EFFECT OF PLASMA TREATMENT ON THE SURFACE COMPOSITION OF SAPPHIRE – page 387
Nilov D.Yu.
A graph model of the enthalpy of formation calculation for alkanes C11H24 with respect of multiple non-valence interactions in three atoms along the chain – page 391
Palatnikov M.N., Shcherbina O.B., Sidorov N.V., Drogobuzhskaya S.V.
MODIFICATION OF LITHIUM TANTALATE CRYSTALS BY HIGH-TEMPERATURE TREATMENT OF VTE – page 393
Repchenkov V.I., Nagorny Y.E., Akavity A.V.
DISCRETE MODELING AT THE ATOMIC-MOLECULAR LEVEL OF MECHANICAL PROCESSES IN NANOCOMPOSITES – page 400
Samsonov V.M., Vasilyev S.A., Bembel A.G.
MOLECULAR DYNAMICS MODEL OF THE TECHNOLOGY OF AMORPHOUS METAL FILMS PRODUCTION BY CONDENSATION ON THE COOLED SUBSTRATE – page 407
Samsonov V.M.
ON ALTERNATIVE APPROACHES TO DETERMINATION OF RADIUS AND OTHER GEOMETRIC CHARACTERISTICS OF NANOPARTICLES – page 413
Samsonov M.V., Samsonov V.M.
ON BOUNDARY WETTING CONDITIONS FOR ROUGH SOLID SURFACE – page 425
Sdobnyakov N.Yu., Samsonov V.M., Bazulev A.N., Novozhilova D.A.
EVALUATION OF THE PROPORTIANALITY COEFFICIENT IN RUSANOV`S FORMULA FOR THE SURFACE TENSION ON THE BASIS OF COMPUTER SIMULATION OF NANOPARTICLES – page 431
Sdobnyakov N.Yu., Novozhilov N.V., Antonov A.S., Voronova E.A., Mikhailova O.V.
ON THE TECHNIQUE OF THE EVALUATION OF THICKNESS DEPENDENCES OF REFRACTIVE INDEX FOR NANOSIZED LIQUID FILMS BY ELLIPSOMETRIC METHOD – page 444
Selemeneva D.G., Kravtsov A.A., Blinov A.V., Jasnaja M.A.
INFLUENCE OF CALCINATION TEMPERATURE ON STRUCTURAL CHANGES OF NANOSIZED ZIRCONIA – page 450
Semenova E.M., Lyakhova M.B., Ivanova A.I., Lukin A.A., Kuznetsova Yu.V., Karpenkov D.Yu.
STUDY ON THE MICRO- AND NANOSTRUCTURE OF NdPrGdDyTbFeCoBAl PERMANENT MAGNETS – page 456
Skachkov V.M., Yatsenko S.P., Pasechnik L.A., Sabirzyanov N.A.
EFFECT OF SOLID COMPONENT OF DIFFUSION-HARDENING SOLDERS ON PROPERTIES OF CONNECTING LAYER – page 463
Smirnov A.V., Gorbachev I.A., Sinev I.V.
EFFECT OF THE CONTENT TUNGSTEN ON THE MECHANICAL PROPERTIES AND THERMAL STABILITY OF COMPOSITE MATERIAL BASED ON POLYSTYRENE. – page 471
Startsev Yu.K.
THE CHANGING OF GLASS PROPERTY SURFACE LAYERS, PROCESSED IN MELT SALT – page 479
Startsev Yu.K.
Phenomenological description of vitrification and structural relaxation processes – page 494
Umreiko D.S., Komyak A.I., Vileishikova E.V., Zajogin A.P.
INVESTIGATION OF THE FORMATION PROCESSES OF URANIUM AND ALUMINUM OXIDES NANOCLUSTERS ON THE SURFACE OF OXIDIZED ALUMNUM USING DOUBLE LASER PULSES – page 505
Umreiko D.S., Komyak A.I., Vileishikova E.V., Zajogin A.P.
THE EFFECT OF CALCIUM NITRATE ON THE PHOTOCHEMICAL FORMATION PROCESSES OF URANIUM NANOCLUSTERS IN THE SOLUTIONS OF URANYL PERCHLORATE IN ACETONE – page 509
Chepkasov I.V.
CHANGING THE SHAPE AND STRUCTURE OF COPPER NANOCLUSTERS SYNTHESIZED FROM THE GAS PHASE – page 515
Shama M.S., Kravtsov A.A., Blinov A.V., Jasnaja M.A., Selemeneva D.G.
SYNTHESIS AND STUDYING OF ACID-BASE PROPERTIES OF TiO -Ag 2 NANOCOMPOSITE – page 519
Shepelevich V.G.
STRUCTURE, MICROHARDNESS AND THERMAL STABILITY OF RAPIDLY SOLIDIFIED Bi31Sn34Pb35 ALLOY – page 527
Shimanovich D.L.
CONSTRUCTIVELY TECHNOLOGICAL PRINCIPLES OF CAPACITIVE HUMIDITY SENSING Al2O3 NANOSTRUCTURES AND SENSITIVE PARAMETERS STUDY – page 533
Esser A.A., Myasnichenko V.S., Myasnichenko L.A., Sdobnyakov N.Yu.
Modelling of the copper cluster’s growth: topological description, stability and occurrence in intermetallics – page 541
Yurov V.M.
THE SIZE DEPENDENCE OF SURFACE TENSION AND HOMOGENEOUS NUCLEATION OF CRYSTALS – page 548