Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Articles archive – Issue 16 (2024)


1. EXPERIMENTAL STUDIES OF NANOPARTICLES, NANOSYSTEMS, AND NANOMATERIALS – page 7

Antonov A.S., Sdobnyakov N.Yu., Anofriev V.A., Afanasiev M.S., Semenova E.M., Makaev V.V.
Comprehensive approach to studying fractal structures on iron surfaces – page 7

Akhmatov Z.A., Khokonov A.Kh., Sergeev I.N., Ambartsumov M.G.
Study of potassium intercalated graphite by Raman spectroscopy – page 24

Barabanova E.V., Ospelnikov N.M., Ivanova A.I.
Effect of Bi-doping on the electrophysical properties of sodium niobate solid solutions – page 33

Bezverkhniy V.P., Gagarina A.Y., Muratova E.N., Maximov A.I., Moshnikov V.A.
Investigation of optical properties of metal-doped CsPbX3 perovskite nanocrystals – page 41

Bobreva L.A., Titov R.A., Smirnov M.V., Biryukova I.V., Masloboeva S.M., Pyatyshev A.Yu., Sidorov N.V., Palatnikov M.N.
Comparative studies of structural features of LiNbO3:Er:Zn crystals of different genesis – page 48

Bobreva L.A., Titov R.A., Smirnov M.V., Biryukova I.V., Masloboeva S.M., Pyatyshev A.Yu., Palatnikova O.V., Sidorov N.V., Palatnikov M.N.
Comparative studies of photoluminescent and optical properties, concentration of OH– groups in double-doped LiNbO3: Er:Zn crystals – page 60

Bolshakova N.N., Ivanova A.I., Druginina N.Yu., Semenova E.M., Schipilov S.S.
Switching processes in alanine doped triglycine sulfate crystals – page 72

Guseva A.M., Sinkevich A.I., Smetannikova S.D., Semenova E.M., Pastushenkov Yu.G.
Analysis of domain structure parameters of RFe11Ti (R = Y, Gd, Ho, Er) single crystals based on magnetic force microscopy data – page 85

Dunaeva G.G., Karpenkov A.Yu.
Towards the investigation of the magnetization processes of uniaxial magnetic materials by means of the analysis of transformation of their domain structure: experiment and computer modeling – page 96

Zernitsa D.A., Shepelevich V.G.
Structural features and properties of the Sn-Zn-Si-Al system alloys obtained by the method of rapid solidification from the melt – page 110

Zigert A.D., Kuz`min N.B., Semenova E.M., Karpenkov A.Yu., Ivanova A.I., Sdobnyakov N.Yu.
Correlation of magnetic characteristics and fractal dimension of magneto-optical images of permanent magnets – page 119

Ivanov V.I., Myagotin A.V.
Тhe holographic method for diagnostics of nanoparticles in dense nanosuspensions – page 128

Ivanov V.I., Egorshin I.N.
A modulation method of light-induced pseudo-prism in nanosuspension – page 134

Ivanov Yu.F., Akhmadeev Yu.Kh., Klopotov A.A., Prokopenko N.A., Petrikova E.A., Krysina O.V., Shugurov V.V., Shmakov A.N., Lavrov V.Yu.
X-ray diffraction studies of the growth process of thin films of high-entropy TiNbZrTaHfCu alloy in situ using synchrotron radiation – page 140

Ivanova A.I., Dudilovskaya A.V., Zhuravlev O.E., Kaphtanov A.D.
Application of ionic liquids in scanning electron microscopy studies of dielectric microstructure – page 154

Kabirov Yu.V., Utoplov A.A., Lyanguzov N.V., Sidorenko E.N., Prutsakova N.V., Chebanova E.V.
Thermopower of magnetoresistive composites based on La0,7Sr0,3MnO3 – page 164

Kislova I.L., Kiselev D.A., Kholkin A.L., Solnyshkin A.V., Muhin O.A., Kolkov G.G.
Features of the dynamic pyroelectric response and the local domain structure in PZN-PT crystals – page 171

Kozhevnikova N.S., Bogdanova E.A., Skachkov V.M., Baklanova I.V., Tyutyunnik A.P., Buldakova L.Yu., Yanchenko M.Yu., Yushkov A.A.
Ex-situ modification of nanostructured hydroxyapatite by colloidal CdS particles – page 183

Kravchenko D.A., Kolosov A.Yu., Sokolov D.N., Nepsha N.I., Bogdanov S.S., Sdobnyakov N.Yu.
An integrated approach to studying the structure of ternary CoCrMo alloy: scanning electron microscopy and atomistic simulation – page 198

Lapushkin M.N.
Adsorption of barium on surface of GaN(0001) – page 210

Mamaev D.V., Malyshkina O.V., Ivanova A.I.
Porous ceramics of sodium potassium niobate system – page 219

Medyanik E.V., Malyavin F.F., Lapin V.A., Kravtsov A.A., Suprunchuk V.E., Tarala L.V.
Study of the influence of sintering additives and vacuum sintering conditions on optical properties of LuAG:Er (1 at.%) ceramics – page 229

Novik O.D., Gavrilova N.D., Malyshkina O.V.
Low-frequency impedance spectroscopy of polymers and crystals with a hydrogen-bond network. Quantum collective excitations of nuclei in molecules – page 239

Rakunov P.A., Lyakhova M.B., Semenova E.M., Karpenkov A.Yu.
Magnetic properties and magnetic reversal processes of the Sm-Gd-Zr-Co-Cu-Fe alloys – page 258

Salomatina A.Yu., Fedotov A.Yu., Severyukhina O.Yu., Vinogradov F.A.
Study of Co-Fe nanocomposite magnetic properties – page 267

Sidorov N.V., Bobreva L.A., Palatnikov M.N., Pyatyshev A.Yu., Tarabrin M.K., Bushunov A.A.
Features of the defect structure of LiNbO3:Cu crystals and their manifestation in the IR absorption spectrum in the region of stretching vibrations of hydrogen atoms OН– -group – page 277

Staritsyn M.V., Pronin V.P., Khinich I.I., Krushelnitsky A.N., Senkevich S.V., Kaptelov E.Y., Pronin I.P.
Effect of electron channeling in the crystal lattice of radiant spherulites – page 289

Teplyakova N.A., Sidorov N.V., Palatnikov M.N.
Clusters in the structure of non-stochiometric lithium niobate crystals – page 300

Utoplov A.A., Prutsakova N.V., Rudskaya A.G., Nazarenko A.V., Belokobylsky M.V., Kabirov Yu.V.
Magnetoresistance of LSMO/(Cu2O, Ag) composites – page 307

2. THE THEORY OF NANOSYSTEMS – page 318

Apekov A.M., Shebzukhova I.G., Khamukova L.A.
Interphace energy of aluminum crystals at the boundary with nonpolar organic liquids – page 318

Belavin V.O., Brylkin Yu.V., Zaletaev S.V., Kusov A.L., Pavlikov V.V., Potapov A.A., Tsarkova V.A.
Problems of quantitative assessment of the friction couple contact area – page 327

Belyaeva I.N., Korsunov N.I., Chekanov N.A., Chekanov A.N.
Calculation of the spectrum of a gallium arsenide semiconductor with a triangular potential function by the power series method – page 337

Golov D.O., Petrov N.A., Tsirulev A.N.
Variational quantum algorithm for low-dimensional systems in the Pauli basis – page 343

Ionin V.V., Mikhalevsky V.A., Burtsev A.A., Kiselev A.V., Nevzorov A.A., Eliseev N.N., Lotin A.A.
Modelling of radiation propagation in a photonic integrated circuit based on a polymer waveguide and phasechange material nanoparticles – page 351

Kolosov A.Yu., Veresov S.A., Serov S.V., Sokolov D.N., Savina K.G., Grigoryev R.E., Sdobnyakov N.Yu.
Size effect in four-component Au-Cu-Pd-Pt nanoparticles and their stability – page 361

Magomedov R.A., Akhmedov E.V.
Calculation of state equation isobars of carbon dioxide and methane in pressure interval from 2 to 20 MPa – page 373

Malyshkin Yu.A.
Geometric preferential attachment with choice-based edge step – page 381

Samsonov V.M., Talyzin I.V., Zhigunov D.V.
Segregation of components as a necessary condition for the eutectic nature of an alloy and nanoalloy – page 387

Sdobnyakov N.Yu., Kolosov A.Yu., Sokolov D.N., Savina K.G., Nepsha N.I., Savel’ev Ya.P., Lomonosov G.D.
To the problem of tight binding potential parameters approbation: influence of the ratio between pair and many-body interaction on the process of the structure formation in binary Pd-Pt nanoparticles – page 399

Tvardovskiy A.V.
Model prerequisites for derivation of the Dubinin-Radzhdkevich adsorption equation – page 409

Tvardovskiy A.V.
Equation of interphase adsorption equilibrium – page 419

Shishulin A.V., Shishulina A.V., Kuptsov A.V.
Several notes on the melting behavior of mesoporous materials – page 427

Shishulin A.V., Shishulina A.V., Kuptsov A.V.
Peculiarities of «liquid – solid» phase equilibria in Six-Ge1-x nanoparticles for various mutual arrangements of phases – page 437

3. FIRST PRINCIPLES AND ATOMISTIC MODELING – page 448

Bespalov D.V., Golovanova O.A.
Quantum-chemical calculation of magnesium(II) compound with tryptophan: synthesis, structure, properties – page 448

Gafner Yu.Ya., Ryzhkova D.A., Gafner S.L., Cherepovskaya A.A.
Determination of the size limit of stability of the fcc phase of Ag nanoparticles – page 457

Karakeyan I.V., Puitov V.V., Talyzin I.V., Samsonov V.M.
Icosahedral metallic nanoclusters: low-temperature structures or pre-melting ones? – page 468

Komarov P.V., Malyshev M.D., Baburkin P.O.
Studying the interaction of polyacrylonitrile oligomer chains with carbon fillers – page 481

Kotomkin A.V., Orlov Yu.D.
Structure – property relationship for the fluorinealcanes – page 493

Kuznetsov Yu.A., Lapushkin M.N.
Au adsorption on W(100): calculation – page 501

Mikhailov G.P.
Calculation of the electronic absorption spectrum of a nanocluster (TiO2)15 doped with a nitrogen atom – page 510

Nepsha N.I., Sokolov D.N., Kolosov A.Yu., Savina K.G., Grigoryev R.E., Sdobnyakov N.Yu.
On the problem of stability/instability in core-shell ternary Cu-Fe-Ni nanoparticles – page 517

Savina K.G., Veselov A.D., Grigoryev R.E., Veresov S.A., Ershov P.M., Zorin D.R., Sdobnyakov N.Yu.
Structural transformations in binary Ti-V nanoparticles: size effect and effect of composition change – page 532

Sokolov D.N., Myasnichenko V.S., Polev O.V., Savina K.G., Sdobnyakov N.Yu.
On the stability and structure relaxation of metallic nanocages – page 543

Cherepovskaya A.A., Gafner S.L., Gafner Yu.Ya., Ryzhkova D.A.
Analysis of thermal stability of the internal structure of Ag-Cu nanoparticles – page 557

4. PHYSICAL AND CHEMICAL BASES OF NANOTECHNOLOGIES – page 565

Akhmedov A.K., Asvarov A.Sh., Murliev E.K., Shomakhov Z.V.
High-mobility transparent conductive layers based on indium oxide doped with tungsten – page 565

Akhmedov A.K., Asvarov A.Sh., Murliev E.K., Shomakhov Z.V.
Some features of localization of Al, Ga and In impurities in ZnO layers – page 575

Bibanaeva S.A., Skachkov V.M., Sabirzyanov N.A.
Sorption purification of solutions with synthetic zeolites – page 584

Bolotov A.N., Novikova O.O.
On the nature of anomalously high value of yield stress of nanostructured magnetic fluid – page 592

Burtsev A.A., Kiselev A.V., Mikhalevsky V.A., Ionin V.V., Nevzorov A.A., Eliseev N.N., Lotin A.A.
Kinetics of laser-induced crystallization of GeTe and Ge2Sb2Te5 chalcogenide phase-change material thin films – page 603

Burtsev A.A., Mikhalevsky V.A., Nevzorov A.A., Kiselev A.V., Konnikova M.R., Ionin V.V., Eliseev N.N., Lotin A.A.
Synthesis of phase-change material Ge2Sb2Te5 nanoparticles by laser-induced forward transfer techniques – page 612

Devitsky O.V.
Pulsed laser deposition OF III-V semiconductor thin films: review – page 621

Devitsky O.V.
Methods for reducing droplet formation density on the surface of thin semiconductor films by pulse laser deposition: review – page 631

Izmailov V.V., Novoselova M.V.
On the profile characteristics of technical surfaces as applied to nanoroughness – page 643

Kiselev A.V., Mikhalevsky V.A., Nevzorov A.A., Burtsev A.A., Ionin V.V., Eliseev N.N., Lotin A.A.
Modelling of adaptive phase-shifting filter cells with optical control based on multilayer structures of phasechange materials – page 651

Korolkov O.E., Misochenko A.A., Stolyarov V.V.
Electrostimulated plasticity of titanium under tension – page 658

Kul’kov V.G., Kul’kova V.V.
Internal friction at grain boundaries in nanocrystalline material with pores – page 670

Malashenko V.V.
Dynamic drag of dislocations in aged aluminum alloys under laser irradiation – page 679

Polukhin V.A., Estemirova S.Kh.
Metal membranes for hydrogen purification: problems, trends and prospects of application – page 686

Ryzhkova D.A., Cherepovskaya A.A.
Modification of perovskite and dye-sensitized solar cells with plasmonic nanoparticles – page 711

Solnyshkin A.V., Vostrov N.V., Gudkov S.I., Belov A.N.
Temperature evolution of dielectric characteristics of PVDF and P(VDF-TrFE) films produced by 4D printing – page 720

Stolyarov V.V.
Size effects of friction in pure titanium – page 729

Fronya A.A., Sahakyan A.T.
Surface structuring of silicon wafers with low-frequency giant pulses YAG:ND laser – page 738

5. NANOCHEMISTRY – page 746

Blinov A.V., Pirogov M.A., Yasnaya M.A., Askerova A.S., Shevchenko I.M., Artyushin S.V.
Synthesis and investigation of nanoscale magnesium carbonate stabilized with hyaluronic acid – page 746

Blinova A.A., Gvozdenko A.A., Rehman Z.A., Blinov A.V., Taravanov M.A., Nazaretova E.D.
Development and optimization of the synthesis procedure of selenium nanoparticles stabilized by methylcellulose – page 758

Bogdanova E.A., Khonina T.G., Sabirzyanov N.A.
Investigation of transport properties of hydroxyapatite and its silicon-substituted derivatives – page 767

Bogdanova E.A., Skachkov V.M., Nefedova K.V.
Study of the possibility of obtaining composites based on nanoscale hydroxyapatite reinforced with titanium oxide and calcium fluoride – page 779

Bui C.D., Nalimova S.S., Shomakhov Z.V., Guketlov A.M., Buzovkin S.S., Rybina A.A.
ZnO/Zn2SnO4 nanorod heterostructure coatings for effective detection of acetone – page 794

Gerk S.A., Golovanova O.A.
Influence of hyaluric acid on the structure of nanohydroxyapatite and morphological characteristics of their compositions – page 805

Glazov I.E., Krut’ko V.K., Musskaya O.N., Kulak A.I.
Stabilization of amorphous calcium phosphate in the structure of hydroxyapatite during liquid-phase synthesis – page 815

Golovanova O.A., Kiselev V.M.
Morphology of nanocrystalline structures of hydroxyapatite based on fractal analysis – page 826

Golovanova O.A.
Synthesis of nanohydroxyapatite modified with lanthanum and cerium ions: composition and properties – page 837

Doroshenko A.E., Krut’ko V.K., Musskaya O.N., Kulak A.I.
Electrochemical and biomimetic deposition of calcium phosphates on titanium alloys – page 848

Dyudyun O.A., Komarova A.A., Elbekyan K.S.
Obtaining fullerene dispersions and investigation of their physical and chemical properties – page 857

Zaritovskii A.N., Kotenko E.N., Grishchuk S.V., Glazunova V.A., Volkova G.K.
Studying catalytic synthesis of carbon nanostructures during microwave-assisted pyrolysis of cellulose – page 864

Kartashynska E.S.
Description of complexation thermodynamic parameters for alkanes and polyaromatic hydrocarbons in the framework of semiempirical methods – page 873

Klychkov N.A., Simakov V.V., Sinev I.V., Efanova V.V., Zakharevich A.M.
The effect of water vapor on the conductivity and response of gas-sensitive nanostructured ZnO layers to ethanol vapors at room temperature – page 891

Klychkov N.A., Simakov V.V., Sinev I.V.
The effect of deep surface acceptor states on the temperature-dependent conductivity of zinc oxide nanoparticles – page 906

Krut’ko V.K., Maslova L.Yu., Suchok V.A., Musskaya O.N., Kulak A.I.
Release of cisplatin from bioinert templates in mixture with hydroxyapatite – page 922

Menshikov S.Yu., Malyshev A.N., Kurmacheva V.S., Fedorov S.A., Tonkushina M.O., Ostroushko A.A.
The effect of FeSO4, nanoscale silver and { Mo72Fe30} cluster on the oxidation of ethylene glycol by H2O2 – page 933

Musskaya O.N., Krut’ko V.K., Glazov I.E., Krutsko E.N., Kulak A.I.
Liquid-phase synthesis of magnesium phosphates in the presence of gallic acid – page 942

Nagdalian A.A., Leontiev P.S., Golik A.B., Askerova A.S., Serov A.M., Tatov A.V.
Investigation of the process of polymer stabilization of mixed iron oxide with amylopectin – page 951

Rekh Yu.V., Bibanaeva S.A., Valova M.S., Skachkov V.M., Fedorova O.V., Sabirzyanov N.A.
Sorption of La3+ cations by zeolites from aqueous solutions – page 960

Ryashentsev D.S., Belenkov M.E., Kovalenko L.Y.
Structural varieties of 2D boron nitride – page 971

Sabanin K.I., Skachkov V.M., Medyankina I.S., Bogdanova E.A., Sabirzyanov N.A.
Investigation of the effect of titanium and zirconium oxides on the strength characteristics of nanoscale hydroxyapatite – page 981

Sattorov M.Sh., Spivak Y.M., Kotcur Y.M., Kuznetsov A., Flisyuk E.V., Moshnikov V.A.
Spectroscopy of porous silicon nanoparticles impregnated with a drug maloben substance – page 995

Skachkov V.M., Bogdanova E.A., Bibanaeva S.A., Shirokova A.G.
Development of a material based on hydroxyapatite and aluminosilicate zeolites with a binding agent for the formation of bioactive coatings – page 1004

Suprunchuk V.E., Kravtsov A.A., Tarala L.V., Medyanik E.V., Malyavin F.F., Lapin V.A., Bedrakov D.P.
Synthesis of yttrium aluminum garnet ceramic powder doped with ruthenium – page 1016

Tonkushina M.O., Gagarin I.D., Sharadgah B.T.M.A.., Gavrilyuk V.R., Piunov K.A., Ostroushko A.A.
Formation of hybrid carriers based on albumin and polyoxometalate for targeted drug delivery – page 1025

Chupakhina T.I., Uporova A.M., Gyrdashova O.I., Buldakova L.Yu., Deeva Y.A., Baklanova I.V., Yanchenko M.Yu.
Solid Sr2Ti1-xMnxO4 (x = 0; 0,01; 0,025; 0,05; 0,1) solutions with K2NiF4 structure – page 1035

Shirokova A.G., Bibanaeva S.A., Bogdanova E.A., Skachkov V.M., Koryakova O.V.
Study of the physico-chemical properties of composites obtained by mechanochemical synthesis of nanoscale hydroxyapatite and synthetic zeolites – page 1046

Shomakhov Z.V., Nalimova S.S., Zyryanova O.D., Kondratev V.M., Kalazhokov Z.Kh., Bui C.D., Moshnikov V.A.
Gas sensitivity of WOx/WS2 nanocomposites at room temperature under ultraviolet irradiation – page 1060

Shostak N.A.
Features of determining the parameters of crystal lattice of ice-like associates of water molecules during hydrate formation – page 1071