Foreword – page 7

1. EXPERIMENTAL STUDIES OF NANOPARTICLES, NANOSYSTEMS, AND NANOMATERIALS – page 8

Bazzal K., Voropay E.S., Alekseenko N.A., Kovalenko M.N., Trinh N.H., Zajogin A.P.
Research of Al2O3 and Al nanopowder formation processes in plasma under the influence of defocused dual laser pulses on aluminum in the air atmosphere – page 8

Bernatskii D.P., Pavlov V.G.
Field desorption of intercalated caesium atoms from graphene on the (100) iridium face – page 18

Bernatskii D.P., Pavlov V.G.
Field desorption microscopy of carbon-coated field electron emitters – page 25

Blinov A.V., Gvozdenko A.A., Blinova A.A., Kobina A.V., Golik A.B., Maglakelidze D.G., Vishnitskaya O.K.
Determination of optimal parameters for synthesis of silver nanoparticles stabilized with polyethylene glycol – page 32

Bolotov A.N., Novikova O.O.
Viscometry of nanodisperse magnetic liquids and lubricating oils. 1. Instrumentation for rheological studies of magnetic nanodisperse liquid media – page 44

Bolotov A.N., Novikova O.O., Meshkov V.V.
Viscometry of nanodisperse magnetic liquids and lubricating oils. 2. Metrological analysis of a device for rheological studies of magnetic nanodisperse liquid media – page 56

Bolshakova N.N., Vahterov E.V., Ivanova A.I., Ped`ko B.B., Semenova E.M.
Thermal-induced domain processes in triglycine sulfate crystals with chromium impurities – page 65

Greshnyakov V.A., Belenkov E.A.
Formation of a novel diamond-like bilayer based on 5-7 graphene – page 76

Guseva O.S., Malyshkina O.V., Ivanova A.I., Boitsova K.N.
Barium and calcium niobate ceramics: specific features of their structure – page 85

Devitsky O.V., Kravtsov A.A., Sysoev I.A.
Study of the composition of GaAs1-yBiy films obtained by pulsed laser deposition – page 96

Devitskiy O.V.
Roughness and structure of InGaAsN thin films on Si – page 106

Dyshekova A.Kh., Karmokov A.M., Khasanov A.I., Kalmykov R.M., Shomakhov Z.V.
Morphology and composition of the interface boundary of sodium chloride single crystals with lead – page 115

Efremov V.V., Palatnikov M.N., Shcherbina O.B.
Metastable state with high electric conductivity in Li0,12Na0,88Tа0,25Nb0,75O3 synthesized at high pressure – page 123

Zigert A.D., Dunaeva G.G., Sdobnyakov N.Yu.
Fractal analysis of the maze-like domain structure of ferrite-garnet films in the process of magnetization – page 134

Ivanov V.I., Pyachin S.A.
Separation of particles in polydisperse nanosuspension in the laser radiation field – page 146

Ivanov D.V., Antonov A.S., Semenova E.M., Ivanova A.I., Anofriev V.A., Sdobnyakov N.Yu.
Different schemes for obtaining fractal relief of nanosized platinum films – page 156

Ivanova A.I., Zigert A.D., Tretyakov S.A., Semenova E.M., Dilmieva E.T., Karpenkov A.Yu., Barabanova E.V., Sdobnyakov N.Yu.
Micromorphology of the surface of rapidly quenched Heusler-alloys – page 166

Ivanova A.I., Marinicheva K.A., Tret’yakov S.A., Ivanov A.M., Molchanov S.V., Kaplunov I.A.
Temperature dependence of optical transmission of germanium single crystals – page 177

Kalmykov R.M., Karmokov A.M., Shomakhov Z.V., Dyshekova A.Kh.
Nanosized structures in PbTe matrix with CdSe impurities – page 187

Kartashynska E.S.
On estimation of the area per a surfactant molecule in a 2D monolayer during the liquid-expanded-liquid-condensed phase transition at the air/water interface – page 196

Kovalenko M.N., Alekseenko N.A., Markova L.V., Rutkovskaiy L.S., Patapovich M.P., Zajogin A.P.
Studies of processes of the precursor formation for production of CuAl2O4 nanoceramics at the effect of double laser pulses on AD1 and M2 alloys in the air atmosphere – page 209

Kravtsov A.A., Chikulina I.S., Vakalov D.S., Chapura O.M., Krandievsky S.O., Devitskiy O.V., Lapin V.A.
Luminescence of YAG: Ce doped with silver nanoparticles – page 220

Krylov A.A., Alekseev V.G., Feofanova M.A., Ivanova A.I., Baranova N.V.
Change in the surface structure of semiconductor polymer films during reverse oxidation-reduction – page 228

Kuznetsov Yu.A., Lapushkin M.N.
Electron-stimulated desorption of lithium atoms adsorbed on the surface of gold-lithium intermetallic – page 235

Kuznetsova Yu.V.
Improving the efficiency of the contact force method of the atomic force spectroscopy – page 243

Kuleshov D.S., Blinov A.V., Blinova A.A., Yasnaya M.A., Maglakelidze D.G., Vishnitskaya O.K.
Comparison of the efficiency of different detectors of the scanning electronic microscope « MIRA-LMH» for studying microstructure of nanomaterials – page 250

Lapin V.A., Kravtsov A.A., Kuleshov D.S., Malyavin F.F.
Investigation of possibility of the misfit dislocation density reduction in Ge / Si films with a buffer layer – page 263

Malashenko V.V., Malashenko T.I.
Specific features of inelastic processes in materials with nanoscale defects – page 272

Malyshkina O.V., Patsuev K.V., Ivanova A.I., Ali M.
Comparative analysis of the properties of sodium niobate and sodium – lithium niobate ceramics – page 278

Mamaev D.V., Merkuryev S.A., Malyshkina O.V.
Pore percentage estimation of piezoelectric ceramics using CCANN and image made with SEM – page 286

Maraeva E.V., Moshnikov V.A.
Nitrogen thermal desorption of as a control method for determination of the nanoparticle size in compositions based on zinc oxide and hydroxyapatite – page 294

Matveev A.V., Mashukov M.Y., Nartova A.V., Sankova N.N., Okunev A.G.
Automatic analysis of microscopy images using the DLgram01 cloud service – page 300

Muratova E.N.
Thermal studies of porous aluminum oxide membranes – page 312

Musskaya O.N., Krut’ko V.K., Kulak A.I., Krutsko E.N.
Composites based on calcium phosphates and copper nanoparticles – page 320

Mustafaev G.A., Mustafaev A.G., Cherkesova N.V.
Charge distribution in the Al2O3-SiO2 system exposed to ionizing radiation – page 329

Permiakov N.V.
The use of liquid probes based on an eutectic solution for studying the conducting properties of thin films – page 338

Polukhin V.A., Belyakova R.M., Kurbanova E.D.
Influence of alloying Ti, Mo and W on the kinetic and strength characteristics of membrane alloys based on Nb and V – page 345

Sverdlik G.I., Ataeva A.Yu., Ataev A.R., Khadzaragova E.A., Vazieva L.T.
Analysis of methods for studying the size of nanoparticles – page 358

Semenova E.M., Lyakhova M.B., Sinkevich A.I., Ivanov D.V., Antonov A.S., Sdobnyakov N.Yu.
Fractal analysis of the nanostructure of a heterogeneous high coercity alloy – page 368

Sidorov N.V., Teplyakova N.A., Palatnikov M.N.
Hydrogen bonds in lithium niobate crystals of different composition – page 376

Sidorov N.V., Teplyakova N.A., Palatnikov M.N.
Influence of the method of doping on uniformity and optical properties of LiNbO3:Mg crystals – page 383

Skachkov V.M., Pasechnik L.A., Medyankina I.S., Sabirzyanov N.A.
Study of the properties of diffusion-hardening composite solders modified with a Ti – Mo powder mixture – page 392

Staritsyn M.V., Fedoseev M.L., Kaptelov E.Yu., Senkevich S.V., Pronin I.P.
Structure changing of submicron PZT films with a fine variation of the composition corresponding to morphotropic phase boundary – page 400

Starodub O.S., Voskresenskij V.M., Sidorov N.V., Palatnikov M.N.
Comparative analysis of the influence of doping ions of yttrium and boron formation of defects in lithium niobate crystals – page 411

Khubolov B.M.
Physico-chemical properties of electrochromic complex tungsten oxides – page 421

Khubolov B.M.
Optical properties of amorphous thin films of sodium-tungsten oxide bronzes – page 430

Shebzukhova I.G., Aref`eva L.P.
Influence of polymorphic transformations on anisotropy of the surface energy and the work function of the electron of lithium – page 439

Shomakhov Z.V., Nalimova S.S., Kalmykov R.M., Aubekerov K., Moshnikov V.A.
Study of the microstructure and composition of tin dioxide layers modified by silver nanoparticles – page 447

2. THE THEORY OF NANOSYSTEMS – page 457

Izmailov V.V., Novoselova M.V.
Correlation-spectral analysis of the topography of engineering surfaces at the nanoscale level – page 457

Kramynin S.P.
Influence of size and pressure on the temperature dependencies of thermodynamic properties of platinum – page 465

Kuznetsov Yu.A., Lapushkin M.N.
Calculation of electronic structure of 2D NaAu intermetallic layers – page 475

Malyshkin Yu.A.
Preferential attachment with fitness dependent choice – page 483

Myasnichenko V.S., Matrenin P.V., Sdobnyakov N.Yu.
Prediction of bonding energy by structural descriptors of metal nanoalloys – page 495

Samsonov V.M., Talyzin I.V., Puitov V.V., Vasilyev S.A.
To the problem of applicability of the Tamman temperature concept to nanosized objects: to the 160th anniversary of Gustav Tamman – page 503

Skobin M.I., Feofanova M.A., Kryukov T.V.
Theoretical and experimental study of macromolecular nanostructures based on heparin and lanthanoids – page 513

Yurov V.M., Goncharenko V.I., Oleshko V.S., Guchenko S.A.
Surface layer thickness and anisotropy of the surface energy of cubic ruthenium crystals – page 522

3. FIRST PRINCIPLES AND ATOMISTIC MODELING – page 534

Alekseev V.G., Baburkin P.O., Tung S., Komarov P.V.
Computer simulation of π – π interactions of tetrathiophene molecules – page 534

Belenkov M.E., Chernov V.M.
Simulation of polymorphic varieties of hexagonal graphene functionalized by hydroxyl groups – page 541

Belyakova R.M., Kurbanova E.D., Polukhin V.A.
Analysis of Nb – Ni and V – Ni based membrane characteristics – page 552

Malyshev M.D., Tung S-H., Komarov P.V.
Molecular-dynamic simulation of mixtures of modified fullerenes and 1,8-octandithiol – page 562

Myasnichenko V.S., Eshov P.M., Savina K.G., Veselov A.D., Bogdanov S.S., Sdobnyakov N.Yu.
Regularities of structure formation in bimetallic nanoparticles with different crystallization temperatures – page 568

Pan’kin N.A.
Change in the structure of titanium nanoclusters under thermal exposure: molecular dynamic simulation – page 580

Ryzhkova D.A., Gafner S.L., Gafner Yu.Ya.
Role of «magic» HCP numbers in stability of the internal structure of Ag89 and Ag153 nanoclusters – page 593

Ryzhkova D.A., Gafner S.L., Gafner Yu.Ya.
Structural stability of Ag55 and Ag147 nanoclusters with a change in the initial morphology – page 604

Sdobnyakov N.Yu., Bogdanov S.S., Veselov A.D., Savina K.G., Nepsha N.I., Kolosov A.Yu., Myasnichenko V.S.
Influence of the size effect on the regularities of the structure formation in bimetallic Au-Co nanoparticles – page 612

Sokolov D.N., Sdobnyakov N.Yu., Savina K.G., Kolosov A.Yu., Myasnichenko V.S.
New opportunities for high-performance simulations of nanosystem using Metropolis software – page 624

Chepkasov I.V.
Study of potassium intercalation in the graphene / MoS2 structure – page 639

4. PHYSICAL AND CHEMICAL BASES OF NANOTECHNOLOGIES – page 646

Bakhvalova E.S., Bykov A.V., Nikoshvili L.Zh., Kiwi-Minsker L.
Influence of halogen nature on the adsorption ability of aryl halides on palladium clusters – page 646

Bogdanova E.A., Skachkov V.M., Giniyatullin I.M., Pereverzev D.I., Nefedova K.V.
Preparation of biocomposites based on nanoscale hydroxyapatite with zirconium and silicon oxides – page 655

Bogdanova E.A., Skachkov V.M.
Promising composite materials based on nanoscale apatite with gelatin as a binding agent – page 664

Zernitsa D.A., Shepelevich V.G.
Study of the structure and properties of lead-free rapidly solidified zinc-based alloys during a heat treatment – page 672

Ivanov D.V., Anofriev V.A., Koshelev V.A., Antonov A.S., Vasilyev S.A., Sdobnyakov N.Yu.
Simulation of layer by layer growth of fractal metal Pt-Rh films – page 682

Ivanov Yu.F., Abzaev Yu.A., Klopotov A.A., Prokopenko N.A., Tolkachev O.S., Nikitin P.Yu., Shugurov V.V., Teresov A.D., Petyukevich M.S.
Features of the structural phase state of a film based on a high-entropy AlNbTiZrСu alloy synthesized by deposition of a multi-element metal plasma – page 693

Klychkov N.A., Simakov V.V., Sinev I.V., Timoshenko D.A.
Dynamics of response of a sensor based on a nanostructured tin dioxide layer exposed to the isopropanol vapors – page 708

Kovtun A.I., Mysyura A.G.
Physico-chemical properties of a nanocomposite hydrogel coating on a textile carrier for the wound treatment – page 717

Kurbanova E.D., Belyakova R.M., Polukhin V.A.
Specific structure of effective membrane alloys based on niobium, vanadium and zirconium – page 728

Malyshkina O.V., Shishkov G.S., Ivanova A.I.
Optimization of technology for producing a composite based on barium ferrite and barium titanate – page 740

Masloboeva S.M.
Analysis of methods for synthesis of a boron-doped lithium niobate charge used for growing single crystals – page 750

Ponomareva A.A., Sitnikova V.E., Tсoi K.A.
Formation of sol-gel catalytic coatings to improve the ecological parameters of intermetallic porous burners – page 760

Pravilnikova T.I., Golovanova O.A.
Precipitation of calcium phosphates from a model blood plasma solution on steel grade 12X18N10T – page 769

Raksha E.V., Glazunova V.A., Oskolkova O.N., Sukhov P.V., Volkova G.K., Davydova A.A., Berestneva Yu.V., Savoskin M.V.
Carbon nanoparticles based on thermally expanded graphite: effect of the TEG obtaining route on the particles morphology – page 777

Skachkov V.M.
Change in properties of diffusion-hardening solder in dependence on the composition of the liquid metal component – page 788

Timoshenko D.A., Sinev I.V., Simakov V.V., Klychkov N.A.
Recognition of gas-air mixtures by a single gas sensor based on the tin dioxide nanowhiskers – page 796

Fomin A.I., Pan’kin N.A.
Phase composition, substructure and residual macrostresses in the surface layer of a tape obtained by electric contact welding – page 802

5. NANOCHEMISTRY – page 809

Bibanaeva S.A., Skachkov V.M.
The effect of metal additives on conversion hematite in the processing of bauxite by the Buyer method – page 809

Glazov I.E., Krut’ko V.K., Vlasov R.A., Musskaya O.N., Kul’bitskaya L.V., Kulak A.I.
Precipitation of hybrid hydroxyapatite / autofibrin nanocomposites – page 818

Golovanova O.A.
Synthesis and properties of Sr-containing trycalcium phosphate – page 829

Gubarev Yu.A., Lebedeva N.Sh., Tonkushina M.O., Gagarin I.D., Golub A.Yu., Ostroushko A.A.
Interaction of iron-containing nanocluster polyoxometalate with doxorubicin – page 841

Klychkov N.A., Simakov V.V., Sinev I.V., Timoshenko D.A.
Multiparametric recognition of organic vapors by using a gas sensor based on a nanostructured tin dioxide film – page 852

Krut’ko V.K., Doroshenko A.E., Musskaya O.N., Rabchynski S.M., Kulak A.I.
Apatites formation on electrodeposited calcium phosphates in the Ca(NO3)2 / NH4H2PO4 and CаCO3 / Ca(H2PO4)2 systems – page 860

Krut’ko V.K., Maslova L.Yu., Musskaya O.N., Safronova T.V., Kulak A.I.
Modification of calcium phosphate foam ceramics with bioapatite in SBF solution – page 870

Kryukov T.V., Feofanova M.A., Skobin M.I., Ivanova A.I.
Synthesis and physicochemical study of the cerium and cefazolin metal complex – page 881

Malkanduev Yu.A., Kokoevа A.A., Dzhalilov A.T.
Polymerization by interaction α-haloacrylic acids with tertiary amines – page 890

Medyankina I.S., Skachkov V.M., Pasechnik L.A.
Kinetics aspect of hydrochemical fluorination of silicon-containing industrial waste – page 900

Nalimova S.S., Shomakhov Z.V., Punegova K.N., Ryabko A.A., Maximov A.I.
Synthesis and study of gas-sensitive nanostructures of the Zn–Sn–O system – page 910

Rozhentsev D.A., Mansurov R.R., Tkachev N.K., Russkikh O.V., Ostroushko A.A.
Catalytic properties in the heterogeneous Fenton reaction of the surface of nanoporous iron obtained by electrochemical dealoiyng in melted chloride mixtures – page 919

Kharaev A.M., Bazheva R.Ch.
Study of relaxation transitions in some aromatic polyesters – page 928

Yasnaya M.A., Blinov A.V., Golik A.B., Maglakelidze D.G., Gvozdenko A.A., Kravtsov A.A., Blinova A.A.
Influence of the polyethylene glycol molecular mass on thermal transitions of nanosized copper oxide – page 937