Nanodispersed magnetic oil: relationship between liquid phase composition and tribological characteristics

A.N. Bolotov, V.V. Novikov, O.O. Novikova

Tver State Technical University

DOI: 10.26456/pcascnn/2025.17.577

Original article

Abstract: The use of nanodispersed magnetic oil for lubricating plain bearings of modern high-tech equipment allows to increase its durability and performance. The paper assesses the effect of the dispersion medium, nanodispersed magnetic phase, antiwear additives and fillers on the tribological properties of magnetic oil. Three-component magnetic lubricating oils with different dispersion medium compositions were studied. Synthetic organosilicon fluids belonging to different groups were used as dispersion medium. Magnetic oils stabilized by using organosilicon acids, ionogenic surfactants, fatty acids, etc. were tested. According to the results of tribological tests, it was found that in a wide range of friction conditions, the lubricating properties of nanodispersed magnetic oil are higher, the higher these properties are in the dispersed medium. The effect of surfactants stabilizing the colloidal structure of nanooils on the corrosion-mechanical component of wear was studied. A conclusion has been made about some advantage of oils with polymer shells on particles. A method has been proposed for removing agglomerates of ferroparticles formed during the synthesis of lubricant and as a result of particle flocculation under the action of magnetic forces, by the action of a force non-uniform magnetic field. The need to continue research in this direction has been shown.

Keywords: nanodispersed magnetic oil, triboproperties of magnetic oils, dispersion medium, antiwear additives, friction, wear

  • Alexander N. Bolotov – Dr. Sc., Professor, Head of the Applied Physics Department, Tver State Technical University
  • Vladislav V. Novikov – Ph. D., Full Docent, Applied Physics Department, Tver State Technical University
  • Olga O. Novikova – Ph. D., Full Docent, Applied Physics Department, Tver State Technical University

For citation:

Bolotov A.N., Novikov V.V., Novikova O.O. Nanodispersnoe magnitnoe maslo: vzaimosvyaz sostava zhidkoj fazy i tribotekhnicheskikh kharakteristik [Nanodispersed magnetic oil: relationship between liquid phase composition and tribological characteristics], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 577-584. DOI: 10.26456/pcascnn/2025.17.577.

Full article (in Russian): download PDF file

References:

1. Odenbach S. Colloidal magnetic fluids: basics, develoрment and aррlication of ferrofluids, Lecture Notes in Physics. Springer, Berlin, Heidelberg, 2009, vol. 763, X, 430 p. DOI: 10.1007/978-3-540-85387-9.
2. Trivedi K., Parekh K., Upadhyay R.V. Nanolubricant: Magnetic nanoparticle based, Materials Research Express, 2017, vol. 4, no. 11, art. no. 114003, 10 p. DOI: 10.1088/2053-1591/aa95e1.
3. Zhang Y., Yang Z., Li D. The roller chain lubricated with ferrofluids, Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology, 2019, vol. 233, issue 6, pp. 927-935. https://doi.org/10.1177/1350650118806799.
4. Berkovskij B.M., Medvedev V.F., Krakov M.S. Magnitnyye zhidkosti [Magnetic fluids]. Moscow: Khimiya, 1989, 240 p. (In Russian).
5. Odenbach S., Thurm S. Magnetoviscous effects in ferrofluids, Ferrofluids. Lecture Notes in Physics. Springer, Berlin, Heidelberg, 2002, vol. 594, pp. 185-201. DOI: 10.1007/3-540-45646-5_10.
6. Hu Z., Yan H., Yang J., Wang X., Yu R. Effect of Components on Friction Property of Carbonyl Iron-Based Magnetorheological Fluid, Arabian Journal for Science and Engineering, 2014, vol. 39, issue 10, pp. 7355-7361. DOI: 10.1007/s13369-014-1358-2.
7. Bolotov A.N., Novikova O.O., Novikov V.V. Magnitnye siloksanovye nanozhidkosti adaptirovannye dlya uslovij granichnogo treniya [Silicone magnetic nanofluids adapted for the conditions of boundary friction], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 546-556. DOI 10.26456/pcascnn/2020.12.546. (In Russian).
8. Chauhan V., Kumar A., Sham R. Magnetorheological fluids: A comprehensive review, Manufacturing Review, 2024, vol. 11, art. no. 6, 15 p. DOI: 10.1051/mfreview/2024005.
9. Shah K.R., Shukla A., Patel N, Katiyar J.K. Effect of ferrofluid lubrication on tribological performance of metal tribopairs, Proceedings of the Institution of Mechanical Engineers, Part J: Journal of Engineering Tribology, 2024, vol. 238, issue 5, pp. 569-580. DOI: 10.1177/13506501241227093.
10. Bolotov A.N., Novikov V.V., Novikova O.O. Komplekt oborudovaniya dlya issledovaniya fiziko-khimicheskikh svojstv nanodispersnykh magnitnykh smazochnykh sred. Chast' 3 [A set of equipment for studying the physical and chemical properties of nanodispersed magnetic lubricating media. Part 3], Mekhanika i fizika protsessov na poverkhnosti i v kontakte tverdykh tel, detalej tekhnologicheskogo i energeticheskogo oborudovaniya [Mechanics and Physics of Processes on the Surface and in Contact of Solids, Parts of Technological and Power Equipment], 2015, no. 8, pp. 66-70. (In Russian).
11. Bolotov A.N., Novikova O.O. Smazochnye svojstva magnitnykh nanozhidkostej na osnove efirov karbonovykh kislot [Lubrication properties of magnetic nanoliquids based on carboxylic acids], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 555-563. DOI: 10.26456/pcascnn/2019.11.555. (In Russian).
12. Damdinov B.B., Mitypov Ch.M. Vliyanie dobavok melkodispersnykh chastits metallov na kharakteristiki smazochnykh materialov [Influence of finely dispersed metal particles additives on lubricants characteristics], Vestnik Buryatskogo gosudarstvennogo universiteta. Khimiya. Fizika [Bulletin of Buryat State University. Chemistry. Physics], 2021, no. 1, pp. 28-42. DOI: 10.18101/2306-2363-2021-1-28-42. (In Russian).
13. Breki A.D., Tyurikova I.A., Shatul'skij A.A., Gvozdev A.E., Kutepov S.N. Vliyanie magnitnykh nanochastits Fe3O4 na trenie i iznos stali 10H17N13M2T v rezhime vercheniya v srede smazochnogo masla [Effect of Fe3O4 magnetic nanoparticles on friction and wear of 10Kh17N13M2T steel in rotation mode in lubricating oil environment], Vestnik Rybinskoj gosudarstvennoj aviacionnoj tekhnologicheskoj akademii im. P.A. Solov'eva [Bulletin of the Rybinsk State Aviation Technological Academy named after P.A. Solovyov], 2018, no. 4, pp. 103-111. (In Russian).

⇐ Prevoius journal article | Content | Next journal article ⇒