Effect of annealing time on the structural and electrophysical properties of strontium ferromolybdate films
S.S. Starukhina1, T.S. Ilina1, A.S. Bykov1, N.A. Kalanda2, A.V. Petrov2, D.A. Kiselev1
1 National University of Science and Technology «MISIS»
2 Scientific- Practical Materials Research Centre NAS of Belarus
DOI: 10.26456/pcascnn/2025.17.182
Original article
Abstract: Thin films of strontium ferromolybdate Sr2FeMoO6 are a promising material for spintronic applications. To comprehensively study the relationship between structure, electrophysical properties, and magnetic characteristics of films deposited by ion-beam sputtering on Al2O3 substrates followed by reductive annealing at 900°C, a set of modern microscopic and spectroscopic techniques was employed. Specifically, Raman spectroscopy, atomic force microscopy, conductive microscopy, Kelvin probe force microscopy, and magnetic force microscopy were used to investigate in detail how different annealing durations (0.5, 1, and 1.5 hours) affect key parameters of the material. It has been found that the duration of annealing significantly influences the surface roughness, electrophysical properties, and most importantly, the formation of magnetic domain structures in Sr2FeMoO6 films. Analysis of the obtained data revealed that optimal structural characteristics are achieved after annealing for 1 hour, while the best magnetic domain structure is observed in samples subjected to annealing for 1,5 hours. These results are important for optimizing the synthesis process of Sr2FeMoO6 films with improved characteristics, which contributes to more efficient use of this material in various spintronic devices.
Keywords: strontium ferromolybdate films, scanning probe microscopy, I-V characteristics, magnetic force microscopy
- Sofya S. Starukhina – 1st year postgraduate student of the Department of Materials Science of Semiconductors and Dielectrics, National University of Science and Technology «MISIS»
- Tatyana S. Ilina – Ph. D., Senior Researcher of the Department of Materials Science of Semiconductors and Dielectrics, National University of Science and Technology «MISIS»
- Alexander S. Bykov – Ph. D., Associate Professor, Department of Materials Science of Semiconductors and Dielectrics, National University of Science and Technology «MISIS»
- Nikolay A. Kalanda – D. Sc., Leading Researcher of the Laboratory of Physics of Magnetic Materials, Scientific- Practical Materials Research Centre NAS of Belarus
- Alexander V. Petrov – Ph. D., Senior Researcher of the Laboratory of Physics of Magnetic Materials, Scientific- Practical Materials Research Centre NAS of Belarus
- Dmitry A. Kiselev – Ph. D., Head of the Department of Materials Science of Semiconductors and Dielectrics, National University of Science and Technology «MISIS»
For citation:
Starukhina S.S., Ilina T.S., Bykov A.S., Kalanda N.A., Petrov A.V., Kiselev D.A. Vliyanie vremeni otzhiga na strukturnye i elektrofizicheskie svojstva plenok ferromolibdata strontsiya [Effect of annealing time on the structural and electrophysical properties of strontium ferromolybdate films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 182-189. DOI: 10.26456/pcascnn/2025.17.182. ⎘
Full article (in Russian): download PDF file
References:
1. Cibert J., Bobo J.F., Lüders U. Development of new materials for spintronics, Comptes Rendus Physique, 2005, vol. 6, issue 9, pp. 977-996. DOI: 10.1016/j.crhy.2005.10.008.
2. Serrate D., De Teresa J.M., Ibarra M.R. Double perovskites with ferromagnetism above room temperature. Journal of Physics: Condensed Matter, 2007, vol. 19, no. 2, art. no. 023201, 86 p. DOI: 10.1088/0953-8984/19/2/023201.
3. Tomioka Y., Okuda T., Okimoto Y., Kumai R., Kobayashi K.-I. Magnetic and electronic properties of a single crystal of ordered double perovskite Sr₂FeMoO₆, Physical Review B, 2000, vol. 61, issue 1, pp. 422-427. DOI: 10.1103/PhysRevB.61.422.
4. Kobayashi K.-I., Kimura T., Sawada H., Terakura K., Tokura Y. Room-temperature magnetoresistance in an oxide material with an ordered double-perovskite structure, Nature, 1998, vol. 395, issue 6703, pp. 677-680. DOI: 10.1038/27167.
5. Bibes M., Bouzehouane K., Barthélémy A. et al. Tunnel magnetoresistance in nanojunctions based on Sr₂FeMoO₆, Applied Physics Letters, 2003, vol. 83, issue 13, pp. 2629-2631. DOI: 10.1063/1.1612902.
6. Kim T.H., Uehara M., Cheong S.-W., Lee S. Large room-temperature intergrain magnetoresistance in double perovskite SrFe₁₋ₓ(Mo or Re)ₓO₃, Applied Physics Letters, 1999, vol. 74, issue 12, pp. 1737-1739. DOI: 10.1063/1.123672.
7. Yarmolich M.V., Kalanda N.A., Demyanov S.E., Silibin M.V., Gorokh G.G. Synthesis and study of strontium ferromolybdate nanopowders with high degree of superstructural ordering for spintronics, Technology and design in electronic equipment, 2016, issue 2-3, pp. 41-48.
8. Nečas D., Klapetek P. Gwyddion: An open-source software for SPM data analysis, Open Physics, 2012, vol. 10, issue 1, pp. 181-188. DOI: 10.2478/s11534-011-0096-2.
9. Weber M.C., Kreisel J., Thomas, P.A. et al. Phonon Raman scattering of RCrO₃ perovskites (R= Y, La, Pr, Sm, Gd, Dy, Ho, Yb, Lu), Physical Review B, 2012, vol. 85, issue 5, pp. 054303-1-054303-9. DOI: 10.1103/PhysRevB.85.054303.
10. Yadav E., Harisankar S., Soni K., Mavani K.R. Effects of Cu-doping on the vibrational and electronic properties of epitaxial PrNiO3 thin films, Vibrational Spectroscopy, 2021, vol. 112, art. no. 103185, 8 p. DOI: 10.1016/j.vibspec.2020.103185.
11. Son L.H., Phuc N.X., Phuc P.V., Hong N.M., Hong L.V. Observation of phase decomposition of Sr2FeMoO6 by Raman spectroscopy, Journal of Raman Spectroscopy, 2001, vol. 32, issue 10, pp. 817-820. DOI: 10.1002/jrs.764.
12. Navarro J., Frontera C., Rubi D., Mestres N., Fontcuberta J. Aging of Sr₂FeMoO₆ and related oxides, Materials Research Bulletin, 2003, vol. 38, issue 9-10, pp. 1477-1486. DOI: 10.1016/S0025-5408(03)00171-5.
13. Metsänoja M., Majumdar S., Huhtinen H., Paturi P. Effect of ex situ post-annealing treatments on Sr₂FeMoO₆ thin films, Journal of superconductivity and novel magnetism, 2022, vol. 25, pp. 829-833. DOI: 10.1007/s10948-011-1355-6.