Yb3-xErхAl5O12 for optical thermometry: measurement of luminescence caused by transitions from non-thermal coupled levels

I.V. Baklanova, V.N. Krasil’nikov, Y.V. Baklanova

Institute of Solid State Chemistry Ural Branch of the RAS

DOI: 10.26456/pcascnn/2025.17.015

Original article

Abstract: Erbium-doped ytterbium aluminum garnet has been synthesized by a precursor method. The samples were characterized by Infrared spectroscopy and scanning electron microscopy. Under infrared excitation at 980 nm, the compounds exhibit intense upconversion red luminescence in the visible range. According to the concentration dependences of upconversion luminescence, the optimal concentration of erbium in Yb3-xErхAl5O12 compounds was x=0,3. The thermoluminescent characteristics for Yb2,7Er0,3Al5O12 garnet were determined by the ratio of band intensities in the visible and near-infrared ranges due to transitions from non-thermal coupled energy levels 4F9/2 and 4I9/2 of Er3+ ion. The maximum values of absolute and relative sensitivity in the temperature interval of 25-225°C have been determined. The results obtained show that it is reasonable to use the method of comparing two luminescent lines assigned to non-thermal coupled energy levels of lanthanide ions for optical thermometry and that phosphors based on Yb3-xErхAl5O12 garnet hold promise as materials for temperature sensors.

Keywords: ytterbium aluminum garnet, erbium, precursor synthesis, luminescence, upconversion

  • Inna V. Baklanova – Ph. D., Senior Researcher, Laboratory of quantum chemistry and spectroscopy after professor A.L. Ivanovsky, Institute of Solid State Chemistry Ural Branch of the RAS
  • Vladimir N. Krasil’nikov – Dr. Sc., Principal Researcher, Laboratory of inorganic synthesis, Institute of Solid State Chemistry Ural Branch of the RAS
  • Yana V. Baklanova – Ph. D., Senior Researcher, Laboratory of quantum chemistry and spectroscopy after professor A.L. Ivanovsky, Institute of Solid State Chemistry Ural Branch of the RAS

For citation:

Baklanova I.V., Krasil’nikov V.N., Baklanova Y.V. Yb3-xErkhAl5O12 dlya opticheskoj termometrii: izmerenie lyuminestsentsii, vyzvannoj perekhodami s temperaturno-nesvyazannykh urovnej [Yb3-xErхAl5O12 for optical thermometry: measurement of luminescence caused by transitions from non-thermal coupled levels], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 015-025. DOI: 10.26456/pcascnn/2025.17.015.

Full article (in Russian): download PDF file

References:

1. George N.C., Denaut K.A., Seshadri R. Phosphors for solid-state white lighting, Annual Review of Materials Research, 2013, vol. 43, pp. 481-501. DOI: 10.1146/annurev-matsci-073012-125702.
2. Lee S., Seo S.Y. Optimization of yttrium aluminum garnet: Ce3+ phosphors for white light-emitting diodes by combinatorial chemistry method, Journal of The Electrochemical Society, 2002, vol.149, no. 11, pp. J85-J88. DOI: 10.1149/1.1511755.
3. Chen D., Xiang W., Liang X. et al. Advances in transparent glass-ceramic phosphors for white light-emitting diodes - A review, Journal of the European Ceramic Society, 2015, vol. 35, issue 3, pp. 859-869. DOI: 10.1016/j.jeurceramsoc.2014.10.002.
4. Xu L., Liu Y., Zhou Z. et al. New role of Yb3+-energy reservoir for lanthanide upconversion luminescence, Nanoscale, 2021, vol. 13, issue 22, pp. 9978-9988. DOI: 10.1039/D0NR08205H.
5. Auzel F. Upconversion and anti-stokes processes with f and d ions in solids, Chemical Reviews, 2004, vol. 104, issue 1, pp. 139-174. DOI: 10.1021/cr020357g.
6. Baklanova I.V., Krasil'nikov V.N., Tyutyunnik А.P., Baklanova Ya.V. Upconversion multicolor tuning in Er3+ and Yb3+ doped yttrium oxide prepared by precursor technique, Inorganic Chemistry Communications, 2024, vol. 166, art. no. 112615, 11 p. DOI: 10.1016/j.inoche.2024.112615.
7. Thirumavalavan M., Kumar J., Gnanam F.D., Ramasamy P. Vibrational spectra of Y3Al5O12 crystals grown from Ba- and Pb-based flux systems, Infrared Physics, 1986, vol. 26, issue 2, pp. 101-103. DOI: 10.1016/0020-0891(86)90029-1.
8. Zhang J., Wang S., An L., Liu M., Chen L. Infrared to visible upconversion luminescence in Er3+:Y2O3 transparent ceramics, Journal of Luminescence, 2007, vol. 122-123, pp. 8-10. DOI: 10.1016/j.jlumin.2006.01.065.
9. Lu H., Hao H., Shi G. et al. Optical temperature sensing in b-NaLuF4:Yb3+/Er3+/Tm3+ based on thermal, quasi-thermal and non-thermal coupling levels, RSC Advances, 2016, vol. 6, issue 60, pp. 55307-55311. DOI: 10.1039/c6ra08311k.
10. Zhao Y., Wang X., Zhang Y., Li Y., Yao X. Optical temperature sensing of up-conversion luminescent materials: Fundamentals and progress, Journal of Alloys and Compounds, 2020, vol. 817, art. no. 152691, 27 p. DOI: 10.1016/j.jallcom.2019.152691.
11. Lipina O.A., Baklanova Ya.V., Spiridonova T.S., Khaikina E.G. Upconversion luminescence and temperature measurement performance of Ho3+/Yb3+ and Tm3+/Yb3+ codoped Na5Rb7Sc2(WO4)9 phosphors, CrystEngComm, 2024, vol. 26, issue 3, pp. 277-285. DOI: 10.1039/d3ce01020a.
12. Gao W., Ge W., Shi J., Chen X., Li Y. A novel upconversion optical thermometers derived from non-thermal coupling levels of CaZnOS:Tm/Yb phosphors, Journal of Solid State Chemistry, 2021, vol. 297, art. no. 122063, 7 p. DOI: 10.1016/j.jssc.2021.122063.
13. Han Q., Hao H., Yang J. et al. Optical temperature sensing based on thermal, non-thermal coupled levels and tunable luminescent emission colors of Er3+/Tm3+/Yb3+ tri-doped Y7O6F9 phosphor, Journal of Alloys and Compounds, 2019, vol. 786, pp. 770-778. DOI: 10.1016/j.jallcom.2019.02.047.
14. Li Z., Zheng J., Zhang W. et al. A promising high-entropy thermal barrier material with the formula (Y0.2Dy0.2Ho0.2Er0.2Yb0.2)3Al5O12, Materials, 2022, vol. 15, issue 22, art. № 8079? 12 p. DOI: 10.3390/ma15228079.
15. Li X., Guan Z., Liu Z. et al. Impact of nitridation on the up-conversion luminescence property of Yb3Al5O12:Er3+ phosphors upon 980 nm excitation, Inorganic Chemistry Communications, 2024, vol. 160, art. no. 111905, 11 p. DOI: 10.1016/j.inoche.2023.111905.
16. dos Santos P.V., de Araujo M.T., Gouveia-Neto A.S., Medeiros Neto J.A., Sombra A.S.B. Optical temperature sensing using upconversion fluorescence emission in Er3+/Yb3+-codoped chalcogenide glass, Applied Physics Letters, 1998, vol. 73, issue 5, pp. 578-580. DOI: 10.1063/1.121861.
17. Zhang Y., Chai X., Li J., Wang X., Li Y., Yao X. Enhanced up-conversion luminescence and excellent temperature sensing properties in Yb3+ sensitized Er3+-doped Bi3Ti1.5W0.5O9 multifunctional ferroelectric ceramics, Journal of Alloys and Compounds, 2018, vol. 735, pp. 473-479. DOI: 10.1016/j.jallcom.2017.11.085.
18. Savchuk Ol.A., Carvajal J.J., Massons J. et al. Novel low-cost, compact and fast signal processing sensor for ratiometric luminescent nanothermometry, Sensors and Actuators A: Physical, 2016, vol. 250, pp. 87-95. DOI: 10.1016/j.sna.2016.08.031.
19. Alencar M.A.R.C., Maciel G.S., de Araújo C.B., Patra A. Er3+-doped BaTiO3 nanocrystals for thermometry: Influence of nanoenvironment on the sensitivity of a fluorescence based temperature sensor, Applied Physics Letters, 2004, vol. 84, issue 23, pp. 4753-4755. DOI: 10.1063/1.1760882.
20. Kelly K.L. Color designations for lights, Journal of the Optical Society of America, 1943, vol. 33, issue 11, pp. 627-632. DOI: 10.1364/JOSA.33.000627.

⇐ Prevoius journal article | Content | Next journal article ⇒