Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Spectroscopy of porous silicon nanoparticles impregnated with a drug maloben substance

M.Sh. Sattorov1, Y.M. Spivak1, Y.M. Kotcur2, A. Kuznetsov3, E.V. Flisyuk2, V.A. Moshnikov1

1 St. Petersburg Electrotechnical University «LETI»
2 St. Petersburg State Chemical and Pharmaceutical University
3 Moscow Institute of Physics and Technology (National Research University)

DOI: 10.26456/pcascnn/2024.16.995

Original article

Abstract: Using electrochemical anodic etching, porous silicon layers were formed with subsequent production of nanoparticles. The study of the nature of interaction of porous silicon nanoparticles with a new promising 4,4′-(propanediamido) sodium dibenzoate (malobene) substance was performed using infrared and Raman spectroscopy. It was revealed that during the incorporation process, an interaction occurs between the nanoparticle and maloben, during which the degree of influence of porous Si particles during joint scattering of light decreases, and the vibrational modes of the sodium 4,4′-(propanediamido) dibenzoate molecule become more intense. Characteristic absorption bands associated with the formation of chemical bonds by wave and Raman numbers were detected, and an interpretation of the obtained results from the point of view of the formation of the finished substance was proposed.

Keywords: porous silicon, nanostructured layer, nanoparticles, maloben, chemical bonds, infrared Fourier spectroscopy, Raman spectroscopy, scanning electron microscopy

  • Mansurjon Sh. Sattorov – 4th year postgraduate student, Department of Micro- and Nanoelectronics, St. Petersburg Electrotechnical University «LETI»
  • Yulia M. Spivak – Dr. Sc., Professor, Department of Micro- and Nanoelectronics, St. Petersburg Electrotechnical University «LETI»
  • Yulia M. Kotcur – Ph. D., Senior Researcher, GMP training center, St. Petersburg State Chemical and Pharmaceutical University
  • Alexey . Kuznetsov – Junior Researcher, Moscow Institute of Physics and Technology (National Research University)
  • Elena V. Flisyuk – Dr. Sc., Professor, Department of Technology of Dosage Forms, St. Petersburg State Chemical and Pharmaceutical University
  • Vyacheslav A. Moshnikov – Dr. Sc., Professor, Department of Micro- and Nanoelectronics, St. Petersburg Electrotechnical University «LETI»

For citation:

Sattorov M.Sh., Spivak Y.M., Kotcur Y.M., Kuznetsov A.., Flisyuk E.V., Moshnikov V.A. Spektroskopiya nanochastits poristogo kremniya, impregnirovannykh lekarstvennoj substantsiej malobena [Spectroscopy of porous silicon nanoparticles impregnated with a drug maloben substance], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 995-1003. DOI: 10.26456/pcascnn/2024.16.995.

Full article (in Russian): download PDF file

References:

1. Moshnikov V.A., Spivak YU.M., Len'shin A.S. Poristyi kremnii i ego primenenie v biomeditsine [Porous silicon and its application in biomedicine], Issledovanie, tekhnologiya i ispol'zovanie nanoporistykh nositelei lekarstv v meditsine [Research, technology and use of nanoporous drug carriers in medicine], ed. V.Ya. Shevchenko, O.I. Kiseleva, V.N. Sokolova. Saint-Petersburg, Khimizdat Publ., 2015, pp. 70-116. (In Russian).
2. Spivak Yu.M., Korolev D.V., Sattorov M.Sh. et al. Potential antiviral drug for the treatment of SARS-CoV-2 based on quinacrine and porous silicon, Biomedical Journal of Scientific & Technical Research, 2022, vol. 42, issue 2, pp. 33513-33517. DOI: 10.26717/BJSTR.2022.42.006735.
3. Tiu T., Al'ba M., Ehlnatan R. et al. Advances in porous silicon-based nanomaterials for diagnostic and therapeutic applications, Advanced Therapeutics, 2018, vol. 2, no. 1, art. no. 1800095, 25 p. DOI: 10.1002/adtp.201800095.
4. Martins YA.P., D'Oria R., Lyu D. Engineered multifunctional albumin-decorated porous silicon nanoparticles for fcrn translocation of insulin, Small, 2018, vol. 14, issue 27, art. no. 1800462, 11 p. DOI: 10.1002/smll.201800462.
5. Spivak Yu.M., Korolev D.V., Moshnikov V.A. Porous nanocarriers for targeted drug delivery and theranostics, Smart Micro‑ and Nanomaterials for Drug Delivery, ed. by A. Bekhera, A.K. Nayak, R.K. Mokhapatra, A.A. Rabaan. Boca Raton, CRC Press, 2024, pp. 343-372. DOI: 10.1201/9781003468424-18.
6. Zhuravskii S.G., Yukina G.YU., Sukhorukova E.G. et al. Kharakter granulyomoobrazovaniya v pecheni krys kak otrazhenie mekhanizma internalizatsii submikronnykh chastits poristogo kremniya [The character of granuloma formation in the liver of rats as a reflection of the mechanism of internalization of submicron silicon particles], Byulleten' eksperimental'noj biologii i meditsiny [Bulletin of Experimental Biology and Medicine], 2023, vol. 176, no. 9, pp. 386-390. (In Russian).
7. Xu T., Fan L., Wang L. et al. Hierarchical mesoporous silicon and albumin composite microparticles delivering DOX and FU for liver cancer treatment, International Journal of Biological Macromolecules, 2024, vol. 268, part 1, art. no. 131732, 10 p. DOI: 10.1016/j.ijbiomac.2024.131732.
8. Belykh M.A. Vliyanie 4,4’-(propandiamido)dibenzoata natriya na proyavleniya eksperimental'nogo nealkogol'nogo steatogepatita [Impact of 4,4’-(propanediamide)dibenzoate sodium on manifestations of experimental non-alcoholic steatohepatitis], Biomeditsina [Biomedicine], 2021, vol. 17, no. 3, pp. 95-99. DOI: 10.33647/2074-5982-17-3-95-99. (In Russian).
9. Flisyuk E.V., Kotsur Yu.M., Narkevich I.A. et al. Razrabotka metodiki provedeniya testa «Rastvorenie» dlya tabletok 4,4’-(propandiamido)dibenzoata natriya s prolongirovannym vysvobozhdeniem [Development of the «dissolution» test method for tablets of sodium 4,4'-(propanediamido)dibenzoate with sustained release], Razrabotka i registratsiya lekarstvennykh sredstv [Drug development & registration], 2021, vol. S4, no. 10, pp. 146-154. DOI: 10.33380/2305-2066-2021-10-4(1)-146-154. (In Russian).
10. Spivak Yu.M., Belorus A.O., Panevin A.A. et al. Porous silicon as a nanomaterial for disperse transport systems of targeted drug delivery to the inner ear, Technical Physics, 2018, vol. 63, issue 9, pp. 1352-1360. DOI: 10.1134/S1063784218090207.
11. Sattorov M.Sh., Bespalova K., Panov M.F., Spivak Yu.M. Osobennosti adsorbtsii organicheskikh molekul v poristom kremnii po dannym IK-spektroskopii [Features of adsorption of organic molecules in porous silicon according to IR spectroscopy data], Sbornik materialov VII Nauchno-practicheskoi konferentsii s mezhdunarodnym uchastiem «Nauka nastoyashchego i budushchego» dlya studentov, aspirantov i molodykh uchenykh [Proceedings of VII Scientific and Practical Conference with international participation «Science of the present and the future» for students, postgraduates and young scientists, Saint-Petersburg, May, 16-18, 2019. Saint Petersburg Electrotechnical University «LETI» Publ., 2019, vol. 3. pp. 128-131. (In Russian).
12. Sattorov M.Sh., Spivak Yu.M., Gavazyuk N.O., Panov M.F. The effect of anodization current density on the functionalization of porous silicon nanoparticles with an antibiotic, Journal of Physics: Conference Series, 2020, vol. 1697, art. no. 012122, 6 p. DOI: 10.1088/1742-6596/1697/1/012122.
13. Pradkhan M.M., Garg R.K., Arora M. Multiphoton infrared absorption in silicon, Infrared Physics, 1987, vol. 27, issue 1, pp. 25-30. DOI: 10.1016/0020-0891(87)90046-7.

⇐ Prevoius journal article | Content | Next journal article ⇒