Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Obtaining fullerene dispersions and investigation of their physical and chemical properties

O.A. Dyudyun, A.A. Komarova, K.S. Elbekyan

Stavropol State Medical University

DOI: 10.26456/pcascnn/2024.16.857

Short communication

Abstract: Prospects for successful use of fullerenes in biology and medicine relate to the possibility of obtaining their non-toxic hydrophilic derivatives, which are able to participate in the metabolism occurring in a living organism. An effective solution to this problem is associated with creation of water-soluble molecular complexes, in which the fullerene molecule is enclosed in a larger water-soluble capsule. A new method for producing colloidal suspensions and aqueous dispersions of fullerenes based on vegetable oil and polyvinyl alcohol by ultrasonic dispersion in an Elmasonic S10H chamber has been proposed. Transmission spectra of the synthesized samples were recorded on a UNICO 2100 spectrophotometer. The hydrodynamic radius of particles was measured on a Photocor Compact-Z particle size analyzer. To create theoretical models, as well as carry out quantum chemical calculations, the 3D modeling program ArgusLab 4.0.1 was used. The structures of hydrogel films of fullerene dispersions were studied by scanning electron microscopy (MIRA-LMH microscope from Tescan).

Keywords: colloidal solutions of fullerenes, fullerene dispersions, ultrasonic dispersion, 3D modeling, physical and chemical analysis

  • Olga A. Dyudyun – Ph. D., Associate Professor, Department of General and Biological Chemistry, Stavropol State Medical University
  • Anastasia A. Komarova – Assistant, Department of General and Biological Chemistry, Stavropol State Medical University
  • Karina S. Elbekyan – Dr. Sc., Professor, Head of the Department of General and Biological Chemistry, Stavropol State Medical University

For citation:

Dyudyun O.A., Komarova A.A., Elbekyan K.S. Poluchenie kolloidnykh suspenzij i vodnykh dispersij fullerenov i issledovanie ikh fizikokhimicheskikh svojstv [Obtaining fullerene dispersions and investigation of their physical and chemical properties], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 857-863. DOI: 10.26456/pcascnn/2024.16.857.

Full article (in Russian): download PDF file

References:

1. Andreev S.M., Bashkatova E.N., Purgina D.D. et al. Fullereny: biomeditsinskij aspekt [Fullerenes: biomedical aspects], Immunologiya [Immunology], 2015, vol. 36, no. 1, pp. 57-61. (In Russian).
2. Fjodorova N., Novič M., Venko K. et al. How fullerene derivatives (FDs) act on therapeutically important targets associated with diabetic diseases, Computational and Structural Biotechnology Journal, 2022, vol. 20, pp. 913-924. DOI: 10.1016/j.csbj.2022.02.006.
3. Semenov K.N., Charykov N.A., Arapov O.V. et al. Rastvorimost' legkikh fullerenov v nekotorykh efirnykh i rastitel'nykh maslakh [Solubility of light fullerenes in some essential and vegetable oils], Khimija rastitel'nogo syr'ja [Chemistry of plant raw material], 2010, no. 2, pp. 147-152. (In Russian).
4. Semenov K.N., Ivanova D.A., Ageev S.V. et al. Evaluation of the C60 biodistribution in mice in a micellar ExtraOx form and in an oil solution, Scientific Reports, 2021, vol. 11, art. no 8362, 13 p. DOI: 10.1038/s41598-021-87014-3.
5. Elbekyan K.S., Komarova A.A., Dyudyun O.A. et al. Izuchenie biologicheskikh svojstv fullerenov v eksperimente [Experimental study of the biological properties of fullerenes], Aktualnaja biotehnologija [Topical biotechnology], 2021, № 1 (35), p. 174. (In Russian).
6. Albagachiev Sh.I., Khamchiev B.A., Albogachieva M.Kh. et al. Razrabotka optimal'nogo rezhima ekstraktsionnogo vydeleniya fullerenov S60 i S70 [Development of an optimal extraction mode for the separation of fullerenes C60 and C70], Ecology and environmental management, International scientific and practical conference: proceedings, Magas, October, 21-23, 2020. Magas: LLC «KEP» Publ., 2020, pp. 9-14. (In Russian).
7. Elbekyan K.S., Komarova A.A., Dyudyun O.A. et al. Metod ul'trazvukovogo dispergirovaniya kak sposob polucheniya kompozitsii fullerenov na osnove rastitel'nogo masla [Ultrasonic dispersion method as a method for obtaining a composition of fullerenes based on vegetable oil], Aktualnaja biotehnologija [Topical biotechnology], 2020, № 3 (34), p. 388. (In Russian).
8. Думпис М.А., Николаев Д.Н., Литасова Е.В. и др. Biologicheskaya aktivnost' fullerenov – realii i perspektivy [Biological activity of fullerenes – reality and prospects], Obzory po klinicheskoj farmakologii i lekarstvennoj terapii [Reviews on clinical pharmacology and drug therapy], 2018, vol. 16, no. 1, pp. 4-20. DOI: 10.17816/RCF1614-20. (In Russian).
9. ArgusLab 4.0.1. Available at: www.url: https://mybiosoftware.com/arguslab-4-0-1-molecular-modeling-graphics-drug-design-program.html. (accessed 30.06.2024).
10. Volkova T.O., Shirinkin S.V., Shaposhnikov A.A. Obzor dannykh o mekhanizmakh vliyaniya gidratirovannykh fullerenov na biologicheskie sistemy [Review of data on the mechanisms of influence of hydrated fullerenes on biological systems], Nauchnye vedomosti Belgorodskogo gosudarstvennogo universiteta. Seriya: Estestvennye nauki [Scientific bulletins of Belgorod State University. Series: Natural Sciences], 2011, no. 21 (116). pp. 64-70. (In Russian).
11. Ray A. Fullerene (C60) molecule – a review, Asian Journal of Pharmaceutical Research, 2012, vol. 2, issue 2, pp. 47-50. DOI: 10.5958/2231–5691.
12. Castro E., Garcia A.H., Zavala G., Echegoyen L. Fullerenes in biology and medicine, Journal of Materials Chemistry B, 2017, vol. 5, issue 32, pp. 6523-6535. DOI: 10.1039/C7TB00855D.

⇐ Prevoius journal article | Content | Next journal article ⇒