Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Development and optimization of the synthesis procedure of selenium nanoparticles stabilized by methylcellulose

A.A. Blinova, A.A. Gvozdenko, Z.A. Rehman, A.V. Blinov, M.A. Taravanov, E.D. Nazaretova

North Caucasus Federal University

DOI: 10.26456/pcascnn/2024.16.758

Original article

Abstract: As a result of the work performed, a method for synthesizing selenium nanoparticles stabilized with methylcellulose was developed and optimized. Selenious acid was used as a selenium-containing precursor, ascorbic acid as a reducing agent, and methylcellulose as a stabilizer. A multifactorial experiment was conducted to optimize the method for synthesizing selenium nanoparticles stabilized with methylcellulose. It was found that for the synthesis of selenium nanoparticles with the smallest average hydrodynamic radius, the molar concentration of selenious acid in the solution should be in the range from 0,0036 to 0,1033 mol/l, the mass of methylcellulose – from 3,0 to 3,985 g, the molar concentration of ascorbic acid – from 1,52 to 2,12 mol/l. It is shown that pH of the medium, charge and concentration of sodium and barium ions do not affect the average hydrodynamic radius of selenium nanoparticles stabilized with methylcellulose. However, when exposed to iron ions, the radius increases from 150 to 270 nm. It is established that an increase in the concentration and charge of anions has a significant effect on the average hydrodynamic radius of selenium nanoparticles stabilized with methylcellulose. With an increase in the concentration of chlorine ions from 0,1 to 1 mol/l, an increase in the average hydrodynamic radius of particles occurred from 143 to 156 nm, with an increase in the concentration of sulfate ions from 0,1 to 1 mol/l, an increase in the average hydrodynamic radius of particles – from 165 to 6129 nm, with an increase in the concentration of phosphate ions from 0,1 to 1 mol/l, an increase in the average hydrodynamic radius of particles – from 149 to 17000 nm.

Keywords: selenium, nanoparticles, methylcellulose, average hydrodynamic radius, optimization

  • Anastasia A. Blinova – Ph. D., Docent, Department of Physics and Technology of Nanostructures and Materials, Faculty of Physics and Technology, North Caucasus Federal University
  • Alexey A. Gvozdenko – Assistant, Department of Physics and Technology of Nanostructures and Material, Faculty of Physics and Technology, North Caucasus Federal University
  • Zafar A. Rehman – Assistant, Department of Physics and Technology of Nanostructures and Material, Faculty of Physics and Technology, North Caucasus Federal University
  • Andrey V. Blinov – Ph. D., Docent, Department of Physics and Technology of Nanostructures and Materials, Faculty of Physics and Technology, North Caucasus Federal University
  • Maxim A. Taravanov – Laboratory Assistant, of the Department of Physics and Technology of Nanostructures and Material, Faculty of Physics and Technology, North Caucasus Federal University
  • Ekaterina D. Nazaretova – Laboratory Assistant, Department of Physics and Technology of Nanostructures and Material, Faculty of Physics and Technology, North Caucasus Federal University

For citation:

Blinova A.A., Gvozdenko A.A., Rehman Z.A., Blinov A.V., Taravanov M.A., Nazaretova E.D. Razrabotka i optimizatsiya metodiki sinteza nanochastits selena, stabilizirovannykh metiltsellyulozoj [Development and optimization of the synthesis procedure of selenium nanoparticles stabilized by methylcellulose], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 758-766. DOI: 10.26456/pcascnn/2024.16.758.

Full article (in Russian): download PDF file

References:

1. Burceva T.I., Selen: essentsial'nyj mikroelement (obzor) [Selenium: an essential trace element], Vestnik Orenburgskogo gosudarstvennogo universiteta [Vestnik of the Orenburg State University], 2006, no. 2 (52-2), pp. 7-9. (In Russian).
2. Akhmedzhanova Z.I., Zhiemuratova G.K., Danilova E.A., Karimov D.A. Makro-i mikroelementy v zhiznedeyatel'nocti organizma i ikh vzaimosvyaz' s immunnoj sistemoj (obzor literatury) [Macro- and microelements in the vital activity of the organism and their relationship with the immune system (literature review)], Zhurnal teoreticheskoj i klinicheskoj meditsiny [Journal of Theoretical and Clinical Medicine], 2020, no. 1, pp. 16-21. (In Russian).
3. Salimadze E.A.O., Kasharnaya O.V., Ermilova T.S., Samburova M.A. Selen i ego biologicheskaya rol' v zhivykh organizmakh [Selenium and its biological role in living organisms], Tendentsii razvitiya nauki i obrazovaniya [Trends in the development of science and education], 2021, no. 80-3, pp. 39-45. (In Russian). DOI: 10.18411/trnio-12-2021-120.
4. Varlamova E.G., Maltseva V.N. Micronutrient selenium: uniqueness and vital functions, Biophysics, 2019, vol. 64, issue 4, pp. 510-521. DOI: 10.1134/S0006350919040213.
5. Burk R.F., Hill K.E. Regulation of selenium metabolism and transport, Annual Review of Nutrition, 2015, vol. 35, pp. 109-134. DOI: 10.1146/annurev-nutr-071714-034250.
6. Skorinova K.D., Kuzmenko V.V., Vasilenko I.A. Perspektiva sozdaniya lekarstvennykh preparatov na osnove nanochastits selena (obzor) [The prospect of creating medicines based on selenium nanoparticles (review)], Razrabotka i registraciâ lekarstvennyh sredstv [Drug development & registration], 2020, vol. 9, no. 2, pp. 33-44. (In Russian).
7. Shurygina I.A., Shurygin M.G. Selenium nanocomposites - the prospects of application in oncology [Selenium nanocomposite promising applications in oncology], Vestnik novykh meditsinskikh tekhnologij [Journal of New Medical Technologies], 2020, vol. 27, no. 1, pp. 81-86. DOI: 10.24411/1609-2163-2020-16517 (In Russian).
8. Egorov N.P., Shafronov O.D., Egorov D.N., Suleimanov E.V. Development and experimental estimation of application efficiency of new nanotechnology fertilizers in crop production [Development and experimental evaluation of the effectiveness of using new types of inventions in crop production obtained using nanotechnology], Vestnik Nizhegorodskogo universiteta im. N.I. Lobachevskogo. [Vestnik of Lobachevsky University of Nizhni Novgorod], 2008, no. 6, pp. 94-99. (In Russian).
9. Geljahov I.M., Kompantsev D.V., Privalov I.M., Stepanova E.F. Sozdanie i issledovanie kosmetsevticheskogo sredstva s biologicheski aktivnymi kompozitsiyami nanoselena [Creation and investigation of a cosmetrovic means with biologically active compositions of a nanoselene], Sovremennye problemy nauki i obrazovaniya [Modern problems of science and education], 2017, no. 5, art. no. 73, 8 p. (In Russian).
10. Perumal S., Samy, M.V.G. Subramanian D., Selenium nanoparticle synthesis from endangered medicinal herb (Enicostema axillare), Bioprocess and Biosystems Engineering, 2021, vol. 44, issue 9, pp. 1853-1863. DOI: 10.1007/s00449-021-02565-z.
11. Kushnir S.E., Kazin P.E., Trusov L.A., Tretyakov Yu.D. Self-organization of micro- and nanoparticles in ferrofluids, Russian Chemical Reviews, 2012, vol. 81, issue 6, pp. 560570, DOI: 10.1070/RC2012v081n06ABEH004250.
12. Kipper A.I., Borovikova L.N., Yakovlev I.V., Pisarev O.A. Synthesis and properties of organo-inorganic composites based on daunomycin, polyvinylpyrrolidone, and selenium nanoparticles, Russian Journal of Applied Chemistry, 2018, vol. 91, issue 1, pp. 121-126. DOI: 10.1134/S1070427218010196.
13. Kravtsov A.A., Chikulina I.S., Vakalov D.S. et al. Issledovanie lyuminestsentsii YAG: Ce, dopirovannogo nanochastitsami serebra [Luminescence of YAG: Ce doped with silver nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 220-227. DOI: 10.26456/pcascnn/2021.13.220.
14. Yasnaya M.A., Blinov A.V., Blinova A.A. et al. Opredelenie optimal'nykh rezhimov izmereniya razmera kolloidnykh chastits metodami fotonno-korrelyatsionnoj i akusticheskoj spektroskopii [Determination of optimal modes for measuring the size of colloidal particles by photon-correlation spectroscopy and acoustic spectroscopy], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 232-242. DOI: 10.26456/pcascnn/2020.12.232.
15. STATISTICA 12.0. Available at: https://statistica.software.informer.com/12.0/ (accessed 02.08.2024).
16. Nejronnye seti. STATISTICA Neural Networks: Metodologiya i tekhnologii sovremennogo analiza dannykh [Neural networks. STATISTICA Neural Networks: Methodology and technologies of modern data analysis], ed. by V.P. Borovikov, 2nd ed. Moscow, Goryachaya Liniya – Telecom Publ., 2008, 392 p. (In Russian).
17. Volkova A.V., Golikova E.V., Ermakova L.E. Photometric study of the kinetics of TiO2 hydrosol coagulation in electrolyte solutions, Colloid Journal, 2012, vol. 74, issue 1, pp. 32-37. DOI: 10.1134/S1061933X11060184.

⇐ Prevoius journal article | Content | Next journal article ⇒