Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Surface structuring of silicon wafers with low-frequency giant pulses YAG:ND laser

A.A. Fronya1,2, A.T. Sahakyan1

1 P.N. Lebedev Physical Institute of the Russian Academy of Sciences
2 National Research Nuclear University MEPhI

DOI: 10.26456/pcascnn/2024.16.738

Original article

Abstract: Experimental results on the silicon wafers irradiation by a low-frequency giant nanosecond pulses neodymium-doped yttrium-aluminum garnet laser with a wavelength of 1,064 μm are presented. The pulse duration at the half-height was 170 ns, and the pulse repetition frequency was 2 Hz. The experiments were carried out for the cases of silicon wafers placements in air and in bidistilled water. For the case of irradiation in air, a nanostructured region with a uniform distribution of particles was succeeded to form on the surface of the silicon wafer. The exposure time was 2 minutes, which corresponded to 240 laser pulses. In this case, the particles were formed mainly from silicon dioxide as a result of the thermal oxidation during ablation in air. When the exposure time was doubled, this effect was not achieved, and destruction areas of wafer were formed. For the case of irradiation in bidistilled water within two and four minutes, the mechanical and thermal destructions prevail on the surface of the silicon wafer, which manifest themselves in cracking along the edges of the crystal structure and in the form of the surface solidified melted regions.

Keywords: laser radiation, nanosecond pulses, silicon, surface structuring, destruction, nanoparticles

  • Anastasiya A. Fronya – Senior Researcher, P.N. Lebedev Physical Institute of the Russian Academy of Sciences, Associate Professor National Research Nuclear University MEPhI
  • Artyom T. Sahakyan – Acting Head of Laboratory, (Laboratory of the Laser Radiation Effect), P.N. Lebedev Physical Institute of the Russian Academy of Sciences

For citation:

Fronya A.A., Sahakyan A.T. Strukturirovanie poverkhnosti kremnievykh plastin gigantskimi impulsami nizkochastotnogo YAG:ND lazera [Surface structuring of silicon wafers with low-frequency giant pulses YAG:ND laser], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 738-745. DOI: 10.26456/pcascnn/2024.16.738. ⎘

Full article (in Russian): download PDF file

References:

1. Haug H., Koch S.W. Quantum theory of the optical and electronic properties of semiconductors, 5th ed. Singapore, World Scientific Publishing, 2009, 484 p. DOI: 10.1142/7184.
2. Handbook of porous silicon, ed. by L Canham. Cham, Springer, 2018, 1000 p. DOI: 10.1007/978-3-319-04508-5.
3. Ishchenko A.A., Fetisov G.V., Aslanov L.A. Nanosilicon: Properties, synthesis, applications, methods of analysis and control, 1st ed. Boca Raton, CRC Press, 2014, 735 p. DOI: 10.1201/b17170.
4. Agranovich V.M., Gartstein Y.N., Litinskaya M. Hybrid resonant organic–inorganic nanostructures for optoelectronic applications, Chemical Reviews, 2011, vol. 111, issue 9, pp. 5179-5214. DOI: 10.1021/cr100156x.
5. Minnullin A.N., Shevtsov S.V. Photoluminescence kinetics of a metastable SiGe/Si layer with ring microstructures on the surface, Bulletin of the Lebedev Physics Institute, 2015, vol. 42, issue 11, pp. 302-304. DOI: 10.3103/S1068335615100061.
6. Nesterov V.Y., Sokolovskaya O.I., Golovan L.A. et al. Laser fragmentation of silicon microparticles in liquids for solution of biophotonics problems, Quantum Electronics, 2022, vol. 52, no. 2, art. no. 160, 11 p. DOI: 10.1070/QEL17984.
7. Zabotnov S.V., Kashaev F.V., Shuleiko D.V. et al. Silicon nanoparticles as contrast agents in the methods of optical biomedical diagnostics, Quantum Electronics, 2017, vol. 47, no. 7, art. no. 638, 9 p. DOI: 10.1070/QEL16380.
8. Gongalsky M.B., Osminkina L.A., Pereira A. et al. Laser-synthesized oxide-passivated bright Si quantum dots for bioimaging, Scientific Reports, 2016, vol. 6, art. no. 24732, 8 p. DOI: 10.1038/srep24732.
9. Low S.P., Williams K.A., Canham L.T., Voelcker N.H. Evaluation of mammalian cell adhesion on surface-modified porous silicon, Biomaterials, 2006, vol. 27, issue 26, pp. 4538-4546. DOI: 10.1016/j.biomaterials.2006.04.015.
10. Fronya A.A., Antonenko S.V., Kharin A.Y. et al. Tailoring Photoluminescence from Si-based nanocrystals prepared by pulsed laser ablation in He-N2 gas mixtures, Molecules, 2020, vol. 25, issue 3, art. no. 440, 11 p. DOI: 10.3390/molecules25030440.
11. Ganichkina K.A., Latukhina N.V. Electrical properties of porous silicon as a biosensor material, Journal of Biomedical Photonics & Engineering, 2020, vol. 6 no. 1, pp. 010306-1-010306-7. DOI: 10.18287/JBPE20.06.010306.
12. Kotkovskiy G.E., Kuzishchin Y.A., Martynov I.L. et al. The photophysics of porous silicon: technological and biomedical implications, Physical Chemistry Chemical Physics, 2012, vol. 14, issue 40, pp. 13890-13902. DOI:10.1039/c2cp42019h.
13. Marks M.R., Cheong K.Y., Hassan Z. A review of laser ablation and dicing of Si wafers, Precision Engineering, 2022, vol. 73, pp. 377-408. DOI: 10.1016/j.precisioneng.2021.10.001.
14. Jee Y., Becker M.F., Walser R.M. Laser-induced damage on single-crystal metal surfaces, Journal of the Optical Society of America B, 1988, vol. 5, issue 3, pp. 648-659. DOI: 10.1364/JOSAB.5.000648.
15. Nguyen P.T., Jang J., Kim S.-M. et al. Nanosecond laser-induced reshaping of periodic silicon nanostructures, Current Applied Physics, 2021, vol. 22, pp. 43-49. DOI: 10.1016/j.cap.2020.12.003.
16. Kuznetsov L.G., Pyshkov N.I., Svyakhovsky S.E. Local laser oxidation of porous silicon photonic crystals, Technical Physics Letters, 2023, vol. 49, issue 8, pp. 61-63. DOI: 10.61011/TPL.2023.08.56691.19610.

⇐ Prevoius journal article | Content | Next journal article ⇒