Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


On the profile characteristics of technical surfaces as applied to nanoroughness

V.V. Izmailov, M.V. Novoselova

Tver State Technical University

DOI: 10.26456/pcascnn/2024.16.643

Original article

Abstract: The parameters of the structure of a technical surface at the nanoscale level, determined by the profile method, are considered. The possibility of applying the parameters determined in accordance with domestic and international standards for the roughness profile (microscale level) to the characteristics of the surface at the nanoscale level, which goes beyond the standards, is shown. This possibility is provided by the model of the profile of a technical surface that underlies modern standards as an implementation of a broadband random normal process. An experimental verification of the normality of the process was carried out by comparing the experimental values of the integral probability distribution function of the profile ordinates with theoretical values that obey the normal distribution. The experimentally obtained values of the nine most important parameters, as well as their some relationships between them, are presented, confirming the reliability of the surface profile model as a normal random process. The use of standard surface profile parameters ensures to avoid errors and misunderstandings associated with ambiguous interpretation of one or another parameter.

Keywords: surface structure, nanoroughness, profile method, profile parameters, normal random process

  • Vladimir V. Izmailov – Dr. Sc., Professor, Department of Applied Physics,, Tver State Technical University
  • Marina V. Novoselova – Ph. D., Docent, Department of Applied Physics, Tver State Technical University

For citation:

Izmailov V.V., Novoselova M.V. O profilnykh kharakteristikakh tekhnicheskikh poverkhnostej primenitelno k nanosherokhovatosti [On the profile characteristics of technical surfaces as applied to nanoroughness], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 643-650. DOI: 10.26456/pcascnn/2024.16.643. ⎘

Full article (in Russian): download PDF file

References:

1. Ivanov I.A., Gubenko S.V., Kononov D.P. Poverkhnost' detalei mashin i mekhanizmov : uchebnoe posobie dlya vuzov [The surface of machine parts and mechanisms: a textbook for universities]. Sankt-Peterburg: Lan', 2021, 156 p. (In Russian).
2. GOST R ISO 4287-2014. Geometricheskie kharakteristiki izdelij (GPS). Struktura poverkhnosti. Profil'nyj metod. Terminy, opredeleniya i parametry struktury poverkhnosti [Russian State Standard ISO 4287-2014 Geometrical Product Specifications (GPS). Surface texture. Profile method. Terms, definitions and surface texture parameters]. Moscow, Standartinform Publ., 2014. 20 p. (In Russian).
3. GOST 2789-73. Sherokhovatost' poverkhnosti. Parametry i kharakteristiki [Surface roughness. Parameters and characteristics]. Moscow, Standartinform Publ., 2018. 7 p. (In Russian).
4. GOST 25145-82. Sherokhovatost' poverkhnosti. Terminy i opredeleniya [Surface roughness. Terms and definitions]. Moscow, Standart Publ., 1982. 20 p. (In Russian).
5. ISO 4287:1997. Geometrical Product Specifications (GPS) – Surface texture: Profile method – Terms, definitions and surface texture parameters. Geneva, ISO copyright office, 1997. 36 p.
6. ISO 21920-2:2021. Geometrical product specification (GPS) – Surface texture: Profile – Part 2: Terms, definitions, and surface texture parameters. Geneva, ISO copyright office, 2021. 78 p.
7. Ivanov D.V., Antonov A.S., Sdobnyakov N.YU. et. al. Fraktal'nye svojstva nanorazmernykh plenok nikelya i khroma [Fractal properties of nano-sized films of nickel and chromium] // Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 138-152. DOI: 10.26456/pcascnn/2019.11.138. (In Russian).
8. Antonov A.S., Sdobnyakov N.YU., Ivanov D.V., Podbolotov K.B. Issledovanie morfologii rel'efa plenok medi na poverkhnosti slyudy [Research of morphology of the relief of copper films on the mica surface], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2017, issue 9, pp. 19-26. DOI: 10.26456/pcascnn/2017.9.019. (In Russian).
9. Ivanov D.V., Antonov A.S., Semenova E.M. et. al. Razlichnye skhemy polucheniya fraktal'nogo rel'efa nanorazmernykh plenok platiny [Different schemes for obtaining fractal relief of nanosized platinum films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 156-165. DOI: 10.26456/pcascnn/2021.13.156. (In Russian).
10. Izmailov V.V., Novoselova M.V. Vliyanie nanotopografii poverkhnostej na kharakteristiki diskretnogo kontakta tverdykh tel [The influence of surfaces nanotopography on characteristics of solids discrete contact], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2016, issue 8, pp. 139-144. (In Russian).
11. Izmailov V.V., Novoselova M.V. O parametrakh nanotopografii tekhnicheskoj poverkhnosti i eyo profilya [On nanotopographic parameters of engineering surface and its profile], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2018, issue 10, pp. 313-321. DOI: 10.26456/pcascnn/2018.10.313. (In Russian).
12. Grigor'ev A.YA. Fizika i mikrogeometriya tekhnicheskikh poverkhnostei [Physics and microgeometry of engineering surfaces]. Minsk: Belaruskaya navuka, 2016, 247 p. (In Russian).
13. Whitehouse D. Surfaces and their measurement. Oxford, Elsevier Science & Technology, 2004. 432 p.

⇐ Prevoius journal article | Content | Next journal article ⇒