Synthesis of phase-change material Ge2Sb2Te5 nanoparticles by laser-induced forward transfer techniques
A.A. Burtsev, V.A. Mikhalevsky, A.A. Nevzorov, A.V. Kiselev, M.R. Konnikova, V.V. Ionin, N.N. Eliseev, A.A. Lotin
National Research Centre «Kurchatov Institute»
DOI: 10.26456/pcascnn/2024.16.612
Original article
Abstract: Experimental results on the synthesis of nanoparticles of Ge2Sb2Te5 phase-change material by the direct laser-induced transfer method are presented. Thin films obtained by the thermal vacuum deposition were used as a donor material and silicon wafers as an acceptor. The laser-induced forward transfer was carried out using the sub-nanosecond pulsed laser irradiation. The morphology, topology, and size of the obtained nanoparticles were analyzed by scanning electron microscopy. Structural studies were performed by Raman scattering. A quasi-uniform distribution of nanoparticles on the substrate and a quasi-uniform size distribution were achieved. It was shown that it is possible to achieve a nanoparticle diameter of less than 100 nm. Raman spectra show that the nanoparticles obtained are in the crystalline state. The results show the possibility of creating an element based on nanoparticles with a specific distribution in size as a technological alternative to devices based on thin films. The use of nanoparticles will make it possible to achieve the energy efficiency, greater flexibility, and smoothness of switching as well as to realize neuromorphic and stochastic computation.
Keywords: chalcogenides, phase-change materials, nanoparticles, nanoclusters, laser-induced forward transfer, phase transitions
- Anton A. Burtsev – Researcher, National Research Centre «Kurchatov Institute»
- Vladimir A. Mikhalevsky – Researcher, National Research Centre «Kurchatov Institute»
- Alexey A. Nevzorov – Ph. D., Researcher, National Research Centre «Kurchatov Institute»
- Alexey V. Kiselev – Ph. D., Researcher, National Research Centre «Kurchatov Institute»
- Maria R. Konnikova – Junior Researcher, National Research Centre «Kurchatov Institute»
- Vitaly V. Ionin – Researcher, National Research Centre «Kurchatov Institute»
- Nikolay N. Eliseev – Junior Researcher, National Research Centre «Kurchatov Institute»
- Andrey A. Lotin – Ph. D., Deputy Head of the branch, National Research Centre «Kurchatov Institute»
For citation:
Burtsev A.A., Mikhalevsky V.A., Nevzorov A.A., Kiselev A.V., Konnikova M.R., Ionin V.V., Eliseev N.N., Lotin A.A. Poluchenie nanochastits fazoizmenyaemogo materiala Ge2Sb2Te5 metodom pryamogo lazernoindutsirovannogo perenosa [Synthesis of phase-change material Ge2Sb2Te5 nanoparticles by laser-induced forward transfer techniques], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 612-620. DOI: 10.26456/pcascnn/2024.16.612. ⎘
Full article (in Russian): download PDF file
References:
1. Phase change materials: science and applications, ed. by S. Raoux and M. Wutting. New York, Springer Science+Business Media, LLC, 2009, 450 p. DOI: 10.1007/978-0-387-84874-7.
2. Kolobov A.V., Tominaga J. Chalcogenides: metastability and phase change phenomena. Berlin, Heidelberg, Springer-Verlag, 2012, XVI+284 p. DOI: 10.1007/978-3-642-28705-3.
3. Kozyukhin S.A., Lazarenko P.I., Popov A.I., Eremenko I.L. Phase change memory materials and their applications, Russian Chemical Reviews, 2022, vol. 91, issue 9, art. no. RCR5033, 37 p. DOI: 10.1070/RCR5033.
4. Ovshinsky S.R. Reversible electrical switching phenomena in disordered structures, Physical Review Letters, 1968, vol. 21, issue 20, pp. 1450-1453. DOI: 10.1103/PhysRevLett.21.1450.
5. Feinleib J, DeNeufville J., Moss S.C., Ovshinsky S.R. Rapid reversible light‐induced crystallization of amorphous semiconductors, Applied Physics Letters, 1971, vol. 18, issue 6, pp. 254-257. DOI: 10.1063/1.1653653.
6. Yamada N., Ohno E., Nishiuchi K. et al. Rapid‐phase transitions of GeTe‐Sb2Te3 pseudobinary amorphous thin films for an optical disk memory, Journal of Applied Physics, 1991, vol. 69, issue 5, pp. 2849-2856. DOI: 10.1063/1.348620.
7. Wuttig M., Yamada N. Phase-change materials for rewriteable data storage, Nature Materials, 2007, vol. 6, issue 11, pp. 824-832. DOI: 10.1038/nmat2009.
8. Sarwat S.G. Materials science and engineering of phase change random access memory, Materials Science and Technology, 2017, vol. 33, issue 16, pp. 1890-1906. DOI: 10.1080/02670836.2017.1341723.
9. Papandreou N., Pantazi A., Sebastian A. et al. Multilevel phase-change memory, 17th IEEE International Conference on Electronics, Circuits and Systems, 12-15 December 2010, Athens, New York, IEEE Publ., 2010, pp. 1017-1020. DOI: 10.1109/ICECS.2010.5724687.
10. Guo P., Sarangan A. M., Agha I. A review of germanium-antimony-telluride phase change materials for non-volatile memories and optical modulators, Applied Sciences, 2019, vol. 9, issue 3, art. no. 530, 26 p. DOI: 10.3390/app9030530.
11. Wuttig M., Raoux S. The science and technology of phase change materials, Zeitschrift für anorganische und allgemeine Chemie, 2012, vol. 638, issue 15, pp. 2455-2465. DOI: 10.1002/zaac.201200448.
12. Zhang W., Mazzarello R., Wuttig M., Ma E. Designing crystallization in phase-change materials for universal memory and neuro-inspired computing, Nature Reviews Materials, 2019, vol. 4, issue 3, pp. 150-168. DOI: 10.1038/s41578-018-0076-x.
13. Suzdalev I.P. Elektricheskie i magnitnye perekhody v nanoklasterakh i nanostrukturakh [Electrical and magnetic transitions in nanoclusters and nanostructures], Moscow, URSS, 2016, 480 p. (In Russian).
14. Suzdalev I.P. Nanotekhnologiya: Fiziko-khimiya nanoklasterov, nanostruktur i nanomaterialov [Nanotechnology: Physical chemistry of nanoclusters, nanostructures and nanomaterials], Moscow, URSS, 2017, 592 p. (In Russian).
15. Casarin B., Caretta A., Chen B. et al. Ultralow-fluence single-shot optical crystalline-to-amorphous phase transition in Ge–Sb–Te nanoparticles, Nanoscale, 2018, vol. 10, issue 35, pp. 16574-16580. DOI: 10.1039/c8nr04350g.
16. Caretta A., Casarin B., Chen B., et al. Ultrafast response of Ge2Sb2Te5 nanoparticles: The benefits of low energy amorphization switching with the same read/write speed of bulk memories, APL Materials, 2023, vol. 11, art. no. 071117, pp. 071117-1-071117-5. DOI: 10.1063/5.0156207.
17. Arachchige I.U., Soriano R., Malliakas C.D. et al. Amorphous and crystalline GeTe nanocrystals, Advanced Functional Materials, 2011, vol. 21, issue 14, pp. 2737-2743. DOI: 10.1002/adfm.201100633.
18. Morales M., Munoz-Martin D., Marquez A. et al. Laser-induced forward transfer techniques and applications, Advances in Laser Materials Processing, 2nd ed. Technology, Research and Applications Woodhead Publishing Series in Welding and Other Joining Technologies, Coventry, Woodhead Publishing, 2018, chapter 13, pp. 339-379. DOI: 10.1016/B978-0-08-101252-9.00013-3.
19. Kiselev A.V., Ionin V.V., Burtsev A.A. et al. Dynamics of reversible optical properties switching of Ge2Sb2Te5 thin films at laser-induced phase transitions, Optics & Laser Technology, 2022, vol. 147, art. no. 107701, 6 p. DOI: 10.1016/j.optlastec.2021.107701.
20. Burtsev A.A., Eliseev N.N., Mikhalevsky V.A. et a. Physical properties’ temperature dynamics of GeTe, Ge2Sb2Te5 and Ge2Sb2Se4Te1 phase change materials, Materials Science in Semiconductor Processing, 2022, vol. 150, art. no. 106907, 8 p. DOI: 10.1016/j.mssp.2022.106907.
21. Zhu Z., Liu F.R., Huang Y.N. Raman study on the crystallization characteristics of amorphous Ge2Sb2Te5 film, Applied Mechanics and Materials, 2014, vol. 541-542, pp. 229-233. DOI: 10.4028/www.scientific.net/AMM.541-542.229.