Abstract: The work is devoted to studying the possibility of using synthetic zeolites (nanodispersed hydroxyapatite and mechanically activated hydroxyapatite-zeolite mixture in a ratio of 1:1) as sorbents of chromium and nickel ions from the acidic aqueous solutions. The chemical qualitative and quantitative composition, morphology of the initial reagents and the obtained solutions were studied. It was found that the synthetic zeolite and the hydroxyapatite-zeolite mixture exhibit high sorption activity and sorption capacity with respect to chromium ions (the extraction degree of 99,96%), while nanodispersed hydroxyapatite allows obtaining the extraction degree of 98,73. As for the sorption of nickel from a solution, it was shown that the maximum extraction degree is achieved using the hydroxyapatite-zeolite sorbent (63,83%). The conducted studies allow us to recommend the obtained samples for use as sorbents for cleaning industrial waste solutions from toxic impurities, as well as for further studies with the aim of introducing it not only for the extraction of various ions from aqueous solutions, but also for use in various industries.

Keywords: purification, synthetic zeolite, hydroxyapatite, sorption, heavy metals, aluminosilicate, nickel, chromium

  • Svetlana A. Bibanaeva – Researcher, Laboratory of Heterogeneous Processes in Chemistry, Institute of Solid State Chemistry of the Ural Branch of RAS
  • Vladimir M. Skachkov – Ph.D., Senior Researcher, Laboratory of Heterogeneous Processes in Chemistry, Institute of Solid State Chemistry of the Ural Branch of RAS
  • Nail A. Sabirzyanov – D. Sc., Chief Researcher, Laboratory of Heterogeneous Processes in Chemistry, Institute of Solid State Chemistry of the Ural Branch of RAS

For citation:

Bibanaeva S.A., Skachkov V.M., Sabirzyanov N.A. Sorbtsionnaya ochistka rastvorov sinteticheskimi tseolitami [Sorption purification of solutions with synthetic zeolites], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 584-591. DOI: 10.26456/pcascnn/2024.16.584. ⎘

Full article (in Russian): download PDF file

References:

1. Timofeev K.L., Krayukhin S.A., Mal'tsev G.I. Sorbtsionnaya ochistka nikelevykh rastvorov ot metallov-primesej [Sorption purification of nickel solutions of metal impurities], Vestnik Yuzhno-Ural'skogo gosudarstvennogo universiteta. Seriya «Metallurgiya» [South Ural State University Bulletin. Series «Metallurgy»], 2016, vol. 16, no. 1, pp. 157-165. DOI: 10.14529/met160123. (In Russian).
2. Linnikov O.D., Rodina I.V. Ochistka rastvorov ot ionov nikelya pri ispol'zovanii v kachestve koagulyanta khlorida zheleza(III) [Purification of solutions from nickel ions using iron(III) chloride as a coagulant], Rossijskij khimicheskij zhurnal [Russian Chemical Journal], 2021, vol. 65, no.2, pp. 83-89. DOI: 10.6060/rcj.2021652.7. (In Russian).
3. Bora A.J., Dutta R.K. Removal of metals (Pb, Cd, Cu, Cr, Ni, and Co) from drinking water by oxidation-coagulation-absorption at optimized pH, Journal of Water Process Engineering, 2019, vol. 31, art. no. 100839, 9 p. DOI: 10.1016/j.jwpe.2019.100839.
4. Ye Q., Li Q., Li X. Removal of heavy metals from wastewater using biochars: adsorption and mechanisms, Enviromental Pollutants and Bioavailability, 2022, vol. 34, issue 1, pp. 385-394. DOI: 10.1080/26395940.2022.2120542.
5. Kobya M. Removal of Cr (VI) from aqueous solutions by adsorption onto hazelnut shell activated carbon: kinetic and equilibrium studies, Bioresource Technology, 2004, vol. 91, issue. 3, pp. 317-321. DOI: 10.1016/j.biortech.2003.07.001.
6. Al-Shannag M., Al-Qodah Z., Bani-Melhem K. et al. Heavy metal ions removal from metal plating wastewater using electrocoagulation: kinetic study and process performance, Chemical Engineering Journal, 2015, vol. 260, pp. 749-756. DOI: 10.1016/j.cej.2014.09.035.
7. Dermentzis K., Valsamidou E., Lazaridou A., Kokkinos N. Nickel removal from wastewater by electrocoagulation with aluminum electrodes, Journal of Engineering Science and Technology Review, 2011, vol. 4, issue. 2, pp. 188-192. DOI: 10.25103/JESTR.042.12.
8. Kim T., Kim T-K., Zoh K-D. Removal mechanism of heavy metal (Cu, Ni, Zn, and Cr) in the presence of cyanide during electrocoagulation using Fe and Al electrodes, Journal of Water Process Engineering, 2020, vol. 33, art. no.101109, 9 p. DOI: 10.1016/j.jwpe.2019.101109.
9. Narayanan N.V., Ganesan M. Use of adsorption using granular activated carbon (GAC) for the enhancement of removal of chromium from synthetic wastewater by electrocoagulation, Journal of Hazardous Materials, 2009, vol. 161, issue 1, pp. 575-580. DOI: 10.1016/j.jhazmat.2008.03.113.
10. Ait Ouaissa Y., Chabani M., Amrane A., Bensmaili A. Removal of Cr (VI) from model solutions by a combined electrocoagulation sorption process, Chemical Engineering & Technology, 2013, vol. 36, issue 1, pp. 147-155. DOI: 10.1002/ceat.201200375.
11. Mutongo F., Kuipa O., Kuipa PK. Removal of Cr (VI) from aqueous solutions using powder of potato peelings as a low cost sorbent, Bioinorganic Chemistry and Applications, 2014, vol. 2014, issue 1, 7 p. DOI: 10.1155/2014/973153.
12. Bogdanova E.A., Skachkov V.М., Medyankina I.S. et al. Formation of nanodimensional structures in precipitated hydroxyapatite by fluorine substitution, SN Applied Sciences, 2020, vol. 2, issue 9, art. no. 1565, 7 p. DOI: 10.1007/s42452-020-03388-5.
13. Velarde L., Nabavi M.S., Escalera E. et al. Adsorption of heavy metals on natural zeolites: a review, Chemosphere, 2023, vol. 328, art. no. 138508, 16 p. DOI: 10.1016/j.chemosphere.2023.138508.
14. Ain Q.U., Zhang H., Yaseen M. et al. Facile fabrication of hydroxyapatite-magnetite-bentonite composite for efcient adsorption of Pb (II), Cd (II), and crystal violet from aqueous solution, Journal of Cleaner Production, 2020, vol. 247, art. no. 119088, 52 p. DOI:10.1016/j.jclepro.2019.119088.
15. Bibanaeva S.A., Skachkov V.M. Sorbtsiya tyazhelykh metallov iz vodnykh rastvorov sinteticheskimi tseolitami [Sorption of heavy metals from aqueous solutions with synthetic zeolites], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue.15, pp. 924-929. DOI: 10.26456/pcascnn/2023.15.924. (In Russian).
16. Bibanaeva S.A., Bogdanova E.A., Skachkov V.M. Sintez i issledovanie funktsional'nykh kharakteristik kompozitsionnykh materialov na osnove nanorazmernogo gidroksiapatita i sinteticheskikh tseolitov [Synthesis and investigation of functional characteristics of composite materials based on nanoscale hydroxyapatite and synthetic zeolites], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue.15, pp.913-923. DOI: 10.26456/pcascnn/2023.15.913. (In Russian).

⇐ Prevoius journal article | Content | Next journal article ⇒