Some features of localization of Al, Ga and In impurities in ZnO layers

A.K. Akhmedov1, A.Sh. Asvarov2, E.K. Murliev1, Z.V. Shomakhov3

1 Institute of Physics, Dagestan Federal Research Center of RAS
2 Shubnikov Institute of Crystallography, Kurchatov Complex of Crystallography and Photonics, National Research Center «Kurchatov Institute»
3 Kabardino-Balkarian State University named after H.M. Berbekov

DOI: 10.26456/pcascnn/2024.16.575

Original article

Abstract: Reducing the cost of the materials and technologies used to form functional films is one of the most pressing issues in the rapidly developing transparent electronics industry. In this regard, ZnO-based films deposited by magnetron sputtering are of particular interest, being considered as a real alternative to more expensive indium oxide films when forming transparent electrodes in various optoelectronic applications. However, the choice of optimal film’s compositions and formation modes for each specific application is complicated by the lack of systematic comparative data on these systems obtained under identical conditions. In this work, ZnO films doped with Al, Ga, and In at a level of 1 to 20 at.% were obtained under identical conditions by the magnetron sputtering method. The dependence of the structure and electrical characteristics of ZnO films on the dopant content and deposition temperature was studied. It has been established that the key factors determining the behavior of an impurity in a ZnO matrix are its chemical activity, solubility in the matrix, the ionic radius of the impurity metal in a given coordination, and the electrical characteristics of additional oxide phases of the doping element formed at grain boundaries.

Keywords: thin film, magnetron sputtering, transparent electrode, zinc oxide, doping, carrier transport, microstructure, grain boundary

  • Akhmed K. Akhmedov – Ph. D., Leading Researcher, Institute of Physics, Dagestan Federal Research Center of RAS
  • Abil Sh. Asvarov – Ph. D., Senior Researcher, Shubnikov Institute of Crystallography, Kurchatov Complex of Crystallography and Photonics, National Research Center «Kurchatov Institute»
  • Eldar K. Murliev – Junior Researcher, Institute of Physics, Dagestan Federal Research Center of RAS
  • Zamir V. Shomakhov – Ph. D., Director of the Institute of artificial intelligence and digital technologies, Kabardino-Balkarian State University named after H.M. Berbekov

For citation:

Akhmedov A.K., Asvarov A.Sh., Murliev E.K., Shomakhov Z.V. Osobennosti lokalizatsii primesi Al, Ga i In v sloyakh na osnove ZnO [Some features of localization of Al, Ga and In impurities in ZnO layers], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 575-583. DOI: 10.26456/pcascnn/2024.16.575.

Full article (in Russian): download PDF file

References:

1. Liu H., Avrutin V., Izyumskaya N., Özgür Ü., Morkoç H. Transparent conducting oxides for electrode applications in light emitting and absorbing devices, Superlattices and Microstructures, 2010, vol. 48, issue 5, pp. 458-484. DOI: 10.1016/j.spmi.2010.08.011.
2. Minami T. Transparent conducting oxide semiconductors for transparent electrodes, Semiconductors Science and Technology, 2005, vol. 20, no. 4, pp. S35-S44. DOI: 10.1088/0268-1242/20/4/004.
3. Stadler A. Transparent conducting oxides – an up-to-date overview, Materials, 2012, vol. 5, issue 4, pp. 661-683. DOI: 10.3390/ma5040661.
4. Liu Y., Li Y., Zeng H. ZnO-based transparent conductive thin films: doping, performance, and processing, Journal of Nanomaterials, 2013, vol. 2013. art. id 196521, 9 p. DOI: 10.1155/2013/196521.
5. Bikowski A., Ellmer K. Analytical model of electron transport in polycrystalline, degenerately doped ZnO films, Journal of Applied Physics, 2014, vol. 116, issue 14, pp. 143704-1-143704-11. DOI: 10.1063/1.4896839.
6. Akhmedov A.K., Asvarov A. Sh., Muslimov A.E., Kanevsky V.M. A multi-position drum-type assembly for simulaneos film deposition at different temperatures in a single sputter cycle – application to ITO thin films, Coatings, 2020, vol. 10, issue 11, art. no. 1076, 9 p. DOI: 10.3390/coatings10111076.
7. Serier H., Gaudon M., Ménétrier M. Al-doped ZnO powdered materials: Al solubility limit and IR absorption properties, Solid State Sciences, 2009, vol. 11, issue 7, pp. 1192-1197. DOI: 10.1016/j.solidstatesciences.2009.03.007.
8. Shirouzu K., Ohkusa T., Hotta M., Enomoto N., Hojo J. Distribution and solubility limit of Al in Al2O3-doped ZnO sintered body, Journal of the Ceramic Society of Japan, 2007, vol. 115, issue 1340, pp. 254-258. DOI: 10.2109/jcersj.115.254.
9. Mickan M., Helmersson U., Horwat D. Effect of substrate temperature on the deposition of Al-doped ZnO thin films using high power impulse magnetron sputtering, Surface and Coatings Technology, 2018, vol. 347, pp. 245-251. DOI:10.1016/j.surfcoat.2018.04.089.
10. Lalanne M., Soon J.M., Barnabe A. et al. Preparation and characterization of the defect–conductivity relationship of Ga-doped ZnO thin films deposited by nonreactive radio-frequency–magnetron sputtering, Journal of Materials Research, 2010, vol. 25, issue 12, pp. 2407-2414. DOI: 10.1557/jmr.2010.0300.
11. Wang R., Sleight A.W., Cleary D. High conductivity in gallium-doped zinc oxide powders, Chemistry of Materials, 1996, vol. 8. issue 2, pp. 433-439. DOI: 10.1021/cm950372k.
12. Yoon M.H., Lee S.H., Park H.L. et al. Solid solubility limits of Ga and Al in ZnO, Journal of Materials Science Letters, 2002, vol. 21, issue 21, pp. 1703-1704. DOI: 10.1023/A:1020841213266.
13. Lu Zh.-L., Zou W.-Q., Xu M.-X. et al. Structural and electrical properties of single crystalline Ga-doped ZnO thin films grown by molecular beam epitaxy, Chinese Physics Letters, 2009, vol. 26, no. 11, art. no. 116102, 4 p. DOI: 10.1088/0256-307X/26/11/116102
14. Martins R., Almeida P., Barquinha P. et al. Electron transport and optical characteristics in amorphous indium zinc oxide films, Journal of Non-Crystalline Solids, 2006, vol. 352, issue 9-20, pp. 1471-1474. DOI: 10.1016/j.jnoncrysol.2006.02.009.

⇐ Prevoius journal article | Content | Next journal article ⇒