Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Analysis of thermal stability of the internal structure of Ag-Cu nanoparticles

A.A. Cherepovskaya, S.L. Gafner, Yu.Ya. Gafner, D.A. Ryzhkova

Khakass State University

DOI: 10.26456/pcascnn/2024.16.557

Short communication

Abstract: Binary nanoparticles of the copper-silver alloy of are of great practical interest due to the possibility of fine-tuning their physical and chemical properties by changing the composition, size, shape and structure ofnanoparticles. The processes of formation of the internal structure of Ag-Cu nanoparticles with a diameter from 2.0 to 8.0 nm during their crystallization with three different rates of thermal energy dissipation were studied by the molecular dynamics method. The features of this process were found to be dependent on the target chemical composition of nanoparticles, their size and the intensity of the thermal energy dissipation. The actual appearance and structure of the studied nanoparticles were determined using OVITO and xmakemol visualizers. It was shown that as a result of crystallization from the melt of binary Ag-Cu nanoparticles, metastable states that are sufficiently stable at room temperature (300 K), and the stability of such states after annealing at a temperature of 600 K is also evaluated.

Keywords: binary alloys, copper, silver, nanoparticles, structure, crystallization, metastable states, computer modeling, strong coupling

  • Arina A. Cherepovskaya – 2nd year graduate student of specialty «Modern digital technologies in education», Khakass State University
  • Svetlana L. Gafner – Dr. Sc., Docent, Professor of the Department of Mathematics, Physics and Information Technology, Khakass State University
  • Yury Ya. Gafner – Dr. Sc., Professor, Chief of the Department of Mathematics, Physics and Information Technology, Khakass State University
  • Daria A. Ryzhkova – 4th year postgraduate student, Senior Lecturer, Department of Mathematics, Physics and Information Technology, Khakass State University

For citation:

Cherepovskaya A.A., Gafner S.L., Gafner Yu.Ya., Ryzhkova D.A. Analiz termicheskoj ustojchivosti vnutrennego stroeniya nanochastits Ag-Cu [Analysis of thermal stability of the internal structure of Ag-Cu nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 557-564. DOI: 10.26456/pcascnn/2024.16.557.

Full article (in Russian): download PDF file

References:

1. Bochicchio D., Ferrando R., Panizon E., Rossi G. Structures and segregation patterns of Ag-Cu and Ag-Ni nanoalloys adsorbed on MgO(001), Journal of Physics: Condensed Matter, 2016, vol. 28, no. 5, art.no. 064005, 13 p. DOI: 10.1088/0953-8984/28/6/064005.
2. Nelli D., El Yakout El Koraychy, Cerbelaud M. et. al. Two-steps versus one-step solidification pathways of binary metallic nanodroplets, ACS Nano, 2023, vol. 17, issue 1, pp. 587-596. DOI: 10.1088/0953-8984/28/6/064005.
3. Rapetti D., Roncaglia C., Ferrando R. Optimizing the shape and chemical ordering of nanoalloys with specialized walkers, Advanced Theory and Simulations, 2023, vol. 6, issue 9, art.no. 2300268, 13 p. DOI: 10.1002/adts.202300268.
4. Nelli D., Ferrando R. Core-shell vs. multi-shell formation in nanoalloy evolution from disordered configurations, Nanoscale, 2019, vol. 11, issue 27, pp. 13040-13050. DOI: 10.1039/C9NR02963J.
5. Ryzhkova D.A., Gafner S.L., Gafner Yu.Ya. Use of eutectic effects in the possible creation of phase-change memory cells based on Ag-Cu nanoclusters, Physics of Metals and Metallography, 2023, vol. 124, issue 10, pp. 1041-1048. DOI: 10.1134/S0031918X23601634.
6. Gafner Yu., Gafner S., Redel L., Zamulin I. Dual structural transition in small nanoparticles of Cu-Au alloy, Journal of Nanoparticle Research, 2018, vol. 20, no. 2, art.no. 51,14 p. DOI: 10.1007/s11051-018-4161-2.
7. Rapallo A., Rossi G., Ferrando R. et al. Global optimization of bimetallic cluster structures. I. Size-mismatched Ag-Cu, Ag-Ni, and Au-Cu systems, The Journal of Chemical Physics, 2005, vol. 122, issue 19, pp. 194308-1-194308-13. DOI: 10.1063/1.1898223.
8. Dubkov S.V., Savitskiy A.I., Trifonov A.Yu. et.al. SERS in red spectrum region through array of Ag–Cu composite nanoparticles formed by vacuum-thermal evaporation, Optical Materials: X, 2020, vol. 7, art.no. 100055, 9 p. DOI: 10.1016/j.omx.2020.100055.
9. Gromov D.G., Dubkov S.V., Savitskiy A.I. et. al. Optimization of nanostructures based on Au, Ag, Au-Ag nanoparticles formed by thermal evaporation in vacuum for SERS applications, Applied Surface Science, 2019, vol. 489, pp. 701-707. DOI: 10.1016/j. apsusc.2019.05.286.
10. Gafner Yu.Ya., Gafner S.L., Ryzkova D.A., Nomoev A.V. The role of gold atom concentration in the processes of formation of Cu-Au nanoparticles from the gas phase, Beilstein Journal of Nanotechnology, 2021, vol. 12, pp. 72-81. DOI: 10.3762/bjnano.12.6.

⇐ Prevoius journal article | Content | Next journal article ⇒