Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Equation of interphase adsorption equilibrium

A.V. Tvardovskiy

Tver State Technical University

DOI: 10.26456/pcascnn/2024.16.419

Original article

Abstract: Despite intensive development of adsorption science, there are still many unresolved issues. In this regard, at least one of them can be highlighted in the present paper. As early as 1927 [1], it was established that solids change their dimensions during adsorption of gases and vapors. However, the development of research in this area was hampered for a long time by the lack of theoretical concepts and great experimental and methodological difficulties. Meanwhile, the study of the deformation of solids during adsorption is of great importance both for the development of adsorption thermodynamics and for practical purposes. In the theory of adsorption, a method for describing adsorption equilibrium is widely used, in which the role of a solid is reduced only to the creation of an adsorption force field in which the adsorbate is located. The adsorbent itself is considered thermodynamically inert. It is obvious that the analysis of a two-component system is replaced byconsideration of only one component – the adsorbate. However, the very fact of the existence of deformation of a solid during adsorption directly indicates the insufficient rigor of the description of adsorption equilibrium in the language of concepts of the one-component system, as was accepted in deriving, for example, the classical Henry, Langmuir or BET (Brunauer-Emmett-Teller) equations. Therefore, the greatest value is represented by those works in which attempts are made to construct a general theory of adsorption (and absorption), including phenomena on deformable adsorbents (absorbents). From such a general equation, as special cases, at least the known classical adsorption equations should follow. In work [2], such an equation was proposed and it was shown that from it, as special cases, follow the classical Henry, Langmuir and BET equations with constants that have a clear physical meaning. Thus, the constant in the Henry equation is determined by temperature, the specific surface area adsorbent, size of adsorbate molecules, molar mass of adsorbate, and the isosteric heat of adsorption (the energy of interaction of the adsorbate molecules with the adsorbent surface). In the derived particular BET equation, in contrast to the classical version, a clear dependence of the equation constant on specific physical characteristics of the adsorption system is indicated for the first time. It is determined by the concentration of adsorbate molecules in the liquid phase at temperature under consideration, concentration of adsorbate molecules during the formation of a dense monolayer on the adsorbent surface, the energy of interaction of adsorbate molecules with the adsorbent surface, and the heat of condensation. The approach presented in this work can serve as a basis for modeling a wide variety of adsorption and absorption phenomena, including adsorption on microporous adsorbents and deformable bodies. The present work continues the studies conducted. It is shown that particular cases of the equation presented in [2] are the well-known classical Fowler-Guggenheim, Temkin equations.

Keywords: adsorption, adsorbent, absorption, thermodynamics of phase equilibria, Henry equation, Langmuir equation, Brunauer-Emmett-Teller equation, Fowler-Guggenheim equation, Temkin equation

  • Andrey V. Tvardovskiy – Dr. Sc., Professor, Rector, Tver State Technical University

For citation:

Tvardovskiy A.V. Uravnenie mezhfaznogo adsorbtsionnogo ravnovesiya [Equation of interphase adsorption equilibrium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 419-426. DOI: 10.26456/pcascnn/2024.16.419.

Full article (in Russian): download PDF file

References:

1. Meehan F.T. The expansion of charcoal on sorption of carbon dioxide, Proceedings of the Royal Society of London. Series A, Containing Papers of a Mathematical and Physical Character, 1927, vol. 115, issue 770, pp. 199-207. DOI: 10.1098/rspa.1927.0085.
2. Tvardovskiy A.V. Obshchij fenomenologicheskij podkhod dlya opisaniya adsorbtsionnykh i absorbtsionnykh ravnovesij [General phenomenological approach for the description of adsorption and absorption equilibria], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and
nanomaterials], 2022, issue 14, pp. 321-330. DOI: 10.26456/pcascnn/2022.14.321. (In Russian).
3. Sanchez-Varretti F.O., Bulnes F.M., Ramirez-Pasto A.J. Adsorption of interacting binary mixtures on heterogeneous surfaces: theory, Monte Carlo simulations and experimental results, Adsorption, 2019, vol. 25, issue 7, pp. 1317-1328. DOI: 10.1007/s10450-019-00093-7.
4. Pérez-Chávez N.A., Albesa A.G., Longo G.S. Molecular theory of glyphosate adsorption to pH-responsive polymer layers, Adsorption, 2019, vol. 25, issue 7, pp. 1307-1316. DOI: 10.1007/s10450-019-00091-9.
5. Abbasi A., Abdelrasoul A., Sardroodi J.J. Adsorption of CO and NO molecules on Al, P and Si embedded MoS2 nanosheets investigated by DFT calculations, Adsorption, 2019, vol. 25. issue 5, pp. 1001-1017. DOI: 10.1007/s10450-019-00121-6.
6. Sladekova K., Campbell C., Grant C. et al. The effect of atomic point charges on adsorption isotherms of CO2 and water in metal organic frameworks, Adsorption, 2021, vol. 27, issue 6, pp. 995-1000. DOI: 10.1007/s10450-021-00301-3.
7. Sastre G.J., Kärger J., Ruthven D.M. Surface barriers and symmetry of adsorption and desorption processes, Adsorption, 2021, vol. 27, issue 5 (Topical Issue: Diffusion in Nanoporous Solids, vol. 2), pp. 777-785. DOI: 10.1007/s10450-020-00260-1.
8. Van Assche T.R.C., Baron G.V., Denaye J.F.M. An explicit multicomponent adsorption isotherm model: accounting for the size-effect for components with Langmuir adsorption behavior, Adsorption, 2018, vol. 24, issue 6, pp. 517-530. DOI: 10.1007/s10450-018-9962-1.
9. Dastani N., Arab A., Raiss H. Adsorption of Ampyra anticancer drug on the graphene and functionalized graphene as template materials with high efficient carrier, Adsorption, 2020, vol. 26, issue 6, pp. 879-893. DOI: 10.1007/s10450-019-00142-1.
10. Avijegon G., Xiao G., Li G., May E.F. Binary and ternary adsorption equilibria for CO2/CH4/N2 mixtures on Zeolite 13X beads from 273 to 33 K and pressures to 900 kPa, Adsorption, 2018, vol. 24, issue 4, pp. 381-392. DOI: 10.1007/s10450-018-9952-3.
11. Ghasemi A.S., Mashhadban F., Ravari F. A DFT study of penicillamine adsorption over pure and Al-doped C60 fullerene, Adsorption, 2018, vol. 24, issue 5, pp. 471-480. DOI: 10.1007/s10450-018-9960-3.
12. Berezovsky V., Öberg S. Computational study of the CO adsorption and diffusion in zeolites: validating the Reed–Ehrlich model, Adsorption, 2018, vol. 24, issue 4, pp. 403-413. DOI: 10.1007/s10450-018-9948-z.
13. Henry D.C. A kinetic theory of adsorption, The London, Edinburgh, and Dublin Philosophical Magazine and Journal of Science. Series 6, 1922, vol. 44, issue 262, pp. 689-705. DOI: 10.1080/14786441108634035.
14. Langmuir I. The adsorption of gases on plane surfaces of glass, mica and platinum, Journal of the American Chemical Society, 1918, vol. 40, issue 9, pp. 1361-1403. DOI: 10.1021/ja02242a004.
15. Brunauer S., Emmett P.H., Teller E. Adsorption of gases in multimolecular layers, Journal of the American Chemical Society, 1938, vol. 60, issue 2, pp. 309-319. DOI: 10.1021/ja01269a023.
16. Fowler R.H., Guggenheim E.A. Statistical thermodynamics, Cambridge: The University Press, 1939, X, 693 p.
17. Temkin M.I. Adsorbtsionnoe ravnovesie i kinetika protsessov na neodnorodnykh poverkhnostyakh pri vzaimodejstvii adsorbirovannykh molekul [Adsorption equilibrium and the kinetics of processes on nonhomogeneous surfaces and in the interaction between adsorbed molecules], Zhurnal Fizicheskoi Khimii [Journal of Physical Chemistry], 1941, vol. 15, no. 3, pp. 296-332. (In Russian).

⇐ Prevoius journal article | Content | Next journal article ⇒