Calculation of the spectrum of a gallium arsenide semiconductor with a triangular potential function by the power series method

I.N. Belyaeva1, N.I. Korsunov1, N.A. Chekanov1, A.N. Chekanov2

1 Belgorod National Research University
2 Belgorod Law Institute of MIA of the Russian Federation named after I.D. Putilin

DOI: 10.26456/pcascnn/2024.16.337

Short communication

Abstract: The paper investigates the quantum characteristics of the widely used semiconductor gallium arsenide in the modern promising field of microelectronics. For the energy levels in a triangular potential well, analytical expressions are obtained using the zeros of the Airy function. In addition, the corresponding Schrödinger equation with this potential function is solved by the power series method and both the energy spectrum of the lower levels and the corresponding wave functions are calculated. Satisfactory agreement between the values of the energy levels obtained in both approaches is found, but the prospects of calculating the quantum characteristics directly using the Schrödinger equation are noted. The solution of the Schrödinger equation is sought as a linear combination of two linearly independent solutions in the form of power series. The coefficients of this linear combination depend on the total energy as a parameter. Taking into account the boundaryconditions on the boundary of the integration segment leads to a linear algebraic system of equations. Nontrivial solutions of this system determine both the energy spectrum and the corresponding wave functions. Due to the sharp dependence of the energy levels on the type of wave functions, a careful choice of boundary points is necessary, as well as the number of terms in the series of wave functions. Optimal values of the specified fitting parameters allow us to obtain the values of the energy levels with the desired high accuracy.

Keywords: heterostructures, computer modeling, Schrödinger equation, gallium arsenide, energy spectrum, wave functions, power series method, Airy function

  • Irina N. Belyaeva – Ph. D., Docent, Department of Computer Science, Natural Sciences and Teaching Methods, Belgorod National Research University
  • Nikolay I. Korsunov – Dr. Sc., Professor, Department of Mathematical and Software Information Systems, Belgorod National Research University
  • Nikolay A. Chekanov – Dr. Sc., Professor, Department of Applied Mathematics and Computer Modeling, Belgorod National Research University
  • Aleksandr N. Chekanov – Senior Lecturer, Department of Security at Transport Facilities, Belgorod Law Institute of MIA of the Russian Federation named after I.D. Putilin

For citation:

Belyaeva I.N., Korsunov N.I., Chekanov N.A., Chekanov A.N. Raschet spektra poluprovodnika arsenida galliya s treugolnoj potentsialnoj funktsiej metodom stepennykh ryadov [Calculation of the spectrum of a gallium arsenide semiconductor with a triangular potential function by the power series method], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 337-342. DOI: 10.26456/pcascnn/2024.16.337.

Full article (in Russian): download PDF file

References:

1. Lesovik G. Electronic transport in meso- and nano-scale conductors. Zurich, ETH Zurich, 2008, 156 p. 2. Supriyo D. Quantum transport: atom to transistor, 2nd ed. Cambridge, Cambridge University Press, 2005, 420 p. DOI: 10.1017/CBO9781139164313.
3. Harrison P. Quantum wells, wires and dots: theoretical and computational physics of semiconductor nanostructures, 2nd ed. Chichester, John Willey & Sons, LTD, 2005, 502 p.
4. Demixovskij V.Ya, Vugalter G. A. Fizika nizkorazmernykh system [Physics of quantum low-dimensional structures]. Moscow, Logos Publ., 2000, 248 p. (In Russian).
5. Shik A.Ya, Bakueva L.G., Musixin S.F., Ryghkov S.A. Fizika nizkorazmernykh system [Physics of low-dimensional systems], ed. by A.Ya Shik. Saint Peterburg, Nauka Publ., 2001, 160 p. (In Russian).
6. Hludkov S.S., Tolbanov O.P., Vilisova M.D., Prudaev I.A. Poluprovodnikovye pribory na osnove arsenida galliya s glubokimi primesnymi tsentrami [Gallium arsenide-based semiconductor devices with deep impurity centers], ed, by O.P. Tolbanov. Tomsk, Tomsk State University Publ., 2016, 258 p. (In Russian).
7. Tavger B.A., Demikhovskii V.Ya. Quantum size effects in semiconducting and semimetallic films, Soviet Physics Uspekhi, 1969, vol. 11, issue 5, pp. 644-658. DOI: 10.3367/UFNr.0096.196809d.0061.
8. Demikhovskii V.Ya. Kvantovye yamy, niti, tochki. Chto eto takoe? [Quantum wells, threads, dots. What are they?], Sorosovskij obrazovatel'nyj zhurnal [Soros Educational Journal], 1997, no. 5, p. 80-86. (In Russian).
9. Landau L.D., Lifshits E.M. Kurs teoreticheskoj fiziki [Course of theoretical physics], 10 volumes. Vol. III. Kvantovaya mekhanika (nerelyativistskaya teoriya) [Quantum mechanics (non-relativistic theory)], 6th ed. Мoscow, FIZMATLIT Publ., 2004, 800 p. (In Russian).
10. Stepanov V.V. Kurs differentsial'nykh uravnenij [Course of differential equations]. Moscow, GITTL Publ., 1953, 468 p. (In Russian).
11. Belyaeva I. N., Ukolov Yu.A., Chekanov N.A. Postroenie obshchego resheniya differencial'nykh uravnenij fuksovskogo tipa v vide stepennykh ryadov [Construction of a general solution of differential equations of Fuchsian type in the form of power series]. Moscow, The All-Russian Scientific and Technical Information Center, 2005, no. 50200500089. (In Russian).
12. Airy G.B. On the intensity of light in the neighbourhood of a caustic, Transactions of the Cambridge Philosophical Society, 1838, vol. 6, pp. 379-402.
13. Yakovleva G.D. Tablitsy funktsij Ejri i ikh proizvodnykh [Tables of Airy functions and their derivatives]. Moscow, Nauka Publ., 1969, 377 p. (In Russian).
14. Chekanov N.A., Belyaeva I.N., Kirichenko I.K., Chekanova N.N. Simvol'no-chislennye metody resheniya differentsial'nykh uravnenij klassicheskoj i kvantovoj mekhaniki [Symbolic-numerical methods for solving differential equations of classical and quantum mechanics]. Kharkov: ISMA Publ., 2019, 420 p. (In Russian).
15. Stockman, H.-J. Quantum Chaos. An introduction. Cambridge: Cambridge University Press, 1999, XI, 368 p. DOI: 10.1017/CB09780511524622.

⇐ Prevoius journal article | Content | Next journal article ⇒