Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Correlation of magnetic characteristics and fractal dimension of magneto-optical images of permanent magnets

A.D. Zigert, N.B. Kuz`min, E.M. Semenova, A.Yu. Karpenkov, A.I. Ivanova, N.Yu. Sdobnyakov

Tver State University

DOI: 10.26456/pcascnn/2024.16.119

Original article

Abstract: The article continues a series of studies of permanent magnets with different magnetization reversal mechanisms (nucleation, domain boundary displacement). In this work, a correlation is established between magnetic characteristics of permanent magnets (Y25 and AlNiCo) and the fractal dimension of magneto-optical images of their stray fields. Bismuth-containing ferrite-garnet films were used as an indicator. It is shown that the limiting values of the fractal dimension: 1,76 for a ferrite magnet and 1,85 for an AlNiCo magnet, are consistent with the results obtained for NdFeB (grade N35) and SmCo (grade KC37) magnets, as is the behavior of the field dependence of the fractal dimension. The behavior of the field dependence of magnetization Mmo(Hrev) has similar features to a similar dependence recorded for a permanent magnet NdFeB (grade N35), but the values of the demagnetizing fields for the Y25 sample are much smaller. The paper discusses the relationship between the mechanisms of magnetization reversal of permanent magnets and the behavior of the Mmo(Hrev) dependence.

Keywords: permanent magnets, fractal dimension, magneto-optics, dM(Hrev)/dHrev dependence

  • Alexandr D. Zigert – Senior Lecturer, Applied Physics Department, Tver State University
  • Nickolay B. Kuz`min – 2nd year graduate student, Physical Chemistry Department, Tver State University
  • Elena M. Semenova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University
  • Alexey Yu. Karpenkov – Ph. D., Docent, Head of Condensed Matter Physics Department, Tver State University
  • Alexandra I. Ivanova – Ph. D., Docent, Applied Physic Department, Tver State University
  • Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, General Physics Department, Tver State University

For citation:

Zigert A.D., Kuz`min N.B., Semenova E.M., Karpenkov A.Yu., Ivanova A.I., Sdobnyakov N.Yu. Korrelyatsiya magnitnykh kharakteristik i fraktalnoj razmernosti magnitoopticheskikh izobrazhenij postoyannykh magnitov [Correlation of magnetic characteristics and fractal dimension of magneto-optical images of permanent magnets], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 119-127. DOI: 10.26456/pcascnn/2024.16.119.

Full article (in Russian): download PDF file

References:

1. Sdobnyakov N.Yu., Antonov A.S., Ivanov D.V. Morfologicheskie kharakteristiki i fraktal'nyj analiz metallicheskikh plenok na dielektricheskikh poverkhnostyakh: monografiya [Morphological characteristics and fractal analysis of metal films on dielectric substrates: monography]. Tver: Tver State Unibersity Publ., 2019, 168 p. (In Russian).
2. Zhou W., Cao Y., Zhao H. et al. Fractal analysis on surface topography of thin films: a review, Fractal and fractional, 2022, vol. 6, issue 3, art. no. 135, 30 p. DOI: 10.3390/ fractalfract6030135.
3. Ivanov G.S., Brylkin Yu.V. Fraktal'naya geometricheskaya model' mikropoverkhnosti [Fractal geometric microsurface model], Geometriya i grafika [Geometry & Graphics], 2016, vol. 4, no. 1, pp. 4-11. DOI: 10.12737/18053. (In Russian).
4. Brylkin Yu.V., Kusov A.L., Florov A.V. Testirovanie algoritma modelirovaniya rel'efa sherokhovatoj poverkhnosti na osnove teorii fraktalov [Testing a rough surface relief modeling algorithm based on fractal theory, Izvestiya Kabardino-Balkarskogo gosudarstvennogo universiteta], [Proceedings of the Kabardino-Balkarian State University], 2014, vol. IV, no. 5, pp. 86-89. (In Russian).
5. Ivanova A.I., Semenova E.M., Dunaeva G.G., Ovcharenko S.V., Tretyakov S.A., Zigert A.D. Vliyanie defektov na magnitnye kharakteristiki ferrit-granatovykh plenok [Influence of defects on magnetic characteristics of ferrite-garnet films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 103-112. DOI: 10.26456/pcascnn/2020.12.103. (In Russian).
6. Zigert A.D., Dunaeva G.G., Sdobnyakov N.Yu. Fraktal'nyj analiz labirintnoj domennoj struktury ferrit-granatovykh plenok v protsesse peremagnichivaniya [Fractal analysis of the maze-like domain structure of ferrite-garnet films in the process of magnetization], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 11, pp. 134-145. DOI: 10.26456/pcascnn/2021.13.134. (In Russian).
7. Dovbnya L.A., Naumov D.E., Khramov B.V. Fractal model of magnetization reversal in a strained garnet ferrite film, Journal of Experimental and Theoretical Physics Letters, 2001, vol. 73, issue 7, pp. 366-369. DOI: 10.1134/1.1378121.
8. Zigert A.D., Dunaeva G.G., Semenova E.M. et al. Fractal dimension behaviour of maze domain pattern in ferrite-garnet films during magnetisation reversal, Journal of Superconductivity and Novel Magnetism, 2022, vol. 35, issue 8, pp. 2187-2193. DOI: 10.1007/s10948-022-06301-w.
9. Zigert A.D., Dunaeva G.G., Kuz`min N.B., Semenova E.M., Sdobnyakov N.Yu. The fractal dimension behaviour of the domain patterns in ferrite-garnet films, Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 98-107. DOI: 10.26456/pcascnn/2023.15.098. (In Russian).
10. Zigert A.D., Semenova E.M., Kuz`min N.B., Sdobnyakov N.Yu. Fractal analysis of magneto-optical images of a magnet surface after exposure to a pulsed field, Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 101-107. DOI: 10.26456/pcascnn/2022.14.101. (In Russian).
11. Zigert A.D., Kuz‘min N.B., Semenova E.M. et al. Patterns of the fractal dimension evolution of magneto-optical imagesof magnets after exposure to a pulsed field, Physics of the Solid State, 2023, vol. 65, issue 12, pp. 2037-2039. DOI: 10.61011/PSS.2023.12.57657.5091k.
12. Zigert A.D., Kuz’min N.B., Sdobnyakov N.Yu. et al. Fractal analysis of magneto-optical visualization of the remagnetization of a permanent magnet in a pulsed field // Bulletin of the Russian Academy of Sciences: Physics. – 2023. – V. 87. – I. 10. – P. 1421-1424. DOI: 10.3103/S1062873823703422.
13. Kim D.-H., Cho Y.-C., Choe S.-B., Shin S.-C. Correlation between fractal dimension and reversal behavior of magnetic domain in Co/Pd nanomultilayers, Applied Physics Letters, 2003, vol. 82, no. 21, pp. 3698-3700. DOI: 10.1063/1.1578185.
14. Komogortsev S.V., Iskhakov R.S., Fel’k V.A. Fractal dimension effect on the magnetization curves of exchange-coupled clusters of magnetic nanoparticles, Journal of Experimental and Theoretical Physics, 2019, vol. 128, issue 5, pp. 754-760. DOI: 10.1134/S1063776119040095.
15. Polyakova O.P., Akimova M.L., Polyakova P.A. Remagnetization of a fractal magnetic structure, Bulletin of the Russian Academy of Sciences: Physics, 2020, vol. 84, issue 2, pp. 166-168. DOI: 10.3103/S106287382002029X.
16. Han B.-S., Li D., Zheng D.-J., Zhou Y. Fractal study of magnetic domain patterns, Physical Review B, 2002, vol. 66, issue 1, pp. 014433-1-014433-5. DOI: 10.1103/PhysRevB.66.014433.
17. Persson B.N.J. On the fractal dimension of rough surfaces, Tribology Letters, 2014, vol. 54, issue 1, pp. 99-106. DOI: 10.1007/s11249-014-0313-4.
18. Bathany C., Romancer M.L., Armstrong J.N., Chopra H.D. Morphogenesis of maze-like magnetic domains, Physical Review B, 2010, vol. 82, issue 18, pp. 184411-1-184411-14. DOI: 10.1103/PhysRevB.82.184411. DOI: 10.1103/PhysRevB.82.184411.
19. Fei W.D., Chu W.G., Yang D.Z. Fractal characteristic of the microstructure in Alnico8, Journal of Materials Science Letters, 2000, vol. 19, issue 14, pp. 1221-1223. DOI: 10.1023/A:1006700908456.
20. Zhukov A.S., Barakhtin B.K., Bobyr V.V., Titova A.D. Structural studies of additive hard magnetic alloy Alnico24, IOP Conference Series: Materials Science and Engineering, 2020, vol. 919, art. № 022021, 6 p. DOI: 10.1088/1757-899X/919/2/022021.
21. Otsu N. A threshold selection method from gray-level histograms, IEEE Transactions on Systems, Man, and Cybernetics, 1979, vol. 9, issue 1, pp. 62-66. DOI: 10.1109/TSMC.1979.4310076.
22. Sdobnyakov N.Yu., V.A. Anofriev, A.D. Zigert, N.B. Kuz`min Fractal domains Pro: programma analiza 2D mikrofotografij poverkhnosti i opredeleniya ee fraktal'noj razmernosti [Fractal domains Pro: program for analyzing 2D microphotographs of a surface and determining its fractal dimension]. Certificate RF, no. 2023660111, 2023. (In Russian).

⇐ Prevoius journal article | Content | Next journal article ⇒