Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Switching processes in alanine doped triglycine sulfate crystals

N.N. Bolshakova1, A.I. Ivanova1, N.Yu. Druginina2, E.M. Semenova1, S.S. Schipilov1

1 Tver State University
2 Military Academy of Air and Space Defense named after Marshal of the Soviet Union G. K. Zhukov

DOI: 10.26456/pcascnn/2024.16.072

Original article

Abstract: The paper presents the results of an experimental study of the dielectric and switching characteristics of some initial and annealed alanine-doped crystals of the triglycine sulfate group at room temperature. The results of measurements and calculations of the effective permittivity, switchable polarization, coercive and bias fields, unipolarity coefficient and dielectric loss tangent are presented. It was found that for most samples before and after annealing, the dielectric hysteresis loops are unipolar and shifted along the abscissa axis. This indicates a preferential orientation of domains and the presence of bias fields. As a result of annealing, the values of the coercive field and the unipolarity coefficient of the crystals decrease, and the switchable polarization increases. It is shown that the field dependences of the effective permittivity of the crystals before annealing have extrema lying in the field range of (5-7,5) ∙ 104 V∙m-1 and in the range (5-12) ∙ 104 V∙m-1 after their annealing.

Keywords: triglycine sulfate crystals, hysteresis, switching processes, permittivity

  • Nataly N. Bolshakova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University
  • Alexandra I. Ivanova – Ph. D., Docent, Applied Physics Department, Tver State University
  • Nataly Yu. Druginina – Ph. D., Docent, Military Academy of Air and Space Defense named after Marshal of the Soviet Union G. K. Zhukov
  • Elena M. Semenova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University
  • Sergey S. Schipilov – Master's graduate, Condensed Matter Physics Department, Faculty of Physics and Technology, Tver State University

For citation:

Bolshakova N.N., Ivanova A.I., Druginina N.Yu., Semenova E.M., Schipilov S.S. Protsessy pereklyucheniya alaninsoderzhashchikh kristallov triglitsinsulfata [Switching processes in alanine doped triglycine sulfate crystals], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 72-84. DOI: 10.26456/pcascnn/2024.16.072. ⎘

Full article (in Russian): download PDF file

References:

1. He H., Lu X., Hanc E. et al. Advances in lead-free pyroelectric materials: a comprehensive review, Journal of Materials Chemistry C, 2020, vol. 8 issue 5, pp. 1494-1516. DOI: 10.1039/C9TC05222D.
2. Zhang D., Wu H., Bowen C.R., Yang Y. Recent advances in pyroelectric materials and applications, Small, 2021, vol. 17, issue 51, art. no. 2103960, 23 p. DOI: 10.1002/smll.202103960.
3. Ranu, Bharathi U., Sinha R., Agarwal P.B. CMOS compatible pyroelectric materials for infrared detectors, Materials Science in Semiconductor Processing, 2022, vol. 140, art. no. 106375, 19 p. DOI: 10.1016/j.mssp.2021.106375.
4. Kang M., Yeatman E.M. Coupling of piezo-and pyro-electric effects in miniature thermal energy harvesters, Applied Energy, 2020, vol. 262, art. no. 114496, 10 p. DOI: 10.1016/j.apenergy.2020.114496.
5. Whatmore R. Characterisation of pyroelectric materials, Characterisation of ferroelectric bulk materials and thin films, Springer Series in Measurement Science and Technology, ed. by M. Cain. Dordrecht, Springer, 2014, vol. 2, pp. 65-86. DOI: 10.1007/978-1-4020-9311-1_4.
6. Mai B.D. Analyzing frequency spectra of dielectric loss to clarify influence of L, α-alanine doping on phase transition in triglycine sulfate: phase transition in LATGS, Materials Science, 2022. vol. 28, issue 2, pp. 151-156. DOI: 10.5755/j02.ms.29313.
7. Rafi A.S., Suppuraj P., Balakrishnan C., Kalpana S. Physicochemical analytical studies on yttrium‐doped triglycine sulfate single crystals, Crystal Research and Technology, 2023, vol. 58, issue 4, art. no. 2200225. DOI: 10.1002/crat.202200225.
8. Terasawa Y., Kikuta T., Ichiki M. et al. Preferences of polarity and chirality in triglycine sulfate crystals by alanine ghost, Journal of Physics and Chemistry of Solids, 2021, vol. 151, art. no. 109890, 7 p. DOI: 10.1016/j.jpcs.2020.109890.
9. Bolshakova N.N., Druginina N.Yu., Ivanova A.I. et al. Perepolyarizatsionnye svoistva med'soderzhashchikh kristallov triglitsinsul'fata [Repolarization properties of copper-containing crystals of triglycine sulfate], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 50-60. DOI: 10.26456/pcascnn/2022.14.050. (In Russian).
10. Vakulenko A.F., Vakhrushev S.B., Filimonov A.V., Zhang N. Ustanovka dlya izmereniya petel' segnetoehlektricheskogo gisterezisa na osnove modifitsirovannogo metoda Soiera-Tauehra [An automatic system for measuring the ferroelectric hysteresis loops using the modified Sawyer – Tower circuit], Nauchno-tekhnicheskie vedomosti Sankt-Peterburgskogo gosudarstvennogo politekhnicheskogo universiteta. Fiziko-matematicheskie nauki [St. Petersburg Polytechnical State University Journal. Physics and Mathematics], 2019, vol. 12, issue 4, p. 89-96. DOI: 10.18721/JPM.12409. (In Russian).
11. Ivanova A.I., Grechishkin R.M., Bolshakova N.N., Belyakov V.A. Temperature observation of the evolution of the domain structure of triglycine sulphate by SEM, Journal of Surface Investigation. X-ray, Synchrotron and Neutron Techniques, 2015, vol. 9, issue 5, p. 908-912. DOI: 10.1134/S1027451015050079.
12. Choudhury R.R., Chitra R., Ramanadham M. Investigation of diffraction line broadening due to compositional fluctuations in L-alanine-doped triglycine sulfate, Acta Crystallographica Section B: Structural Science, 2003, vol. 59, issue 5, pp. 647-652. DOI: 10.1107/S0108768103015441.
13. Yamazaki T., Mohamed G.A., Shichi M., Nakatani N. Growth and domain structure of latgsp single crystals, Ferroelectrics, 1998, vol. 219, issue 1, pp. 191-198. DOI: 10.1080/00150199808213516.
14. Pandian M.S., Verma S., Karuppasamy P., Ramasamy P., Tiwari V.S., Karnal A.K. Unidirectional crystal growth of L-alanine doped triglycine sulphate crystals along [010] polar direction in ferroelectric and paraelectric temperature ranges, and their comparative characterizations, Materials Research Bulletin, 2021, vol. 134, art. no. 111118, 9 p. DOI: 10.1016/j.materresbull.2020.111118.
15. Aravazhi S., Jayavel R., Subramanian C. Growth and characterization of L-alanine and L-valine doped triglycine sulphate crystals, Materials Research Bulletin, 1997, vol. 32, issue 11, pp. 1503-1513. DOI: 10.1016/S0025-5408(97)00131-1.

⇐ Prevoius journal article | Content | Next journal article ⇒