Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Investigation of optical properties of metal-doped CsPbX3 perovskite nanocrystals

V.P. Bezverkhniy, A.Y. Gagarina, E.N. Muratova, A.I. Maximov, V.A. Moshnikov

Saint Petersburg Electrotechnical University «LETI»

DOI: 10.26456/pcascnn/2024.16.041

Original article

Abstract: As a part of the research work, inorganic lead-containing halide perovskite nanocrystals with the CsPbX3 structure were obtained by the hot injection. The alloying of single crystals of perovskites was carried out by solution methods, zinc and indium ions acted as dopants. The photoluminescence spectra and optical density spectra of the obtained colloidal solutions were studied. Our studies have shown that doping of perovskite nanocrystals with metal ions leads to an increase in photoluminescence as well as to a shift in the maximum of photoluminescence relative to the reference composition by 4 and 12 nm for bromides and iodides, respectively. Also, it has been shown that the magnitude of the shift does not depend on the type of dopant. It is noted that within the framework of this work, doping does not lead to a change in the position of the edge of its own absorption.

Keywords: perovskites, solar energy, nanocrystals, alloying, optical properties

  • Vladislav P. Bezverkhniy – 4th year postgraduate student, Micro- and Nanoelectronics Department, Saint Petersburg Electrotechnical University «LETI»
  • Alena Y. Gagarina – 3rd year postgraduate student, Micro- and Nanoelectronics Department, Saint Petersburg Electrotechnical University «LETI»
  • Ekaterina N. Muratova – Ph. D., Docent, Micro- and Nanoelectronics Department, Saint Petersburg Electrotechnical University «LETI»
  • Alexander I. Maximov – Ph. D., Docent, Micro- and Nanoelectronics Department, Saint Petersburg Electrotechnical University «LETI»
  • Vyacheslav A. Moshnikov – Dr. Sc., Professor, Micro- and Nanoelectronics Department, Saint Petersburg Electrotechnical University «LETI»

For citation:

Bezverkhniy V.P., Gagarina A.Y., Muratova E.N., Maximov A.I., Moshnikov V.A. Issledovanie opticheskikh svojstv legirovannykh metallami perovskitnykh nanokristallov CsPbX3 [Investigation of optical properties of metal-doped CsPbX3 perovskite nanocrystals], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 41-47. DOI: 10.26456/pcascnn/2024.16.041. ⎘

Full article (in Russian): download PDF file

References:

1. Lin K., Xing J., Quan L. N. et. al. Perovskite light-emitting diodes with external quantum efficiency exceeding 20 per cent. Nature, 2018, vol. 562, issue 7726, pp. 245-248. DOI: 10.1038/s41586-018-0575-3.
2. Dement`ev P.A., Dunaevskij M.S., Matyushkin L.B. et al. Study of CsPbBr3 nanocrystals and their agglomerates by combined scanning probe microscopy and optical spectrometry, Optics and Spectroscopy, 2018, vol. 125, issue 6, pp. 858-863. DOI: 10.1134/S0030400X18120044.
3. Song J., Li J., Xu L. et. al. Room‐temperature triple‐ligand surface engineering synergistically boosts ink stability, recombination dynamics, and charge injection toward EQE‐11.6% perovskite QLEDs, Advanced Materials, 2018, vol. 30, issue 30, art. no. 1800764, 7 p. DOI: 10.1002/adma.201800764.
4. Xue J., Zhu Z., Xu X. et. al. Narrowband perovskite photodetector-based image array for potential application in artificial vision. Nano Letters, 2018, vol. 18, issue 12, pp. 7628-7634. DOI: 10.1021/acs.nanolett.8b03209.
5. Aleshin A.N., Shcherbakov I.P., Kirilenko D.A. et al. Light-emitting field-effect transistors based on composite films of polyfluorene and CsPbBr3 nanocrystals, Physics of the Solid State, 2019, vol. 61, issue 2, pp. 256-262. DOI: 10.1134/S1063783419020021.
6. Gao Y., Huang C., Hao C. et. al. Lead halide perovskite nanostructures for dynamic color display, ACS Nano, 2018, vol. 12, issue 9, pp. 8847-8854. DOI: 10.1021/acsnano.8b02425.
7. Boudjemila L., Aleshin A.N., Malyshkin V.M. et. al. Electrical and optical characteristics of CsPbI3 and CsPbBr3 lead halide perovskite nanocrystal films deposited on c-Si solar cells for photovoltaic applications, Physics of the Solid State, 2022, vol. 64, issue 11, pp. 1670-1674. DOI: 10.21883/PSS.2022.11.54189.418.
8. Percova A., Matyushkin L.B. Synthesis and postsynthetic anion exchange of CsPbX3 (X= Cl, Br, I) quantum dots, Journal of Physics: Conference Series, 2017, vol. 917, issue 6, art. no. 062041, 4 p. DOI: 10.1088/1742-6596/917/6/062041.
9. Chen H., Li M., Wang B., Ming S., Su J. Structure, electronic and optical properties of CsPbX3 halide perovskite: a first-principles study, Journal of Alloys and Compounds, 2021, vol. 862, art. no. 158442, 6 p. DOI: 10.1016/j.jallcom.2020.158442.
10. Stoumpos C.C., Malliakas C.D., Peters J.A., et al. Crystal growth of the perovskite semiconductor CsPbBr3: a new material for high-energy radiation detection, Crystal Growth & Design, 2013, vol. 13, issue 7, pp. 2722-2727. DOI: 10.1021/cg400645t.
11. Posudievsky O.Yu., Konoshchuk N., Karbivskyy V.L. et al. Structural and spectral characteristics of mechanochemically prepared CsPbBr3, Theoretical and Experimental Chemistry, 2017, vol. 53, issue 4, pp. 235-243. DOI: 10.1007/s11237-017-9520-z.
12. Jung S., Kim J.H., Choi J.W. et al. Enhancement of photoluminescence quantum yield and stability in CsPbBr3 perovskite quantum dots by trivalent doping, Nanomaterials, 2020, vol. 10, issue 4, art. no. 710, 10 p. DOI: 10.3390/nano10040710.
13. Nenashev G.V., Aleshin A.N., Ryabko A.A. et al. Effect of barium doping on the behavior of conductivity and impedance of organic-inorganic perovskite films. Solid State Communications, 2024, vol. 388, art. no. 115554, 8 p. DOI: 10.1016/j.ssc.2024.115554.
14. Zhou Y., Chen J., Bakr O. M., Sun H.-T. Metal-doped lead halide perovskites: synthesis, properties, and optoelectronic applications, Chemistry of Materials, 2018, vol. 30, issue 19, pp. 6589-6613 DOI: 10.1021/acs.chemmater.8b02989.
15. Zhang M., Han X., Yang C. et. al. Size uniformity of CsPbBr3 perovskite quantum dots via manganese-doping, Nanomaterials, 2024, vol. 14, issue 15, art. no. 1284, 11 p. DOI: 10.3390/nano14151284.
16. Chmereva T.M., Kucherenko M.G., Mushin F.Yu. Effect of the spherical nanoparticle with a metal shell on deactivation of the excited quantum dot, Russian Physics Journal, 2023, vol. 65, issue 7, pp. 1081-1093. DOI: 10.1007/s11182-022-02735-w.
17. Wang F., Zhang H., Song X. et. al. High-responsivity VIS–NIR photodetector based on a Ag2S/CsPbBr3 heterojunction, ACS Applied Electronic Materials, 2022, vol. 4, issue 8, pp. 3922-3929. DOI: 10.1021/acsaelm.2c00587.
18. Matyushkin L.B., Moshnikov V.A. Photoluminescence of perovskite CsPbX3 (X = Cl, Br, I) nanocrystals and solid solutions on their basis, Semiconductor, 2017, vol. 51, issue 10, pp. 1337-1342. DOI: 10.1134/S106378261710013X.

⇐ Prevoius journal article | Content | Next journal article ⇒