Effect of dislocation density on the dynamic yield strength of alloys with nanoscale defects under high energy external actions

V.V. Malashenko1,2, T.I. Malashenko3,4

1 Donetsk Institute for Physics and Engineering named after A.A. Galkin
2 Donetsk National University
3 Donetsk National Technical University
4 Donetsk National University of Economics and Trade named after Mikhail Tugan-Baranovskiy

DOI: 10.26456/pcascnn/2022.14.176

Short communication

Abstract: A theoretical analysis of inelastic processes in aged alloys under intense external influences is carried out. The analysis was carried out within the framework of the theory of dynamic interaction of defects. An analytical expression for the dependence of the dynamic yield strength on the dislocation density has been obtained. The reason for the different influence of nanostructural defects on the dislocation motion under high strain rate deformation and quasi-static deformation is determined. It is shown that under high strain rate deformation, nanosized defects affect the nature of the dependence of the dynamic yield strength on the dislocation density. This dependence becomes nonmonotonic and has a minimum. At the minimum point, there is a transition from the dominance of the drag of the dislocation by Guinier-Preston zones to the dominance of its drag by other dislocations. Numerical estimates of the contribution of the Guinier-Preston zones to the yield strength are made. It is shown that at a high concentration of Guinier-Preston zones, this contribution is very significant. Numerical estimates are made of the dislocation density at which the Taylor relation is violated.

Keywords: high-speed deformation, dislocations, Guinier-Preston zones, point defects, nanomaterials, Taylor ratio

  • Vadim V. Malashenko – Dr. Sc., Professor, Chief Researcher, Department «Theory of kinetic and electronic properties of nonlinear systems», Donetsk Institute for Physics and Engineering named after A.A. Galkin, Professor, Department of Radiophysics and Infocommunication Technologies Donetsk National University
  • Tatyana I. Malashenko – Senior Lecturer, Department of Physics, Donetsk National Technical University, Senior Lecturer, Department of Natural Sciences and Life Safety Donetsk National University of Economics and Trade named after Mikhail Tugan-Baranovskiy

For citation:

Malashenko V.V., Malashenko T.I. Vliyanie plotnosti dislokatsij na dinamicheskij predel tekuchesti splavov s nanorazmernymi defektami pri vysokoenergeticheskikh vneshnikh vozdejstviyakh [Effect of dislocation density on the dynamic yield strength of alloys with nanoscale defects under high energy external actions], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 176-182. DOI: 10.26456/pcascnn/2022.14.176.

Full article (in Russian): download PDF file

References:

1. Singla A., Ray A., Hugoniot elastic limit of single-crystal tantalum at normal and elevated temperatures subjected to extreme strain rates, Physical Review B, 2022, vol. 105, issue 6, art. no. 064102, 19 p. DOI: 10.1103/PhysRevB.105.064102.
2. Kanel G.I., Savinykh A.S., Garkushin G.V., Razorenov S.V. Effects of temperature and strain on the resistance to high-rate deformation of copper in shock waves, Journal of Applied Physics, 2020, vol. 128, issue 11, pp. 115901-1-115901-8 . DOI: 10.1063/5.0021212.
3. Batani D. Matter in extreme conditions produced by lasers, Europhysics Letters, 2016, vol. 114, no. 6, pp. 65001-p1-650001-p7. DOI: 10.1209/0295-5075/114/65001.
4. Lee J.H., Veysset D., Singer J.P. et al. High strain rate deformation of layered nanocomposites, Nature Communications, 2012, vol. 3, art. no. 1164, 9 p. DOI: 10.1038/ncomms2166.
5. Smith R.F., Eggert J.H., Rudd R.E. et al. High strain-rate plastic flow in Al and Fe, Journal of Applied Physics, 2011, vol. 110, issue 12, pp. 123515-1-123515-11. DOI: 10.1063/1.3670001.
6. Yanilkin A.V., Krasnikov V.S., Kuksin A.Yu., Mayer A.E. Dynamics and kinetics of dislocations in Al and Al-Cu alloy under dynamic loading, International Journal of Plasticity, 2014, vol. 55, pp. 94-107. DOI: 10.1016/j.ijplas.2013.09.008.
7. Malashenko V.V., Malashenko T.I. Vliyanie nanorazmernykh defektov na dinamicheskij predel tekuchesti splavov [The effect of nanoscale defects on the dynamic yield stress of alloys], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 136-141. DOI: 10.26456/pcascnn/2020.12.136. (In Russian).
8. Malashenko V.V. The influence of collective effects on the concentration dependence of the yield stress of alloys under high-energy impacts, Technical Physics Letters, 2020, vol. 46, issue 9, pp. 925-927. DOI: 10.1134/S1063785020090242.
9. Malashenko V.V. Vliyanie vodoroda na mekhanicheskie svoystva metallov v usloviyakh vysokoskorostnoy deformatsii [The effect of hydrogen on the mechanical properties of metals under high strain rate deformation], [Physics of the Solid State], 2022, vol. 64, issue 11, pp. 1804-1806. DOI: 10.21883/FTT.2022.11.53337.416. (In Russian).
10. Malashenko V.V. Dynamic drag of dislocation by point defects in near-surface crystal layer, Modern Physics Letters B, 2009, vol. 23, issue 16, pp. 2041-2047. DOI: 10.1142/S0217984909020199.
11. Malashenko V.V. Dynamic drag of edge dislocation by circular prismatic loops and point defects, Physica B: Condensed Matter, 2009, vol. 404, issue 21, pp. 3890-38932. DOI: 10.1016/j.physb.2009.07.122.
12. Fan H., Wang Q., El-Awady J.A., Raabe D., Zaiser M. Strain rate dependency of dislocation plasticity, Nature Communication, 2021, vol. 12, art. no. 1845, 11 p. DOI: 10.1038/s41467-021-21939-1.

⇐ Prevoius journal article | Content | Next journal article ⇒