Abstract: Catalytic properties of the nanocluster iron-molybdenum polyoxometalate {Mo72Fe30} in solutions during the oxidation of iodide ions by persulfate have been studied. Automated installation based on spectrophotometric method of analysis controlled by computer was used. Comparison of literary data and kinetic datа on the oxidation of iodide with persulfate showed that keplerate {Mo72Fe30} is a heterogeneous catalyst. These data allowed to assume a non-radical mechanism for persulfate decomposition on the surface of cluster molecules at the first stage of the potassium iodide oxidation reaction. The value of the effective activation energy of the process indicates the catalytic effect of {Mo72Fe30} at the intermediate stage of the decomposition of the hydrogen peroxide.
Keywords: nanocluster iron-molybdenum polyoxometalate, keplerate, catalytic properties, oxidation of iodide ions, potassium persulfate, hydrogen peroxide.
- Sergei Yu. Menshikov – Ph.D., Docent of Chemistry Department, Ural State Mining University
- Ksenia A. Belozerova – student of Chemistry Department of Institute of Natural Sciences and Mathematics, Ural Federal University named after the first President of Russia B.N. Yeltsin
- Alexander A. Ostroushko – Dr. Sc., Professor, Professor of Physical and Inorganic Chemistry Department of Institute of Natural Sciences and Mathematics of Ural Federal University named after the first President of Russia B.N. Yeltsin, Chief Researcher and Head of Department of Chemical Materials Science, Scientific Research Institute of Physics and Applied Mathematics of Institute of Natural Sciences and Mathematics of Ural Federal University named after the first President of Russia B.N. Yeltsin
For citation:
Menshikov S.Yu., Belozerova K.A., Ostroushko A.A. Vozdejstvie nanoklasternogo polioksometallata {Mo72Fe30} na okislenie persulfatom jodid-ionov [Influence of the nanocluster {Mo72Fe30} polyoxometalate on oxidation of iodide–ions by persulfate], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 853-859. DOI: 10.26456/pcascnn/2020.12.853. ⎘
Full article (in Russian): download PDF file
⇐ Prevoius journal article | Content | Next journal article ⇒