Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Effect of the synthesis temperature on the structure of sodium-lithium niobate ceramics

O.V. Malyshkina, A.I. Ivanova, K.V. Patsuev

Tver State University

DOI: 10.26456/pcascnn/2020.12.644

Original article

Abstract: The authors synthesized samples and studied the structure of piezoelectric ceramics based on sodium and lithium niobates (Li0,1Na0,9)NbO3 with various technologies for the synthesis of sodium niobate material. A comparative study of the structure and dielectric properties of the obtained samples was carried out.. A significant dependence of grain formation during sintering of the samples on the synthesis temperature of the NaNbO3 composition is shown. It was found that the temperature of the phase transition strongly depends on the temperature of the first synthesis of the sodium niobate (Tmax ~ 375 °С if the first synthesis temperature was 650 °С; Tmax = 425 °С if the first synthesis temperature is 700 °С).

Keywords: piezoelectric ceramics, lead-free materials, grain structure

  • Olga V. Malyshkina – Dr. Sc., Full Professor, Head of the Department of Dissertation Councils and Doctorate Studies, Scientific Research Department, Tver State University
  • Alexandra I. Ivanova – Ph. D., Docent of the Applied Physic Department, Tver State University
  • Kirill V. Patsuev – postgraduate student, Tver State University

For citation:

Malyshkina O.V., Ivanova A.I., Patsuev K.V. Vliyanie temperatury sinteza na strukturu keramiki niobata natriya – litiya [Effect of the synthesis temperature on the structure of sodium-lithium niobate ceramics], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 644-651. DOI: 10.26456/pcascnn/2020.12.644.

Full article (in Russian): download PDF file

⇐ Prevoius journal article | Content | Next journal article ⇒