Lubrication properties of magnetic nanoliquids based on carboxylic acids

A.N. Bolotov, O.O. Novikova

Tver State Technical University, Tver, Russia

DOI: 10.26456/pcascnn/2019.11.555

Abstract: We adduce technological characteristics of synthesis and properties of low-viscous magnetic lubricant nanoliquids with dispersion phase based on diester carboxylic acids. Some physical-chemical and tribological differential characteristic of the diester magnetic lubricant oils are presented. We researched the lubrication properties of the magnetic nanoliquids in various friction conditions and determine their peculiar characteristics. It was analized the influence of the series of antiwear additions on the friction.

Keywords: magnetic lubricant nanoliquid, friction, wear, lubricant, antifriction and antiwear additions.

Bibliography link:

Bolotov, A.N. Lubrication properties of magnetic nanoliquids based on carboxylic acids / A.N. Bolotov, O.O. Novikova // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2019. – I. 11. – P. 555-563.

Full text (in Russian): download PDF file

Comments are closed.