Modeling process of distribution of light flow in the environment with diffusing centers

S.S. Rybina, S.A. Tretyakov

Tver State University, Tver, Russia

DOI: 10.26456/pcascnn/2019.11.356

Abstract: A mathematical model is developed for calculating parameters of light fluxes propagating through a light-scattering and absorbing medium. Single crystals of paratellurite and germanium with known optical parameters and densities of various absorbing and scattering inhomogeneities were chosen as mediums.

Keywords: scattering, reflection, refraction, Bouguer-Lambert law, scattering indicatrix.

Bibliography link:

Rybina, S.S. Modeling process of distribution of light flow in the environment with diffusing centers /S.S. Rybina, S.A. Tretyakov // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2019. – I. 11. – P. 356-363.

Full text (in Russian): download PDF file