Study of the charge generation in the synthesis of nanosized complex oxides in the combustion reactions of organo-inorganic precursors

A.A. Ostroushko, O.V. Russkikh, I.D. Gagarin, E.A. Filonova

Scientific Research Institute of Physics and Applied Mathematics, Ural Federal University named after the first President of Russia B.N. Yeltsin, Yekaterinburg, Russia

DOI: 10.26456/pcascnn/2019.11.215

Abstract: The presence of the generation of electric charges in precursors during the synthesis of nanosized complex oxides in the combustion reactions of compositions including metal nitrates, as well as glycine and glycerin as organic components, is shown. To measure the resulting potential difference, an automated system based on the IPEP-1 electrostatic field parameter meter and a signal amplification system were used.

Keywords: Nanosized complex-oxide materials, combustion synthesis, organic-inorganic compositions, charge generation, measurements.

Bibliography link:

Ostroushko, A.A. Study of the charge generation in the synthesis of nanosized complex oxides in the combustion reactions of organo-inorganic precursors / N.V. Alemasova, M.V. Savoskin, A.N. Vdovichenko et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2019. – I. 11. – P. 215-222.