Electron-stimulated desorption of lithium atoms from oxygen monolayer covered tungsten

Yu.A. Kuznetsov, M.N. Lapushkin

Ioffe Institute, Saint Petersburg, Russia

DOI: 10.26456/pcascnn/2019.11.184

Abstract: The electron-stimulated desorption of neutral lithium atoms from the oxygen monolayer covered the tungsten surface have been studied. The model of the atom electron-stimulated desorption processes on the tungsten surface with the adsorbed oxygen monolayer have been suggested. Both common and different features of the electron-stimulated desorption processes have been foundfor high-energy and low-energy peaks in the kinetic energy distributions of the desorbed atoms.

Keywords: electron-stimulated desorption, adsorption, alkali metals.

Bibliography link:

Kuznetsov, Yu.A. Electron-stimulated desorption of lithium atoms from oxygen monolayer covered tungsten / Yu.A. Kuznetsov, M.N. Lapushkin // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2019. – I. 11. – P. 184-191.

Full text (in Russian): download PDF file

Comments are closed.