Influence of Ti – H hydrides on interatomic interactions and on characteristics of Ti alloying membrane alloys based on V – Ni

R.M. Belyakova1, V.A. Piven2, N.I. Sidorov1, V.A. Polukhin1

1Institute of Metallurgy, Ural Branch of the Russian Academy of Sciences, Yekaterinburg, Russia

2Krasnodar Air Force Institute for Pilots named after Hero of the Soviet Union A.K. Serov, Krasnodar-5, Russia

DOI: 10.26456/pcascnn/2019.11.074

Abstract: Under the conditions of the fast crystallization of melts, the effect of hydrogen on mechanisms of structural transformations in V85Ni15 and V85-xTixNi15 alloys was experimentally studied. Structuring of phase compositions, diffusion, and hydrogen permeability were simulated. The regularities of improving the structural characteristics of alloys as a result of alloying with titanium, as well as the effect of hydrogen dynamics on the stability of the formed phases are revealed.

Keywords: hydrogen, BCC phase, diffusion, permeability, simulation, multiparticle potentials, titanium alloys, microstructure, hybridization of polymorphic-phase transitions, membrane technologies, hydrides.

Bibliography link:

Belyakova, R.M. Influence of Ti – H hydrides on interatomic interactions and on characteristics of Ti alloying membrane alloys based on V – Ni / R.M. Belyakova, V.A. Piven, N.I. Sidorov et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2019. – I. 11. – P. 74-85.