Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials
Founded at 2009


Electron-stimulated oxygen adsorption on the surface of metals and semiconductors

O.G. Ashkhotov, I.B. Ashkhotova, M.A. Aleroev, D.A. Krimshokalova

Kabardino-Balkarian State University named after H.M. Berbekov, Nalchik, Russia

DOI: 10.26456/pcascnn/2019.11.026

Abstract: The phenomenon of electron-stimulated adsorption occurs in almost all devices where electron emission is used. Electron-stimulated adsorption can have a significant effect on the state of the adsorbed layer. This review presents typical results obtained in the study of electronically stimulated processes of the oxygen adsorption from a gas phase and the main patterns of changes in the surface structure caused by electron-stimulated adsorption.

Keywords: spectroscopy, surface, electrons, radiation, dissociation, migration, adsorption, desorption, experiments, exposure.

Bibliography link:

Ashkhotov, O.G. Electron-stimulated oxygen adsorption on the surface of metals and semiconductors / O.G. Ashkhotov, I.B. Ashkhotova, M.A. Aleroev et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2019. – I. 11. – P. 26-39.

Full text (in Russian): download PDF file

Comments are closed.