Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials
Founded at 2009


Grain structure of bismuth-tin alloys, additional doping with indium

DOI:

Abstract:

Keywords:

Reference:

, .. Grain structure of bismuth-tin alloys, additional doping with indium / // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. – Tver: TSU, . — I. . — P. -. DOI: . (In Russian).