Optical characteristics of thin films of potassium-tungsten bronzes

B.M. Khubolov1, V.P. Podlinov2, A.M. Bagov1
1Kabardino-Balkarian State University named after H.M. Berbekov
2North-Caucasus Federal University

DOI: 10.26456/pcascnn/2018.10.656

Abstract: The spectral dependences of the optical density of thin amorphous film of oxide potassium-tungsten bronze of hexagonal structure and composition K0,3WO3 have been measured. The central problems of interpreting of optical spectra of oxide tungsten bronzes have been postulated.
Keywords: tungsten-potassium oxide bronze, thin films, spectral characteristics, discrete evaporation, absorption centers.

Bibliography link:
Khubolov, B.M. Optical characteristics of thin films of potassium-tungsten bronzes / B.M. Khubolov, V.P. Podlinov, A.M. Bagov // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 656-664.