Particularities of the structure and photoelectric fields of LiNbO3 : Zn crystals

N.V. Sidorov, A.M. Shuvalova, N.A. Teplyakova, M.N. Palatnikov
I.V. Tananaev Institute of Chemistry  Subdivision of the Federal Research Centre «Kola Science Centre of the Russian Academy of Sciences»

DOI: 10.26456/pcascnn/2018.10.584

Abstract: Values of intensities of photovoltaic and diffusion fields were determined in congruent LiNbO3 crystals both nominally pure and doped by zinc due to parameters of a photoinduced light scattering. A change in electro-optical properties of LiNbO3 : Zn crystals at an increase in the zinc concentration to a threshold value was shown to be determined by particularities of oxygen octahedra deformations and an order of cation sublattice structure units along the polar axis.
Keywords: single crystal, lithium niobate, doping, photoinduced light scattering, photorefractive effect, photovoltaic field, diffusion field.

Bibliography link:
Sidorov, N.V. Particularities of the structure and photoelectric fields of LiNbO3 : Zn crystals / N.V. Sidorov, A.M. Shuvalova, N.A. Teplyakova et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 584-590.