Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Classification and selection of barbage equipment for collecting dust nanoparticles

G.I. Sverdlik, A.Y. Ataeva, D.A. Kambolov, A.R. Ataev
North Caucasian Institute of Mining and Metallurgy (State Technological University)

DOI: 10.26456/pcascnn/2018.10.566

Abstract: А classification of bubblers according to a constructive feature has been developed on the basis of literature analysis and patent search. A comparison of different types of bubblers has been performed according their ability to effectively capture small particles, including nanoparticles. For this purpose it is recommended to use a jet bubbler developed in the North Caucasian Institute of Mining and Metallurgy (State Technological University) on the basis of the patented distribution cup cap plate.
Keywords: gas emissions, nanoparticles, bubbler classification, jet bubbler, foam regime, experimental installation.

Bibliography link:
Sverdlik, G.I. Classification and selection of barbage equipment for collecting dust nanoparticles / G.I. Sverdlik, A.Y. Ataeva, D.A. Kambolov et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 566-575.

Full text (in Russian): download PDF file