Effect of electronic irradiation on properties, composition of lead-silicate glasses and coefficient of secondary electron emission on their surface

V.I. Savenko
Ltd Vladikavkaz Technological Center «Baspik»
Kabardino-Balkarian State University named after H.M. Berbekov

DOI: 10.26456/pcascnn/2018.10.557

Abstract: The paper discusses the effectiveness of methods for degassing surfaces of lead-silicate glasses by electron irradiation (treatment) in order to increase the efficiency of secondary electron emission. Changes in the properties and composition of the processed materials as a result of additional effects (heat treatment, reactions with ethyl alcohol, etc.) are revealed. Chemical compounds and elements formed as a result of impacts on the surface of lead-silicate glasses are described. The effect of sample storage on a further change in the secondary electron emission coefficient was studied.
Keywords: electron irradiation, electron processing, lead-silicate glass, processed surface of lead-silicate glasses, secondary electron emission, amplification.

Bibliography link:
Savenko, V.I. Effect of electronic irradiation on properties, composition of lead-silicate glasses and coefficient of secondary electron emission on their surface / V.I. Savenko // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 557-565.