Investigation of the bombardment of low-energy isomers of Tin clusters (n = 7, 13, 15, 19)  by titanium atoms: molecular dynamics simulation

N.A. Pan’kin, I.A. Bataykina
National Research N.P. Ogarev Mordovia State University

DOI: 10.26456/pcascnn/2018.10.506

Abstract: The process of bombardment of low-energy isomers of Tin (n = 7, 13, 15, 19) clusters by titanium atoms is considered by molecular dynamics. It is shown that the initial cluster temperature (up to 500 K) does not influence the final results. Ion bombardment leads to the destruction of the initial cluster structure with the release of smaller particles. A significant fraction of the spray/decomposition products are monomers and dimers.
Keywords: isomer, bombardment, distribution functions, cluster.

Bibliography link:
Pan’kin, N.A. Investigation of the bombardment of low-energy isomers of Tin clusters (n = 7, 13, 15, 19)  by titanium atoms: molecular dynamics simulation / N.A. Pan’kin, I.A. Bataykina // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 506-516.

Full text (in Russian): download PDF file