Study of wetting the surface of silicon with NaCl-water solution

M.M. Orakova, G.A. Mustafaev, R.R. Nagaplezheva
Kabardino-Balkarian State University named after H.M. Berbekov

DOI: 10.26456/pcascnn/2018.10.501

Abstract: The dependence of the water runoff angles from the silicon surface on the conditions of their preparation is investigated. The objects of investigation were single-crystal silicon plates KDB-10 with orientations (111) and (100). It is shown that the use of ethanol in the preparation of plates improves wetting with water. It is also established that small doses of NaCl in water do not affect the angle of the droplet flow.
Keywords: adsorption, drain angle, wetting angle, surface tension, Auger analysis.

Bibliography link:
Orakova, M.M. Study of wetting the surface of silicon with NaCl-water solution / M.M. Orakova, G.A. Mustafaev, R.R. Nagaplezheva // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 501-505.

Full text (in Russian): download PDF file