Adsorption-structural properties of calcium phosphates xerogels obtained by liquid-phase synthesis

O.N. Musskaya, A.I. Kulak, V.K. Krut’ko, I.E. Glazov
Institute of General and Inorganic Chemistry of National Academy of Sciences of Belarus

DOI: 10.26456/pcascnn/2018.10.468

Abstract: It has been established that xerogels of basic and medium calcium phosphates obtained by dehydration of calcium phosphate gels in air at 20°C with water-removing agents, cryogenic treatment (at −18 and −196°C) are characterized by a high specific surface (up to 158 m2/g). It was found that high-temperature heating of calcium phosphates at 800−1200°C leads to a significant decrease in their adsorption capacity (ABET 10−17  m2/g).
Keywords: calcium phosphate xerogel, adsorption-structural properties, hydroxyapatite, tricalcium phosphate, brushite, carbonate hydroxyapatite.

Bibliography link:
Musskaya, O.N. Adsorption-structural properties of calcium phosphates xerogels obtained by liquid-phase synthesis / O.N. Musskaya, A.I. Kulak, V.K. Krut’ko et al. // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 468-476.

Full text (in Russian): download PDF file

Comments are closed.